Processing Properties Metric English Comments
Nozzle Temperature 250 - 265 °C
482 - 509 °F
Parker Chomerics PREMIER™ A220-FR EMI Shielding Plastic
Description: PREMIER™ is the world’s first and most versatile commercially available conductive thermoplastic for real world EMI shielding solutions. It is a blend of PC/ABS thermoplastic polymer ..
Nozzle Temperature 245 - 265 °C
473 - 509 °F
Nilit Nilamid B G4 FR HF 20% Glass Fiber Reinforced, Flame Retardant PA6
Description: Nilamid B G4 FR HF is a NYLON 6 based flame retardant compound that does not contain any halogen or red phosphorous. It has a good overall mechanical performance, has an excellent price..
Nozzle Temperature 250 - 265 °C
482 - 509 °F
Lehmann & Voss LUVOCOM® 1850/CF/10/GF/10/GK/10/GS/5/FR PBT, with carbon fiber, glass fiber, glass spheres and glass flakes, fire protection
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High dimensionally stable precision parts, even at elevated temperatures and narrow tolerance r..
Nozzle Temperature 250 - 265 °C
482 - 509 °F
Lehmann & Voss LUVOCOM® 1850/CF/15/TF/10/EM PBT, with carbon fiber, PTFE, easy flowing
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Electrically conductive, suita..
Nozzle Temperature 250 - 265 °C
482 - 509 °F
Lehmann & Voss LUVOCOM® 1850/GF/30/TF/13/SI/2 PBT, with glass fiber, PTFE, lubricant modified
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.High dimensionally stable prec..
Nozzle Temperature 250 - 265 °C
482 - 509 °F
Lehmann & Voss LUVOCOM® 1850/GF/30/TF/13/SI/2/BK PBT, with glass fiber, PTFE, lubricant modified
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.High dimensionally stable prec..
Nozzle Temperature 250 - 265 °C
482 - 509 °F
Lehmann & Voss LUVOCOM® 1850-7431 PBT, with carbon fiber and glass spheres
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Low warpage.Low waterabsorbtion, for dimensional stable precision parts.Par..
Nozzle Temperature 250 - 265 °C
482 - 509 °F
Lehmann & Voss LUVOCOM® 1850-7783-1 PBT, with glass fiber, PTFE, lubricant modified
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.High dimensionally stable prec..
Nozzle Temperature 250 - 265 °C
482 - 509 °F
Lehmann & Voss LUVOCOM® 1850-7853 PBT, with PTFE
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Isotropic shrinkage characteri..
Nozzle Temperature 250 - 265 °C
482 - 509 °F
Lehmann & Voss LUVOCOM® 1850-7942 PBT, with PTFE, lubricant modified
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Isotropic shrinkage characteri..
Nozzle Temperature 250 - 265 °C
482 - 509 °F
Lehmann & Voss LUVOCOM® 1850-7942/RD PBT, with PTFE, lubricant modified
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Isotropic shrinkage characteri..
Nozzle Temperature 250 - 265 °C
482 - 509 °F
Lehmann & Voss LUVOCOM® 1850-8023 PBT, with carbon fiber
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Electrically conductive, suitable for continuous discharging of statically generated electricit..
Nozzle Temperature 250 - 265 °C
482 - 509 °F
Injection Molding
LG Chemical LUMID HI5001AH PA6/PO, High Melt Strength, High Barrier property, CaCl2 Resistance
Feature: Injection Molding, PA6/PO, High Melt Strength, High Barrier property, CaCl2 ResistanceApplication: Automotive (Fuel System Tube)CAS No. 25038-54-4, 9010-79-1 and 9002-88-4Information provid..
Nozzle Temperature 250 - 265 °C
482 - 509 °F
Injection Molding
LG Chemical LUMID HI5006A(W) PA6/ABS, High Impact, Good Dimensional Stability
Feature: Injection Molding, PA6/ABS, High Impact, Good Dimensional StabilityApplication: Pipe Fitting, Electrical and Electronic partsCAS No. 25038-54-4, 9003-56-9 and 9003-54-7Information provided ..
Nozzle Temperature 250 - 265 °C
482 - 509 °F
Injection Molding
LG Chemical Lupox® GP1000D PBT
Description: Injection Molding, PBT, General PurposeApplication: Automotive (Head Lamp Bezel)CAS No. 30965-26-5Information provided by LG Chemical
Nozzle Temperature 245 - 265 °C
473 - 509 °F
Injection Molding
LG Chemical Lupox® GP2100 PBT+GF10%
Description: Injection Molding, PBT+GF10%, General Purpose Application: IT/OA, E&E, Automotive (Connector)CAS No. 65997-17-3 and 24968-12-5Information provided by LG Chemical
Nozzle Temperature 255 - 265 °C
491 - 509 °F
Injection Molding
LG Chemical Lupox® SG3250M PBT+PET+MF25%
Description: Injection Molding, PBT+PET+MF25%, Good SurfaceApplication: Automotive (Head Lamp Bezel)CAS No. 24968-12-5, 25038-59-9 and 14807-96-6Information provided by LG Chemical
Nozzle Temperature 250 - 265 °C
482 - 509 °F
Injection Molding
LG Chemical LUPOY GP5100 PC/ABS+GF10%
Description: Injection Molding, PC/ABS+GF10%, General Purpose, GF ReinforcedApplication: Electrical Appliance Housing, Automotive I/PCAS: 103598-77-2, 9003-56-9 and 65997-17-3Information provided by..
Nozzle Temperature 250 - 265 °C
482 - 509 °F
Injection Molding
LG Chemical LUPOY GP5206F PC/ABS+GF20%, Flame Retardance
Description: Injection Molding, PC/ABS+GF20%, Flame Retardance, General PurposeApplication: IT/OA (Housing)CAS: 103598-77-2, 9003-56-9, 68928-70-1, 1309-64-4 and 65997-17-3Information provided by LG..
Nozzle Temperature 250 - 265 °C
482 - 509 °F
Lehmann & Voss LUVOCOM® 1850/PL/15/BK PBT, with PTFE
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Parts for electric and electro..
Nozzle Temperature 250 - 265 °C
482 - 509 °F
Lehmann & Voss LUVOCOM® 1850-7487 PBT, with carbon fiber
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Electrically conductive, suitable for continuous discharging of statically generated electricit..
Nozzle Temperature 250 - 265 °C
482 - 509 °F
Injection Molding
LG Chemical LUPOY ER5001RF PC/ABS
Description: Injection Molding, PC/ABS, Halogen Free Flame Retardant, EPEATApplication: IT&OA (All in One PC & Notebook PC housing)CAS: 103598-77-2, 9003-56-9 and 181028-79-5Information provided by ..
Nozzle Temperature 250 - 265 °C
482 - 509 °F
Injection Molding
LG Chemical LUPOY ER5001RFA PC/ABS, Halogen Free, Flame Retardant
Description: Injection Molding, PC/ABS, Halogen Free Flame Retardant, EPEATApplication: IT&OA (Notebook PC housing)CAS: 103598-77-2, 9003-56-9 and 181028-79-5Information provided by LG Chemical
Nozzle Temperature 250 - 265 °C
482 - 509 °F
Injection Molding
LG Chemical LUPOY GP1000M PC, Transparent
Description: Injection Molding, PC, General Purpose, TransparencyApplication: IT/OA, Electric & Electronic Housing and Components, Automotive Exterior and InteriorCAS: 103598-77-2Information provide..
Nozzle Temperature 250 - 265 °C
482 - 509 °F
Injection Molding
LG Chemical LUPOY GP1000MR PC, Transparent
Description: Injection Molding, PC, General Purpose, Transparency, Mold ReleaseApplication: IT/OA Housing and Components, Automotive InteriorCAS: 103598-77-2Information provided by LG Chemical
Nozzle Temperature 250 - 265 °C
482 - 509 °F
Injection Molding
LG Chemical LUPOY GP1000MU PC, Transparent
Description: Injection Molding, PC, General Purpose, Transparency, UV StabilityApplication: IT/OA Housing and Components, Automotive Exterior and InteriorCAS: 103598-77-2Information provided by LG C..
Nozzle Temperature 260 - 265 °C
500 - 509 °F
Beijing Chemical Industry KAIFA® MN301-M30 Nylon 66 Resin
Mineral filled, Good flowInformation provided by Beijing Chemical Industry Research Institute (Group)
Nozzle Temperature 260 - 265 °C
500 - 509 °F
Beijing Chemical Industry KAIFA® MN101 Nylon 66 Resin
Good flow, High impactInformation provided by Beijing Chemical Industry Research Institute (Group)
Nozzle Temperature 250 - 265 °C
482 - 509 °F
Average value: 258 °C Grade Count:14
Overview of materials for Polybutylene Terephthalate (PBT), Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Carbon Fiber Filled". Each property range of values reported is minimu..