| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Melt Flow | 11 g/10 min | 11 g/10 min | (Condition L) ASTM D-1238-94a |
|
Multibase Multi-Pro® 3011 CHI Grey 29% Filler Content Polypropylene
Data provided by Multibase.
|
|||
| Melt Flow | 11 g/10 min | 11 g/10 min | ASTM D1238 |
|
Multibase Multi-Pro® 3011 CHI Polypropylene
Calcium Carbonate Filler, 30% by weight.Forms:PelletsProcessing Methods:Injection MoldingInformation provided by Multibase
|
|||
| Melt Flow |
11
g/10 min <br>@Load 2.16 kg,<br> Temperature 230 °C
|
11
g/10 min <br>@Load 4.76 lb,<br> Temperature 446 °F
|
Procedure A; ASTM D1238 |
|
PolyOne Maxxam™ PPH-40T Nat Polypropylene Homopolymer (PP Homopolymer)
PolyOne's Maxxam™ family of polypropylene- and polyethylene-based products covers a wide range of applications, markets and performance requirements. Standard grades are compounded with calcium car..
|
|||
| Melt Flow |
11
g/10 min <br>@Load 10.0 kg,<br> Temperature 190 °C
|
11
g/10 min <br>@Load 22.0 lb,<br> Temperature 374 °F
|
ISO 1133 |
|
Premix Thermoplastics PRE-ELEC® TPE 1501 Conductive Thermoplastic Compound
PRE-ELEC® TPE 1501 is a conductive thermoplastic compound based on a thermoplastic elastomer (TPE). Conductivity is achieved by using a special conductive carbon black. In addition to a low electri..
|
|||
| Melt Flow |
11
g/10 min <br>@Load 5.00 kg,<br> Temperature 260 °C
|
11
g/10 min <br>@Load 11.0 lb,<br> Temperature 500 °F
|
ASTM D1238 |
|
SABIC Innovative Plastics Cycoloy® CX3222ME PC+ABS
Cycoloy* resin grade CX3222ME is an extrudable & thermoformable PC/ABS blend with non brominated and non chlorinated flame retardant systems. Key features of low gloss and good impact make it ideal ..
|
|||
| Melt Flow |
11
g/10 min <br>@Load 1.20 kg,<br> Temperature 300 °C
|
11
g/10 min <br>@Load 2.65 lb,<br> Temperature 572 °F
|
ASTM D1238 |
|
Ravago Manufacturing Americas Hylex® P1010LLT Polycarbonate
Information provided by Ravago.
|
|||
| Melt Flow |
11
g/10 min <br>@Load 5.00 kg,<br> Temperature 190 °C
|
11
g/10 min <br>@Load 11.0 lb,<br> Temperature 374 °F
|
Procedure A; ASTM D1238 |
|
PolyOne Elastamax™ EG-9165 Thermoplastic Elastomer (TPE)
The Elastamax™ EG 9100 Series is a new family of olefin-based TPE compounds offering outstanding elastomeric performance in a lightweight and easy to process material. The EG 9100 Series of compoun..
|
|||
| Melt Flow |
11
g/10 min <br>@Load 2.16 kg,<br> Temperature 400 °C
|
11
g/10 min <br>@Load 4.76 lb,<br> Temperature 752 °F
|
ASTM D1238 |
|
Solvay Specialty Polymers KetaSpire® KT-880 CF30 Polyetheretherketone (PEEK)
(Unverified Data**)
KetaSpire KT-880 CF30 is a high flow, 30% carbon fiber reinforced grade of polyetheretherketone (PEEK). Carbon-fiber reinforcement of KetaSpire PEEK provides the maximum levels of mechanical propert..
|
|||
| Melt Flow | 11 g/10 min | 11 g/10 min | ASTM D1238 |
|
LyondellBasell Microthene® G MU76300 Ethylene Vinyl Acetate Copolymer
General DescriptionMicrothene G polyolefin powders are ground, irregularly-shaped particles designed for use in a broad range of specialty applications. Microthene G powders combine the unique prop..
|
|||
| Melt Flow |
11
g/10 min <br>@Load 5.00 kg,<br> Temperature 200 °C
|
11
g/10 min <br>@Load 11.0 lb,<br> Temperature 392 °F
|
ASTM D1238 |
|
LG Chemical HIPS 406AF PS, Flame Retardant
Description: Injection Molding, PS, Flame RetardantApplication: Office Appliances (Parts of Printer or Copier)CAS: 9003-55-8, 25713-60-4 and 1309-64-4Information provided by LG Chemical
|
|||
| Melt Flow | 11 g/10 min | 11 g/10 min | Condition G |
|
Ineos Nova 3101 General Purpose Crystal Polystyrene
Good balance of flow and set-up properties, Good crack resistanceApplications: Single service cutlery, Single service drinkware, Consumer electronic packagingExposure to gamma radiation in the 2.02-..
|
|||
| Melt Flow |
11
g/10 min <br>@Load 2.16 kg,<br> Temperature 230 °C
|
11
g/10 min <br>@Load 4.76 lb,<br> Temperature 446 °F
|
ASTM D1238 |
|
IRPC Polimaxx Polene 1100NK Polypropylene Homopolymer
CHARACTERISTICS: HIGH FLOWAPPLICATIONS: FOR INJECTION MOLDING GENERAL PURPOSE : HOUSEWARES, CLOSURES, FOOD CONTAINERS
|
|||
| Melt Flow |
11
g/10 min <br>@Load 3.80 kg,<br> Temperature 230 °C
|
11
g/10 min <br>@Load 8.38 lb,<br> Temperature 446 °F
|
ASTM D1238 |
|
LTL Color Compounds ColorFast® FRA205 ABS
Flame-retarded V0, high gloss ABS with superior UV stabilityAll information provided by LTL Color Compounders, Inc.
|
|||
| Melt Flow |
11
g/10 min <br>@Load 2.16 kg,<br> Temperature 230 °C
|
11
g/10 min <br>@Load 4.76 lb,<br> Temperature 446 °F
|
ASTM D1238 |
|
IRPC Polimaxx Polene 1125NA Polypropylene Homopolymer
CHARACTERISTICS: GOOD EXTRUDABILITY, LOW GEL CONTAIN MEDIUM SLIP AND ANTIBLOCK ADDITIVESAPPLICATIONS: CAST FILM AND TUBULAR BLOW FILM WATER QUENCH CPP FILM FOR FOOD PACKAGING, CPP FILM FOR LAMINATIO..
|
|||
| Melt Flow |
11
g/10 min <br>@Load 6.60 kg,<br> Temperature 337 °C
|
11
g/10 min <br>@Load 14.6 lb,<br> Temperature 639 °F
|
ASTM D1238 |
|
SABIC Innovative Plastics ULTEM CRS5011R PEI (Asia Pacific)
Enhanced flow Polyetherimide copolymer (Tg 225C) with internal mold release and enhanced chemical resistance to strong acids, bases, aromatics and ketones. ECO Conforming.
|
|||
| Melt Flow |
11
g/10 min <br>@Load 6.60 kg,<br> Temperature 337 °C
|
11
g/10 min <br>@Load 14.6 lb,<br> Temperature 639 °F
|
ASTM D1238 |
|
SABIC Innovative Plastics ULTEM CRS5011R PEI (Europe-Africa-Middle East)
Enhanced flow Polyetherimide copolymer (Tg 225C) with internal mold release and enhanced chemical resistance to strong acids, bases, aromatics and ketones. Resin is RoHS compliant.
|
|||
| Melt Flow |
11
g/10 min <br>@Load 2.16 kg,<br> Temperature 400 °C
|
11
g/10 min <br>@Load 4.76 lb,<br> Temperature 752 °F
|
ASTM D1238 |
|
Solvay Specialty Polymers KetaSpire® KT-880 CF30 Polyetheretherketone (PEEK), 30% Carbon Fiber
KetaSpire® KT-880 CF30 is a high flow, 30% carbon fiber reinforced grade of polyetheretherketone (PEEK). Carbon-fiber reinforcement of KetaSpire® PEEK provides the maximum levels of mechanical..
|
|||
| Melt Flow |
11
g/10 min <br>@Load 5.00 kg,<br> Temperature 250 °C
|
11
g/10 min <br>@Load 11.0 lb,<br> Temperature 482 °F
|
ASTM D1238 |
|
SABIC Innovative Plastics Xenoy® HX5600HP PBT+PC (Asia Pacific)
Xenoy HX5600HP is PBT based semi-crystalline blend with balanced flow and impact properties. Improved chemical resistance against lab disinfectants and chemicals for healthcare enclosure and housing..
|
|||
| Melt Flow |
11
g/10 min <br>@Load 2.16 kg,<br> Temperature 260 °C
|
11
g/10 min <br>@Load 4.76 lb,<br> Temperature 500 °F
|
ASTM D1238 |
|
Star Plastics PC/ABSFR9001 Molding Grade PC/ABSFR
Information provided by Star Plastics, Inc.
|
|||
| Melt Flow |
11
g/10 min <br>@Load 1.20 kg,<br> Temperature 300 °C
|
11
g/10 min <br>@Load 2.65 lb,<br> Temperature 572 °F
|
ASTM D1238 |
|
Star Plastics PC743 Molding Grade PC
Information provided by Star Plastics, Inc.
|
|||
| Melt Flow |
11
g/10 min <br>@Load 5.00 kg,<br> Temperature 200 °C
|
11
g/10 min <br>@Load 11.0 lb,<br> Temperature 392 °F
|
ASTM D1238 |
|
Samsung Cheil Industries Starex® NH-1926 HIPS, Unreinforced FR
Non-halogen flame-retardant HIPS with high-impact that can be used in the exterior of TV and VCR interior/exterior material of OA devicesInformation provided by Samsung Cheil Industries.
|
|||
| Melt Flow |
11
g/10 min <br>@Load 2.16 kg,<br> Temperature 230 °C
|
11
g/10 min <br>@Load 4.76 lb,<br> Temperature 446 °F
|
ISO 1133 |
|
Borealis EE002AE Polypropylene Elastomer Modified
EE002AE is a reactor elastomer modified polypropylene compound intended for injection molding. The product is available in natural color. This material has excellent balanced mechanical properties..
|
|||
| Melt Flow |
11
g/10 min <br>@Load 5.00 kg,<br> Temperature 260 °C
|
11
g/10 min <br>@Load 11.0 lb,<br> Temperature 500 °F
|
|
|
Covestro Bayblend® KU 2-1480 Polycarbonate/ABS Blend
Increased thermal stability during processing, slightly higher modulus of elasticity and slightly decreased low-temperature toughness compared to BAYBLEND T 65 MN.Information provided by Bayer.As of..
|
|||
| Melt Flow |
11
g/10 min <br>@Load 5.00 kg,<br> Temperature 260 °C
|
11
g/10 min <br>@Load 11.0 lb,<br> Temperature 500 °F
|
ISO 1133 |
|
Covestro Bayblend® T45 Polycarbonate + ABS
General purpose injection molding gradeVicat/B 120 temperature = 112 °CPreprocessingMax. Water content
|
|||
| Melt Flow |
11
g/10 min <br>@Load 1.20 kg,<br> Temperature 300 °C
|
11
g/10 min <br>@Load 2.65 lb,<br> Temperature 572 °F
|
ISO 1133 |
|
Covestro Makrolon® 1837* Polycarbonate, Impact Grade
ISO 7391-PC,MP,(,,)-09-9Global gradeFormerly Makrolon DP1-1837MVR (300 °C/1.2 kg) 11 cm3/10 minImpact modifiedMedium viscosityEasy releaseInjection molding - Melt temperature 280 - 320 °CAvailable..
|
|||
| Melt Flow |
11
g/10 min <br>@Load 2.16 kg,<br> Temperature 230 °C
|
11
g/10 min <br>@Load 4.76 lb,<br> Temperature 446 °F
|
ASTM Data |
|
Dow Prevail® 3150 ABS + Polyurethane
PREVAIL® 3150 thermoplastic resin offers designers and manufacturers a combination of flexibility and low temperature toughness not previously available in an engineering thermoplastic and is used ..
|
|||
| Melt Flow |
11
g/10 min <br>@Load 1.20 kg,<br> Temperature 300 °C
|
11
g/10 min <br>@Load 2.65 lb,<br> Temperature 572 °F
|
ISO 1133 |
|
Covestro Makrolon® ET UV130 Polycarbonate
Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• PC/UV absorber concent..
|
|||
| Melt Flow |
11
g/10 min <br>@Load 5.00 kg,<br> Temperature 200 °C
|
11
g/10 min <br>@Load 11.0 lb,<br> Temperature 392 °F
|
ASTM D1238 |
|
Dynasol Solprene® 4321 Thermoplastic Rubber (SBS)
Solprene 4321 is a linear block copolymer of styrene and butadiene, with 32% styrene content, most of it forming polystyrene block, which gives the polymer a thermoplastic behavior. It has a non-st..
|
|||
| Melt Flow | 11 g/10 min | 11 g/10 min | ASTM D1238 |
|
Buckeye Polymers BP Flex D7030 UC85 TPO
Bumpers, Air damsTPO's are a family of thermoplastic elastomers which exhibit rubber-like properties and are processable on conventional thermoplastic equipment. These resins have excellent UV resi..
|
|||
| Melt Flow |
11
g/10 min <br>@Load 2.16 kg,<br> Temperature 190 °C
|
11
g/10 min <br>@Load 4.76 lb,<br> Temperature 374 °F
|
ASTM D1238 |
|
A. Schulman POLYBATCH™ White 8350/UV5 Concentrate Based In Polyethylene
DescriptionPOLYBATCH® 8350/UV5 is a specialty white color concentrate containing an optimized blend of white and UV stabilizer based in polyethylene. POLYBATCH® 8350/UV5 has been designed to prov..
|
|||