| Category | Polymer , Thermoplastic , ABS Polymer , Acrylonitrile Butadiene Styrene (ABS), Molded |
| Manufacturer | LG Chemical |
| Trade Name | |
| Port | Shanghai port,China |
| Trade Terms | FOB, CFR, CIF |
| Payment Terms | L/C, T/T, Western Union |
| Download PDF | LG Chemical AF312T ABS, Flame Retardant.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.18 g/cc | 1.18 g/cc | ASTM D792 |
| Maximum Moisture Content | 0.010 | 0.010 | Injection Molding |
| Linear Mold Shrinkage, Flow | 0.0040 - 0.0070 cm/cm @Thickness 3.20 mm |
0.0040 - 0.0070 in/in @Thickness 0.126 in |
ASTM D955 |
| Melt Flow | 52 g/10 min @Load 10.0 kg, Temperature 220 °C |
52 g/10 min @Load 22.0 lb, Temperature 428 °F |
ASTM D1238 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Rockwell R | 104 | 104 | ASTM D785 |
| Tensile Strength, Yield | 42.2 MPa @Thickness 3.20 mm |
6120 psi @Thickness 0.126 in |
50 mm/min; ASTM D638 |
| Elongation at Break | 25 % @Thickness 3.20 mm |
25 % @Thickness 0.126 in |
50 mm/min; ASTM D638 |
| Elongation at Yield | >= 5.0 % @Thickness 3.20 mm |
>= 5.0 % @Thickness 0.126 in |
50 mm/min; ASTM D638 |
| Tensile Modulus | 2.16 GPa @Thickness 3.20 mm |
313 ksi @Thickness 0.126 in |
1 mm/min; ASTM D638 |
| Flexural Yield Strength | 68.6 MPa @Thickness 6.40 mm |
9960 psi @Thickness 0.252 in |
15 mm/min; ASTM D790 |
| Flexural Modulus | 2.60 GPa @Thickness 6.40 mm |
377 ksi @Thickness 0.252 in |
15 mm/min; ASTM D790 |
| Izod Impact, Notched | 2.26 J/cm @Thickness 6.40 mm, Temperature 23.0 °C |
4.22 ft-lb/in @Thickness 0.252 in, Temperature 73.4 °F |
ASTM D256 |
| 2.75 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
5.14 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 | |
| Izod Impact, Unnotched | 0.785 J/cm @Thickness 6.40 mm, Temperature -30.0 °C |
1.47 ft-lb/in @Thickness 0.252 in, Temperature -22.0 °F |
ASTM D256 |
| 0.785 J/cm @Thickness 3.20 mm, Temperature -30.0 °C |
1.47 ft-lb/in @Thickness 0.126 in, Temperature -22.0 °F |
ASTM D256 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Deflection Temperature at 0.46 MPa (66 psi) | 84.0 °C @Thickness 6.40 mm |
183 °F @Thickness 0.252 in |
Unannealed; ASTM D648 |
| Deflection Temperature at 1.8 MPa (264 psi) | 76.0 °C @Thickness 6.40 mm |
169 °F @Thickness 0.252 in |
Unannealed; ASTM D648 |
| Vicat Softening Point | 84.0 °C @Load 5.00 kg |
183 °F @Load 11.0 lb |
50°C/h; ASTM D1525 |
| UL RTI, Electrical | 85.0 °C @Thickness >=1.50 mm |
185 °F @Thickness >=0.0591 in |
UL 746B |
| 85.0 °C @Thickness >=2.00 mm |
185 °F @Thickness >=0.0787 in |
||
| 85.0 °C @Thickness >=2.50 mm |
185 °F @Thickness >=0.0984 in |
||
| 85.0 °C @Thickness >=3.00 mm |
185 °F @Thickness >=0.118 in |
||
| UL RTI, Mechanical with Impact | 75.0 °C @Thickness >=1.50 mm |
167 °F @Thickness >=0.0591 in |
UL 746B |
| 75.0 °C @Thickness >=2.00 mm |
167 °F @Thickness >=0.0787 in |
||
| 75.0 °C @Thickness >=2.50 mm |
167 °F @Thickness >=0.0984 in |
||
| 75.0 °C @Thickness >=3.00 mm |
167 °F @Thickness >=0.118 in |
||
| UL RTI, Mechanical without Impact | 75.0 °C @Thickness >=1.50 mm |
167 °F @Thickness >=0.0591 in |
UL 746B |
| 75.0 °C @Thickness >=2.00 mm |
167 °F @Thickness >=0.0787 in |
||
| 75.0 °C @Thickness >=2.50 mm |
167 °F @Thickness >=0.0984 in |
||
| 75.0 °C @Thickness >=3.00 mm |
167 °F @Thickness >=0.118 in |
||
| Flammability, UL94 | V-0 @Thickness >=1.50 mm |
V-0 @Thickness >=0.0591 in |
|
| V-0 @Thickness >=2.00 mm |
V-0 @Thickness >=0.0787 in |
||
| V-0 @Thickness >=2.50 mm |
V-0 @Thickness >=0.0984 in |
||
| V-0 @Thickness >=3.00 mm |
V-0 @Thickness >=0.118 in |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Volume Resistivity | 1.00e+14 ohm-cm | 1.00e+14 ohm-cm | |
| Dielectric Strength | 30.0 kV/mm | 762 kV/in | |
| Comparative Tracking Index | 400 - 600 V | 400 - 600 V | |
| Hot Wire Ignition, HWI | 15 - 30 sec @Thickness >=1.50 mm |
15 - 30 sec @Thickness >=0.0591 in |
|
| 15 - 30 sec @Thickness >=2.00 mm |
15 - 30 sec @Thickness >=0.0787 in |
||
| 15 - 30 sec @Thickness >=2.50 mm |
15 - 30 sec @Thickness >=0.0984 in |
||
| 60 - 120 sec @Thickness >=3.00 mm |
60 - 120 sec @Thickness >=0.118 in |
||
| High Amp Arc Ignition, HAI | >= 120 arcs @Thickness 1.50 mm |
>= 120 arcs @Thickness 0.0591 in |
|
| >= 120 arcs @Thickness 2.00 mm |
>= 120 arcs @Thickness 0.0787 in |
||
| >= 120 arcs @Thickness 2.50 mm |
>= 120 arcs @Thickness 0.0984 in |
||
| >= 120 arcs @Thickness 3.00 mm |
>= 120 arcs @Thickness 0.118 in |
||
| High Voltage Arc-Tracking Rate, HVTR | 25.4 - 50.0 mm/min | 1.00 - 1.97 in/min |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Rear Barrel Temperature | 170 - 190 °C | 338 - 374 °F | Injection Molding |
| Middle Barrel Temperature | 180 - 200 °C | 356 - 392 °F | Injection Molding |
| Front Barrel Temperature | 190 - 210 °C | 374 - 410 °F | Injection Molding |
| Nozzle Temperature | 200 - 230 °C | 392 - 446 °F | Injection Molding |
| Melt Temperature | 200 - 230 °C | 392 - 446 °F | Injection Molding |
| Mold Temperature | 40.0 - 60.0 °C | 104 - 140 °F | Injection Molding |
| Drying Temperature | 70.0 - 80.0 °C | 158 - 176 °F | Injection Molding |
| Dry Time | 2.00 - 4.00 hour | 2.00 - 4.00 hour | Injection Molding |
| Back Pressure | 0.490 - 0.981 MPa | 71.1 - 142 psi | Injection Molding |
| Screw Speed | 30 - 60 rpm | 30 - 60 rpm | Injection Molding |