| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Flexural Modulus | 2.60 GPa | 377 ksi | ASTM D790 |
|
Nylene® Norpex® AX265 PPE (Polyphenylene Ether)
Properties for dry as molded samples.ALM, Nylene Canada, and Custom Resins are all operting companies of Polymeric Resources Corporation.
|
|||
| Flexural Modulus | 2.60 GPa | 377 ksi | 2 mm/min; ISO 178 |
|
SABIC Innovative Plastics Cycoloy® C6840 PC+ABS (Asia Pacific)
Cycoloy* C6840 resin is an injection moldable, flame retardant PC/ABS blend. It contains non-chlorinated & non-brominated flame retardant systems intended to meet governmental regulations and variou..
|
|||
| Flexural Modulus |
2.60
GPa <br>@Temperature 23.0 °C
|
377
ksi <br>@Temperature 73.4 °F
|
ISO 178 |
|
Polykemi AB POLYfill PP HIP16020FCF Polypropylene, Fast Cycle
Information provided by Polykemi AB
|
|||
| Flexural Modulus | 2.60 GPa | 377 ksi | 2 mm/min; ISO 178 |
|
SABIC Innovative Plastics Cycoloy® CX7010 PC+ABS (Asia Pacific)
Cycoloy* CX7010 resin is an injection moldable PC/ABS blend. It contains non-brominated and non-chlorinated flame retardant systems to meet UL-94 V0. Excellent flow combined with good balance of pro..
|
|||
| Flexural Modulus | 2.60 GPa | 377 ksi | ASTM D790 |
|
Polymer Resources AC-GP1 Acetal Copolymer, Low Flow, High Melt Strength
Process: Molding or ExtrusionNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by Polymer Resources Corporation.
|
|||
| Flexural Modulus | 2.60 GPa | 377 ksi | ISO 178 |
|
Radici Radiflam® BN100 AE Polybutylene Terephthalate
PBT Self-extinguishing with halogenInformation provided by Radici group.
|
|||
| Flexural Modulus | 2.60 GPa | 377 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
|
SABIC Innovative Plastics Lexan® DMX1435 PC Copolymer (Europe-Africa-Middle East)
This product will be phased out per January 2015 -- Lexan* DMX1435 is a UV stabilized standard flow polycarbonate copolymer resin with improved scratch resistance.
|
|||
| Flexural Modulus | 2.60 GPa | 377 ksi | 1.3 mm/min, 50 mm span; ASTM D 790 |
|
SABIC Innovative Plastics Lexan® HPB3144G PC Copolymer
Standard flow, transparent, high purity polycarbonate copolymer resin with reduced oxygen permeability and water vapor transmission rate. For medical devices and pharmaceutical applications. Health..
|
|||
| Flexural Modulus | 2.60 GPa | 377 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
|
SABIC Innovative Plastics Lexan® XHT3143 PC Copolymer (Asia Pacific)
XHT3143 is a high flow, UV stabilized, high heat polycarbonate copolymer. It is available in a range of opaque and limited transparent colors.
|
|||
| Flexural Modulus | 2.60 GPa | 377 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
|
SABIC Innovative Plastics Lexan® XHT4143 PC Copolymer (Asia Pacific)
XHT4143 is a high flow, UV stabilized, high heat polycarbonate copolymer blend with an HDT/Af of 162C. It is available in a range of opaque and limited transparent colors.
|
|||
| Flexural Modulus | 2.60 GPa | 377 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
|
SABIC Innovative Plastics Lexan® DMX1435 PC Copolymer (Asia Pacific)
This product will be phased out per January 2015 -- Lexan* DMX1435 is a UV stabilized standard flow polycarbonate copolymer resin with improved scratch resistance.
|
|||
| Flexural Modulus |
2.60
GPa <br>@Thickness 6.40 mm
|
377
ksi <br>@Thickness 0.252 in
|
15 mm/min; ASTM D790 |
|
LG Chemical AF312T ABS, Flame Retardant
Feature: Injection Molding, Flame RetardantApplication: Electric/Electronic Applications (TV, Monitor Housing) IT/OA deviceCAS No. 9003-56-9, 79-94-7 and 1309-64-4Information provided by LG Chemical..
|
|||
| Flexural Modulus | 2.60 GPa | 377 ksi | 2mm/min; ASTM D790 |
|
Kingfa JH960 6111 Non-halogenated Flame Retardant PC/ABS Alloy
Features:Halogen free flame retardant, V-0/1.5mm5VB/1.6mm, 5VA/3.2mmExcellent mechanical propertiesHigh heat resistanceChemical resistance, hydrolysis resistanceGood paint adhesionHigh flow ability,..
|
|||
| Flexural Modulus | 2.60 GPa | 377 ksi | 2 mm/min; ISO 178 |
|
SABIC Innovative Plastics LNP Thermocomp GX061104 PSU (Europe-Africa-Middle East)
LNP* COLORCOMP* GX061104 is a compound based on Polysulfone resin.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
|
|||
| Flexural Modulus | 2.60 GPa | 377 ksi | ASTM D790 |
|
Saint-Gobain Meldin® 7001 Direct Formed Polyimide
Finished parts and basic shapes made from unfilled polyimide material for structural applications requiring requiring high electrical insulative properties, high purity and low outgassing, and high ..
|
|||
| Flexural Modulus | 2.60 GPa | 377 ksi | 2 mm/min; ISO 178 |
|
SABIC Innovative Plastics NORYL GTX GTX678 PPE+PA (Europe-Africa-Middle East)
Noryl GTX678 resin is a high performance blend of PPE/PA that exhibits an excellent balance on non-halogenated flame retardance, conductivity, ductility, and high-heat resistance. This grade can be..
|
|||
| Flexural Modulus | 2.60 GPa | 377 ksi | ASTM D790 |
|
PlastxWorld CEVIAN® LMB10 Laser Markable Grade ABS
Black MarkingThese are typical values and are not intended for specification purposes. UL approved file No. is E47773. Information provided by PlastxWorld Inc.
|
|||
| Flexural Modulus | 2.60 GPa | 377 ksi | ISO 178 |
|
Unitika CX-2500 PA6, Conditioned
Transparent nylonInformation provided by Unitika Ltd.
|
|||
| Flexural Modulus | 2.60 GPa | 377 ksi | ASTM-D790 |
|
Polyram PlusTek PB702 Nylon 6, UV Stabilized
Polyamide 6 UV stabilized for fast cycle injection molding applicationsInformation provided by Polyram Ram On Ind.
|
|||
| Flexural Modulus | 2.60 GPa | 377 ksi | ASTM-D790 |
|
Polyram PlusTek PB801 Nylon 6, Impact Modified
impact modified polyamide 6 for injection molding applicationsInformation provided by Polyram Ram On Ind.
|
|||
| Flexural Modulus | 2.60 GPa | 377 ksi | ASTM-D790 |
|
Polyram RamOfin PPC371B73 Polypropylene, 73% Mineral Filled
73% mineral filled polypropylene for heavy density injection molding applicationsInformation provided by Polyram Ram On Ind.
|
|||
| Flexural Modulus | 2.60 GPa | 377 ksi | ISO 178 |
|
A.D. Compound Adene NCTA Homopolymer 50% CaCO3 Filled Polypropylene
Information provided by A.D. Compound
|
|||
| Flexural Modulus | 2.60 GPa | 377 ksi | ASTM D790 |
|
Ashley Polymers Ashlene® 195-N2 Acetal
A general purpose, medium viscosity natural.Data provided by the manufacturer
|
|||
| Flexural Modulus | 2.60 GPa | 377 ksi | ASTM D790 |
|
Ashley Polymers Ashlene® 520 Nylon 66
A general purpose basic Nylon 66 resin, slightly lubricated.Data provided by the manufacturer
|
|||
| Flexural Modulus | 2.60 GPa | 377 ksi | ASTM D790 |
|
Ashley Polymers Ashlene® PC/ABS Alloy 307WO
General purpose flame retardant with high impact, good low temperature properties and high heat resistance.Data provided by the manufacturer
|
|||
| Flexural Modulus | 2.60 GPa | 377 ksi | 2 mm/min; ISO 178 |
|
SABIC Innovative Plastics LNP LUBRICOMP Cycoloy_C6303 PC+ABS
LNP* Lubricomp* Cycoloy_C6303 compound is a Wear resistant (5% PTFE), flame retardant PC+ABS. High heat and good hydrolytic stability. UL listing from Japan and Pacific.
|
|||
| Flexural Modulus | 2.60 GPa | 377 ksi | ASTM D 790 |
|
Saint-Gobain Meldin® 2030 Bearing
General Notes on Meldin 2000 Series Bearing Products:For High-Temperature, Close-Tolerance Applications. Able to withstand temperatures of 600°F with excursions to 900°F, the Medlin 2000 Series ca..
|
|||
| Flexural Modulus |
2.60
GPa <br>@Thickness 3.20 mm
|
377
ksi <br>@Thickness 0.126 in
|
15 mm/min; ASTM D790 |
|
LG Chemical XR404T ABS, Heat Resistance
Feature: Injection Molding, Heat Resistance, Curl FitApplication: Automotives Interior Housing (P/W Switch Housing Etc)CAS No. 25120-20-1, 9003-56-9, and 9001-96-2Information provided by LG Chemical..
|
|||
| Flexural Modulus |
2.60
GPa <br>@Temperature 23.0 °C
|
377
ksi <br>@Temperature 73.4 °F
|
ISO 178 |
|
DuPont Performance Polymers Delrin® FG100P NC010 Acetal Homopolymer
(Unverified Data**)
Delrin® FG100P is a high viscosity acetal homopolymer, with improved thermal stability for use in easy to fill molds. It has been developed for consideration into applications such as parts for the..
|
|||