Processing Properties | Metric | English | Comments |
---|---|---|---|
Back Pressure | 0.490 - 0.981 MPa | 71.1 - 142 psi | Injection Molding |
LG Chemical AF342F ABS, Flame Retardant, High Flow Feature: Injection Molding, Flame Retardant, High FlowApplication: Electric/Electronic Applications (TV, Monitor Housing) IT/OA deviceCAS No. 9003-56-9, 40039-93-8 and 1309-64-4Information provided .. |
|||
Back Pressure | 0.490 - 0.981 MPa | 71.1 - 142 psi | Injection Molding |
LG Chemical LI911 ASA Description: Good Weatherability, High FlowApplication: Air-conditioner grill, Sawing Machine Cover, Electric/Electronic ApplicationsCAS: 26299-47-8Information provided by LG Chemical |
|||
Back Pressure | 0.490 - 3.04 MPa | 71.1 - 441 psi | Injection Molding |
LG Chemical LUCEL FW700S Modified POM, Friction Resistance, Abrasion Resistance Feature: Injection Molding, Modified POM, Friction Resistance, Abrasion ResistanceApplication: Gears, Printer Roller Pumps, Gear Worm WheelsCAS No. 66455-31-0Information provided by LG Chemical |
|||
Back Pressure | 0.490 - 3.04 MPa | 71.1 - 441 psi | Injection Molding |
LG Chemical LUCEL FW715CS Modified POM, Friction Resistance, Abrasion Resistance Feature: Injection Molding, Modified POM, Friction Resistance, Abrasion ResistanceApplication: Gears, Printer Roller Pumps, Gear Worm WheelsCAS No. 66455-31-0 and 471-34-1Information provided by LG .. |
|||
Back Pressure | 0.490 - 3.04 MPa | 71.1 - 441 psi | Injection Molding |
LG Chemical LUCEL HI510 POM+Rubber, High Impact Feature: Injection Molding, POM+Rubber, High ImpactApplication: Gears, Automobile ClipCAS No. 66455-31-0Information provided by LG Chemical |
|||
Back Pressure | 0.490 - 3.04 MPa | 71.1 - 441 psi | Injection Molding |
LG Chemical LUCEL HI520 POM+Rubber, High Impact Feature: Injection Molding, POM+Rubber, High ImpactApplication: GearsCAS No. 66455-31-0 and 155123-66-3Information provided by LG Chemical |
|||
Back Pressure | 0.490 - 3.04 MPa | 71.1 - 441 psi | Injection Molding |
LG Chemical LUCEL HI525L POM+Rubber, High Impact Feature: Injection Molding, POM+Rubber, High ImpactApplication: GearsCAS No. 66455-31-0 and 155123-66-3Information provided by LG Chemical |
|||
Back Pressure | 0.490 - 3.92 MPa | 71.1 - 569 psi | |
LG Chemical LUPOL GP-3154F General Purpose Polypropylene, 15% Mineral Fillers, High Modulus, Flame Retardant LUPOL resins, based on polyolefin with a wide range of characteristics, are a family of low cost engineering plastics.Applications: Automotive: Bumper cover, instrument panel, glove box, air cleaner.. |
|||
Back Pressure | 0.490 - 3.92 MPa | 71.1 - 569 psi | |
LG Chemical LUPOL HF-3202D High Flow Polypropylene, 20% Mineral Fillers, High Impact LUPOL resins, based on polyolefin with a wide range of characteristics, are a family of low cost engineering plastics.Applications: Automotive: Bumper cover, instrument panel, glove box, air cleaner.. |
|||
Back Pressure | 0.490 - 3.92 MPa | 71.1 - 569 psi | |
LG Chemical LUPOL HF-3208H High Flow Polypropylene, 20% Mineral Fillers, General Purpose LUPOL resins, based on polyolefin with a wide range of characteristics, are a family of low cost engineering plastics.Applications: Automotive: Bumper cover, instrument panel, glove box, air cleaner.. |
|||
Back Pressure | 0.490 - 3.92 MPa | 71.1 - 569 psi | |
LG Chemical LUPOL HF-3308 High Flow Polypropylene, 30% Mineral Fillers LUPOL resins, based on polyolefin with a wide range of characteristics, are a family of low cost engineering plastics.Applications: Automotive: Bumper cover, instrument panel, glove box, air cleaner.. |
|||
Back Pressure | 0.490 - 3.92 MPa | 71.1 - 569 psi | |
LG Chemical LUPOL HM-4354 Heat Resistant Polypropylene, 35% Glass Fiber/Mineral Filler Reinforced, High Strength, High Modulus LUPOL resins, based on polyolefin with a wide range of characteristics, are a family of low cost engineering plastics.Applications: Automotive: Bumper cover, instrument panel, glove box, air cleaner.. |
|||
Back Pressure | 0.490 - 3.92 MPa | 71.1 - 569 psi | |
LG Chemical LUPOL TE-5005H Thermoplastic Elastomer Alloy, Dimensional Stability LUPOL resins, based on polyolefin with a wide range of characteristics, are a family of low cost engineering plastics.Applications: Automotive exterior parts.Information Provided by LG Chem |
|||
Back Pressure | 0.490 - 3.92 MPa | 71.1 - 569 psi | |
LG Chemical LUPOL TE-5006K Thermoplastic Elastomer Alloy, Weather Resistant LUPOL resins, based on polyolefin with a wide range of characteristics, are a family of low cost engineering plastics.Applications: Automotive exterior parts.Information Provided by LG Chem |
|||
Back Pressure | 0.490 - 3.92 MPa | 71.1 - 569 psi | |
LG Chemical LUPOL TE-5104K Thermoplastic Elastomer Alloy, 10% Polymer Alloy, High Modulus LUPOL resins, based on polyolefin with a wide range of characteristics, are a family of low cost engineering plastics.Applications: Automotive exterior parts.Information Provided by LG Chem |
|||
Back Pressure | 0.490 - 1.96 MPa | 71.1 - 284 psi | |
LG Chemical TR-558NS Transparent ABS, Antistatic, Natural and Colored Pellets LG transparent ABS has excellent transparency, impact strength, stiffness, and processability. Since its properties are well balanced, it can be applied widely to a variety of electric and electron.. |
|||
Back Pressure | 0.490 - 1.47 MPa | 71.1 - 213 psi | gage pressure |
Unitika AX-1500 Dry AX series resins are opaque polymer alloys with a high deflection temperature under load without reinforcement and a chemical resistance as high as those of crystalline resins. They are excellent in.. |
|||
Back Pressure | 0.490 - 1.47 MPa | 71.1 - 213 psi | gage pressure |
Unitika AX-1500W Dry Characteristics: A resin succeeding the advantages of AX1500 resin and containing titanium oxide at high concentration. Improved drastically in light reflection and blocking properties, aimed at dis.. |
|||
Back Pressure | 0.490 - 1.47 MPa | 71.1 - 213 psi | gage pressure |
Unitika AXG-1500-300 Dry Characteristics: Glass-reinforced grades of the AX1500 resin, excellent in heat and chemical resistancesFavorable rigidity and dimensional accuracyInformation provided by Unitika Ltd. |
|||
Back Pressure | 0.490 - 1.47 MPa | 71.1 - 213 psi | gage pressure |
Unitika LM-8503-10 Chemical resistance, and excellent lubricant propertyInformation provided by Unitika Ltd. |
|||
Back Pressure | 0.490 - 1.47 MPa | 71.1 - 213 psi | gage pressure |
Unitika P-5001 Engineering Plastic P series resins are resins succeeding the characteristics of the neat polymer, U100, and improved in flowability and optical properties. Among many super engineering plastics, the resins are few tra.. |
|||
Back Pressure | 0.490 - 1.47 MPa | 71.1 - 213 psi | gage pressure |
Unitika UG-100-20 Engineering Plastic Excellent creep resistance, dimensional stability at high temperatureInformation provided by Unitika Ltd. |
|||
Back Pressure | 0.490 - 1.47 MPa | 71.1 - 213 psi | gage pressure |
Unitika P-1001A Engineering Plastic P series resins are resins succeeding the characteristics of the neat polymer, U100, and improved in flowability and optical properties. Among many super engineering plastics, the resins are few tra.. |
|||
Back Pressure | 0.490 - 1.47 MPa | 71.1 - 213 psi | gage pressure |
Unitika TERRAMAC TE-7000 Polylactic Acid (PLA) Heat-resisting grade, Injection grade. Bio-based materials produced from annually renewable raw materials.Information provided by Unitika Ltd. |
|||
Back Pressure | 0.490 - 1.47 MPa | 71.1 - 213 psi | gage pressure |
Unitika TERRAMAC TE-7300 Polylactic Acid (PLA) Heat-resisting grade, Injection grade. Bio-based materials produced from annually renewable raw materials.Information provided by Unitika Ltd. |
|||
Back Pressure | 0.490 - 1.47 MPa | 71.1 - 213 psi | gage pressure |
Unitika TERRAMAC TE-7307 Polylactic Acid (PLA) Heat-resisting grade, Injection grade. Bio-based materials produced from annually renewable raw materials.Information provided by Unitika Ltd. |
|||
Back Pressure | 0.490 - 1.47 MPa | 71.1 - 213 psi | gage pressure |
Unitika TERRAMAC TE-8300 Polylactic Acid (PLA) High-durability, Injection grade. Bio-based materials produced from annually renewable raw materials.Information provided by Unitika Ltd. |
|||
Back Pressure | 0.490 - 1.47 MPa | 71.1 - 213 psi | gage pressure |
Unitika UG-100-30 Engineering Plastic Excellent creep resistance, dimensional stability at high temperatureInformation provided by Unitika Ltd. |
|||
Back Pressure | 0.490 - 1.47 MPa | 71.1 - 213 psi | gage pressure |
Unitika P-3001 Engineering Plastic P series resins are resins succeeding the characteristics of the neat polymer, U100, and improved in flowability and optical properties. Among many super engineering plastics, the resins are few tra.. |
|||
Back Pressure | 0.490 - 0.981 MPa | 71.1 - 142 psi | Injection Molding |
LG Chemical LI912 ASA Description: Good Weatherability, General PurposeApplication: Mail Box, Sprinkler, Sash Joiner, Toy, Satellite Antenna CoverCAS: 26299-47-8Information provided by LG Chemical |