Processing Properties | Metric | English | Comments |
---|---|---|---|
Melt Temperature | 200 - 250 °C | 392 - 482 °F | |
Plastcom SLOVALEN PC 13 T 30 PP, 30% mineral filling FeaturesModified copolymer PP for injection moulding or extrusion parts with the content of 30 % mineral filler. Increased rigidity, strength and impact strenght.Delivered in natural mode and in the.. |
|||
Melt Temperature | 200 - 250 °C | 392 - 482 °F | |
Plastcom SLOVALEN PC 63 T 15 PP reinforced with 15% mineral filler Features: Modified PP for injection moulding with the content of 15% mineral filling. Increased rigidity, strength and thermal. Decreased shrinkage. Application in all automotive interior industry.D.. |
|||
Melt Temperature | 200 - 250 °C | 392 - 482 °F | |
Plastcom SLOVALEN PC 79 GF 20 PP, 20% glass fibre, mod. of mech. prop. FeaturesModified homopolymer PP for injection moulding, chemically reinforced with 20% glass fibre, contains the modifier of mechanical properties. Increased strength in comparison with unfilled PP... |
|||
Melt Temperature | 200 - 250 °C | 392 - 482 °F | |
Plastcom SLOVALEN PC 81 T 30 PP, 30% mineral filling FeaturesModified copolymer PP for injection moulding with the content of 30% microground, floated, chemically modified talc. General application - packing material, garden flower-pots, toys, furnitu.. |
|||
Melt Temperature | 200 - 250 °C | 392 - 482 °F | |
Plastcom SLOVALEN PH 22 T 40 PP, 40% mineral filling FeaturesModified homopolymer PP for injection moulding with the content of 40% microground, floated, chemically modified talc. Special designed for automotive light housings. Delivered in natural mo.. |
|||
Melt Temperature | 200 - 250 °C | 392 - 482 °F | |
Plastcom SLOVALEN PH 71 T 40 PP, 40% mineral filling FeaturesModified homopolymer PP for injection moulding with the content of 40% microground, floated, chemically modified talc. General application in all industry branches - packing material, garden.. |
|||
Melt Temperature | 200 - 250 °C | 392 - 482 °F | |
Plastcom SLOVALEN PH 99 GB 20 PP, 20% glass beads, mod. of mech. prop. FeaturesModified homopolymer PP for injection moulding, chemically reinforced with 20% glass beads, contains the modifier of mechanical properties. Increased strength in comparison with unfilled PP... |
|||
Melt Temperature | 200 - 220 °C | 392 - 428 °F | |
PolyOne OnFlex™ S FR 40A-3S1841 Thermoplastic Elastomer (TPE) OnFlex™-S FR thermoplastic elastomer compounds are based on hydrogenated styrenic block copolymers. This range of compounds are specially flame retarded with a highly effective, RoHS compliant halo.. |
|||
Melt Temperature | 200 - 260 °C | 392 - 500 °F | |
PolyOne OnFlex™ S KG 70A-3S2019 Thermoplastic Elastomer (TPE) OnFlex™-S KG thermoplastic elastomer compounds are based on hydrogenated styrenic block copolymers. This range of compounds are specially compatabilized to provide excellent adhesion to polyamide p.. |
|||
Melt Temperature | 200 - 250 °C | 392 - 482 °F | |
Premix Thermoplastics PRE-ELEC® PP 1378 PRE-ELEC PP 1378 is a conductive thermoplastic compound based on glass-fiber reinforced polypropylene. Conductivity is achieved by using special conductive carbon black. In addition to a low electri.. |
|||
Melt Temperature | 200 - 260 °C | 392 - 500 °F | |
Premix Thermoplastics PRE-ELEC® PP 1399 Dissipative Thermoplastic Compound PRE-ELEC® PP 1399 is a dissipative thermoplastic compound based on polypropylene. The electrical dissipation is achieved by using special conductive carbon black. In addition to stable surface resi.. |
|||
Melt Temperature | 200 - 230 °C | 392 - 446 °F | |
SABIC BM1052 High Density Polyethylene for Blow Molding Product Description: BM1052 grade is a high molecular weight High Density Polyethylene copolymer with broad molecular weight distribution. It has excellent processability and exhibits very high im.. |
|||
Melt Temperature | 200 - 280 °C | 392 - 536 °F | |
Lotte Chemical Titan TITANEX® LF2554 Linear low density polyethylene Hexene-1 resin
(discontinued **) LF2554 is a pelleted linear low density polyethylene Hexene-1 resin formulated with antioxidant. This product is used for slot cast extrusion which offers outstanding toughness, extrudability and d.. |
|||
Melt Temperature | 200 - 230 °C | 392 - 446 °F | Extrusion Molding |
LG Chemical LI968W Co-Extrusion ASA Description: Good WeatherabilityApplication: Window Profile, Siding, Rain GutterCAS: 26299-47-8Information provided by LG Chemical |
|||
Melt Temperature | 200 - 230 °C | 392 - 446 °F | Injection Molding |
LG Chemical LUPOL GP2150 PP+GF15% Description: Injection Molding, PP+GF15%, General PurposeApplication: Electrical & Electronic, Automotive PartsCAS: 9003-07-0 and 65997-17-3Information provided by LG Chemical |
|||
Melt Temperature | 200 - 230 °C | 392 - 446 °F | Injection Molding |
LG Chemical LUPOL GP3202 PP+MF20% Description: Injection Molding, PP+MF10%, General Purpose, Good WeatherabilityApplication: Electrical, Electronic and Automotive Interior PartsCAS: 9003-07-0 and 14807-96-6Information provided by LG.. |
|||
Melt Temperature | 200 - 230 °C | 392 - 446 °F | Extrusion |
Inno-Comp INNOPOL® CS 2-7120 20% Talc Filled Polypropylene Copolymer INNOPOL® CS 2-7120 is a 20 % talc-filled polypropylene block-copolymer compound /PP-B TD20 (ISO 1043)/. This grade is available in natural and custom colored form.INNOPOL® CS 2-7120 is recomme.. |
|||
Melt Temperature | 200 - 280 °C | 392 - 536 °F | |
Iran Petrochemical (PCC) I1 HA 7260 High Density Polyethylene I1 (HA 7260) is a high density polyethylene with propylene as comonomer. It is very easy flowing, high density, hardness and stiffness, largely warpage free, for mass product articles in rapid shot .. |
|||
Melt Temperature | 200 - 230 °C | 392 - 446 °F | Injection Molding |
LG Chemical AF305HT ABS, Flame Retardant, Heat Resistance Feature: Injection Molding, Flame Retardant, Heat ResistanceApplication: Electric/Electronic Applications (TV, Monitor Housing) IT/OA deviceCAS No. 9003-56-9, 9001-96-2, 68928-70-1, and 1309-64-4Inf.. |
|||
Melt Temperature | 200 - 230 °C | 392 - 446 °F | Injection Molding |
LG Chemical AF360 ABS, TBBA-free Flame Retardant Feature: Injection Molding, TBBA-free Flame RetardantApplication: Electric/Electronic Applications (TV, Monitor Housing) IT/OA deviceCAS No. 9003-56-9, 84852-53-9 and 1309-64-4Information provided b.. |
|||
Melt Temperature | 200 - 230 °C | 392 - 446 °F | Injection Molding |
LG Chemical LUPOL HF5157 PP+Rubber+MF, High Flow and Stiffness, High Impact Description: Injection Molding, PP+Rubber+MF, High Flow and Stiffness, High Impact, Good Weatherability, Scratch ResistanceApplication: Automotive Exterior (Slim wall Bumper Fascia)Information provi.. |
|||
Melt Temperature | 200 - 230 °C | 392 - 446 °F | Extrusion |
Ineos Styrenics Polystyrene 145D (NAFTA) A high flow, general purpose polystyrene, offering exceptional processing characteristics for thin wall parts, multi-cavity tools, and complex designs.Information provided by BASF.Ineos Styrenics pu.. |
|||
Melt Temperature | 200 - 240 °C | 392 - 464 °F | Flat film |
Styrolution Polystyrol 143 E GR 2 PS Description: Polystyrol 143 E is a medium strength, easy flowing general purpose grade, suitable for blending with impact modified Polystyrol, Styrolux and coextruded gloss layers.Applications: In b.. |
|||
Melt Temperature | 200 - 230 °C | 392 - 446 °F | Plates |
Styrolution Polystyrol 486 M GR 2 PS Description: Polystyrol 486 M is a normal flowing, high-impact grade that is especially suitable for blends with a high proportion of general-purpose Polystyrol (preferably Polystyrol 165 H or Polys.. |
|||
Melt Temperature | 200 - 240 °C | 392 - 464 °F | Flat film |
Styrolution Polystyrol 486 M GR 2 PS Description: Polystyrol 486 M is a normal flowing, high-impact grade that is especially suitable for blends with a high proportion of general-purpose Polystyrol (preferably Polystyrol 165 H or Polys.. |
|||
Melt Temperature | 200 - 220 °C | 392 - 428 °F | |
Borealis BorSafe™ HE3490-LS-H HDPE Compound for Pressure Pipes BorSafe™ HE3490-LS-H is a bimodal polyethylene compound produced by the advanced Borstar® technology. It includes a combination of pigments and stabilizers to ensure excellent long-term thermal s.. |
|||
Melt Temperature | 200 - 230 °C | 392 - 446 °F | |
DuPont Elvax® 3124 Ethylene-Vinyl Acetate Copolymer Resin for Extrusion Coating 9 wt% Vinyl Acetate.Elvax® 3124 is an extrudable ethylene-vinyl acetate copolymer resin available in pellet form for use in conventional extrusion equipment designed to process polyethylene resins... |
|||
Melt Temperature | 200 - 210 °C | 392 - 410 °F | Injection Molding |
DuPont Performance Polymers Delrin® 100PE NC010A Acetal Homopolymer Delrin® 100PE NC010A is a high viscosity acetal homopolymer, an enhanced version of Delrin® 100P with extremely low VOC emissions. It has improved processing thermal stability, good mechanical pro.. |
|||
Melt Temperature | 200 - 250 °C | 392 - 482 °F | |
Plastcom SLOVALEN PH 91 GF 10 PP, 10% glass fibre FeaturesModified homopolymer PP for injection moulding, chemically reinforced with 10% glass fibre. Increased strength in comparison with unfilled PP. Applied in all industry branches. Increased str.. |
|||
Melt Temperature | 200 - 230 °C | 392 - 446 °F | Injection Molding |
LG Chemical LUPOL GP3100 PP+MF10% Description: Injection Molding, PP+MF30%, General PurposeApplication: Electrical & Electronic, Automotive PartsCAS: 9003-07-0 and 14807-96-6Information provided by LG Chemical |