Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Modulus = 2.16 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 2.16 GPa
313 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP Colorcomp D10009 PC
LNP* Colorcomp* D10009 is a compound based on Polycarbonate resin containing Flame Retardant, Unfilled Custom Color. Added features of this material include: Flame Retardant.This data was supplied ..
Tensile Modulus 2.16 GPa
313 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP Colorcomp D10009 PC (Asia Pacific)
LNP* Colorcomp* D10009 is a compound based on Polycarbonate resin containing Flame Retardant, Unfilled Custom Color. Added features of this material include: Flame Retardant.This data was supplied ..
Tensile Modulus 2.16 GPa

@Thickness 3.20 mm
313 ksi

@Thickness 0.126 in
1 mm/min; ASTM D638
LG Chemical AF312B ABS, Flame Retardant
Feature: Injection Molding, Flame RetardantApplication: Electric/Electronic Applications (TV, Monitor Housing) IT/OA deviceCAS No. 9003-56-9, 79-94-7 and 1309-64-4Information provided by LG Chemical..
Tensile Modulus 2.16 GPa

@Thickness 3.20 mm
313 ksi

@Thickness 0.126 in
1 mm/min; ASTM D638
LG Chemical AF312T ABS, Flame Retardant
Feature: Injection Molding, Flame RetardantApplication: Electric/Electronic Applications (TV, Monitor Housing) IT/OA deviceCAS No. 9003-56-9, 79-94-7 and 1309-64-4Information provided by LG Chemical..
Tensile Modulus 2.16 GPa

@Thickness 3.20 mm
313 ksi

@Thickness 0.126 in
1 mm/min; ASTM D638
LG Chemical AF342F ABS, Flame Retardant, High Flow
Feature: Injection Molding, Flame Retardant, High FlowApplication: Electric/Electronic Applications (TV, Monitor Housing) IT/OA deviceCAS No. 9003-56-9, 40039-93-8 and 1309-64-4Information provided ..
Tensile Modulus 2.16 GPa

@Thickness 3.20 mm
313 ksi

@Thickness 0.126 in
1 mm/min; ASTM D638
LG Chemical AF342T ABS, Flame Retardant, High Impact
Feature: Injection Molding, Flame Retardant, High ImpactApplication: Electric/Electronic Applications (TV, Monitor Housing) IT/OA deviceCAS No. 9003-56-9, 40039-93-8 and 1309-64-4Information provide..
Tensile Modulus 2.16 GPa

@Thickness 3.20 mm
313 ksi

@Thickness 0.126 in
1 mm/min; ASTM D638
LG Chemical AF345 ABS, Flame Retardant
Feature: Injection Molding, Flame RetardantApplication: Electric/Electronic Applications (TV, Monitor Housing) IT/OA deviceCAS No. 9003-56-9, 40039-93-8 and 1309-64-4Information provided by LG Chemi..
Tensile Modulus 2.16 GPa

@Thickness 3.20 mm
313 ksi

@Thickness 0.126 in
1 mm/min; ASTM D638
LG Chemical AF360S ABS, TBBA-free Flame Retardant, Low Flow
Feature: Injection Molding, TBBA-free Flame Retardant, Low FlowApplication: Electric/Electronic Applications (TV, Monitor Housing) IT/OA deviceCAS No. 9003-56-9, 84852-53-9 and 1309-64-4Information ..
Tensile Modulus 2.16 GPa

@Thickness 3.20 mm
313 ksi

@Thickness 0.126 in
1mm/min; ASTM D638
LG Chemical ALPHALAC SH860 HIPS
Description: Injection Molding, General Purpose, Good ProcessabilityApplication: Refrigerator Inner LinerCAS No. 9003-55-8Information provided by LG Chemical
Tensile Modulus 2.16 GPa

@Thickness 3.20 mm
313 ksi

@Thickness 0.126 in
1 mm/min; ASTM D638
LG Chemical ER460 ABS, Medium Heat Resistance, High Flowability
Feature: Injection Molding, Medium Heat Resistance, High FlowabilityApplication: Automobile, Motor Cycle, Electric & Electronic GoodsCAS No. 9003-56-9Information provided by LG Chemical
Tensile Modulus 2.16 GPa
313 ksi
ASTM D638
Ineos Nova Styrosun® 3600 Weather Resistant High Impact Styrenic Polymer
Features: Outdoor weatherablePhysical property retention after UV exposurePaintable and printableExcellent toughness Can be injection molded or co-extruded Easy to process, no drying required Appli..
Tensile Modulus 2.16 GPa

@Thickness 3.20 mm
313 ksi

@Thickness 0.126 in
1 mm/min; ASTM D638
LG Chemical AF308 ABS, Flame Retardant
Feature: Injection Molding, Flame RetardantApplication: Electric/Electronic Applications (TV, Monitor Housing) IT/OA deviceCAS No. 9003-56-9, 40039-93-8 and 1309-64-4Information provided by LG Chemi..
Tensile Modulus 2.16 GPa
313 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP Lubricomp JL003 PES
LNP* Lubricomp* JL003 is a compound based on Polyethersulfone resin containing PTFE.This data was supplied by SABIC-IP for the Americas region.
Tensile Modulus 2.16 GPa
313 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP LUBRILOY RX05498 PA 66
LNP LUBRILOY* RX05498 is a compound based on Nylon 66 resin containing Proprietary Lubricant. Added features of this material include: High Impact, Wear Resistant.
Tensile Modulus 2.16 GPa
313 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP LUBRILOY RX05498 PA 66 (Asia Pacific)
LNP LUBRILOY* RX05498 is a compound based on Nylon 66 resin containing Proprietary Lubricant. Added features of this material include: High Impact.
Tensile Modulus 2.16 GPa
313 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP LUBRILOY RX99650 PA 66
LNP LUBRILOY* RX99650 is a compound based on Nylon 66 resin containing Proprietary Lubricant. Added feature of this material is: Wear Resistant.
Tensile Modulus 2.16 GPa
313 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP LUBRILOY RX99650 PA 66 (Asia Pacific)
LNP LUBRILOY* RX99650 is a compound based on Nylon 66 resin containing Proprietary Lubricant. Added features of this material include: Internally Lubricated.
Tensile Modulus 2.16 GPa
313 ksi
50 mm/min; ASTM D638
Samsung Cheil Industries Infino® QP-1010 PC/ABS, Unreinforced FR
Information provided by Samsung Cheil Industries.
Tensile Modulus 2.16 GPa
313 ksi
5 mm/min; ASTM D638
Samsung Cheil Industries Infino® SI-3109GL PC, Glass Filled High Impact
Information provided by Samsung Cheil Industries.
Tensile Modulus 2.16 GPa
313 ksi
50 mm/min; ASTM D638
Samsung Cheil Industries Infino® UF-1013 PC, Unreinforced FR
Information provided by Samsung Cheil Industries.
Tensile Modulus 2.16 GPa
313 ksi
5 mm/min; ASTM D638
Samsung Cheil Industries Starex® LX-0970 LS ABS, Unreinforced Metallic-Look
Luminous Grade - gives aesthetics of a painted surface without painting. Reduces time, cost, and environmental hazards (such as soilvents).Information provided by Samsung Cheil Industries.
Tensile Modulus 2.16 GPa
313 ksi
50 mm/min; ASTM D638
Samsung Cheil Industries Starex® LX-0971 S ABS, Unreinforced Metallic-Look
Luminous Grade - gives aesthetics of a painted surface without painting. Reduces time, cost, and environmental hazards (such as soilvents).Information provided by Samsung Cheil Industries.
Tensile Modulus 2.16 GPa
313 ksi
5 mm/min; ASTM D638
Samsung Cheil Industries Starex® LX-0989EXS ABS, Unreinforced Metallic-Look
Luminous Grade - gives aesthetics of a painted surface without painting. Reduces time, cost, and environmental hazards (such as soilvents).Information provided by Samsung Cheil Industries.
Tensile Modulus 2.16 GPa
313 ksi
5 mm/min; ASTM D638
Samsung Cheil Industries Starex® PT-0180 ABS, Unreinforced Painting Grade
Information provided by Samsung Cheil Industries.
Tensile Modulus 2.16 GPa
313 ksi
5 mm/min; ASTM D638
Samsung Cheil Industries Starex® LX-0957 ABS, Unreinforced Metallic-Look
Luminous Grade - gives aesthetics of a painted surface without painting. Reduces time, cost, and environmental hazards (such as soilvents).Information provided by Samsung Cheil Industries.
Tensile Modulus 2.16 GPa
313 ksi
5 mm/min; ASTM D638
Samsung Cheil Industries Starex® LX-0970 LS ABS, Unreinforced Metallic-Look
Luminous Grade - gives aesthetics of a painted surface without painting. Reduces time, cost, and environmental hazards (such as soilvents).Information provided by Samsung Cheil Industries.
Tensile Modulus 2.16 GPa
313 ksi
50 mm/min; ASTM D638
Samsung Cheil Industries Starex® LX-0971 S ABS, Unreinforced Metallic-Look
Luminous Grade - gives aesthetics of a painted surface without painting. Reduces time, cost, and environmental hazards (such as soilvents).Information provided by Samsung Cheil Industries.
Tensile Modulus 2.16 GPa
313 ksi
5 mm/min; ASTM D638
Samsung Cheil Industries Starex® SR-0315 V ABS, Unreinforced Heat Resistant
Information provided by Samsung Cheil Industries.
Tensile Modulus 2.16 GPa
313 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP Thermocomp YF004 Polyester Elastomer
LNP THERMOCOMP* YF004 is a compound based on Polyester Elastomer resin containing Glass Fiber.This data was supplied by SABIC-IP for the Americas region.
Tensile Modulus 2.16 GPa
313 ksi
50 mm/min; ASTM D638
Samsung Cheil Industries Infino® LH-1070W PC, FR
Information provided by Samsung Cheil Industries.