| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.18 g/cc | 1.18 g/cc | ASTM D792 |
|
PolyOne Trilliant™ HC 5410-0030RS Natural Polyethylene, High Density (HDPE)
Information provided by PolyOne
|
|||
| Specific Gravity | 1.18 g/cc | 1.18 g/cc | ASTM D792 |
|
SABIC Innovative Plastics Cycoloy® C6840 PC+ABS
Cycoloy* C6840 resin is an injection moldable, flame retardant PC/ABS blend. It contains non-chlorinated & non-brominated flame retardant systems intended to meet governmental regulations and variou..
|
|||
| Specific Gravity | 1.18 g/cc | 1.18 g/cc | ASTM D792 |
|
SABIC Innovative Plastics Cycoloy® CX7010 PC+ABS (Asia Pacific)
Cycoloy* CX7010 resin is an injection moldable PC/ABS blend. It contains non-brominated and non-chlorinated flame retardant systems to meet UL-94 V0. Excellent flow combined with good balance of pro..
|
|||
| Specific Gravity | 1.18 g/cc | 1.18 g/cc | ASTM D792 |
|
SABIC Innovative Plastics Lexan® FXD1414T PC Copolymer (Asia Pacific)
PC-siloxane copolymer in special light diffusion colors. Medium flow. Improved toughness compared to medium flow standard PC in same color. Color package may affect performance.
|
|||
| Specific Gravity | 1.18 g/cc | 1.18 g/cc | ASTM D792 |
|
SABIC Innovative Plastics Lexan® FXM1414T PC Copolymer
PC-siloxane copolymer in special metallic colors. Medium flow. Improved toughness compared to medium flow standard PC in same color. Color package may affect performance.
|
|||
| Specific Gravity | 1.18 g/cc | 1.18 g/cc | ASTM D792 |
|
PolyOne Dynaflex™ G7680-1 (Natural) Thermoplastic Elastomer (TPE)
Dynaflex™ G7680-1 (Natural) is an easy processing, general purpose TPE designed for a wide variety of applications, including those where FDA compliance is required. - Overmold Adhesion to Polyprop..
|
|||
| Specific Gravity | 1.18 g/cc | 1.18 g/cc | ASTM D792 |
|
PolyOne Dynaflex™ G7960-1001-00 Thermoplastic Elastomer (TPE)
Dynaflex™ G7960-1001-00 is an easy processing, general purpose TPE designed for a wide variety of applications, including those where FDA compliance is required. - Overmold Adhesion to Polypropylen..
|
|||
| Specific Gravity | 1.18 g/cc | 1.18 g/cc | ASTM D792 |
|
PolyOne Geon™ Vinyl Flexible XV3725 Polyvinyl Chloride, Flexible (PVC, Flexible)
All ingredients used in the formulation of this compound are listed in the United States FDA Code of Federal Regulations, Title 21. The only restriction is that the plasticizer is For foods of high ..
|
|||
| Specific Gravity | 1.18 g/cc | 1.18 g/cc | ASTM D792 |
|
SABIC Innovative Plastics Cycoloy® C6200 PC+ABS
Non-chlorinated, nombrominated flame retardant PC/ABS offering balanced heat, flow and impact to meet various application needs.
|
|||
| Specific Gravity | 1.18 g/cc | 1.18 g/cc | ASTM D792 |
|
PolyOne Dynaflex™ G7660-1 (Natural) Thermoplastic Elastomer (TPE)
Dynaflex™ G7660-1 (Natural) is an easy processing, general purpose TPE designed for a wide variety of applications, including those where FDA compliance is required. - Overmold Adhesion to Polyprop..
|
|||
| Specific Gravity | 1.18 g/cc | 1.18 g/cc | ASTM D792 |
|
SABIC Innovative Plastics Lexan® EXL9132 PC Copolymer (Europe-Africa-Middle East)
Opaque PC-Siloxane copolymer with excellent processability. Improved flow, low temperature ductility, UV stabilized. Non-chlorinated, non-brominated flame retardant product. UL rated V0/5VA.
|
|||
| Specific Gravity | 1.18 g/cc | 1.18 g/cc | ASTM D792 |
|
Ravago Manufacturing Americas Hybrid S555 ABS + Polycarbonate Alloy
Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava..
|
|||
| Specific Gravity | 1.18 g/cc | 1.18 g/cc | |
|
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 30 PHR N774 Filler
MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje..
|
|||
| Specific Gravity | 1.18 g/cc | 1.18 g/cc | |
|
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 30 PHR N990 Filler
MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje..
|
|||
| Specific Gravity |
1.18
g/cc <br>@Temperature 23.0 °C
|
1.18
g/cc <br>@Temperature 73.4 °F
|
ASTM D792 |
|
Kingfa HF-618 Flame Retardant ABS
Features:UL 94 V-0 @ 1.6-3.0mmHigh toughnessEasy flowApplications:Injection moldingShell of applianceCD-ROMPower switchInformation Provided by Kingfa Sci. & Tech. Co., Ltd.
|
|||
| Specific Gravity | 1.18 g/cc | 1.18 g/cc | ASTM D792 |
|
LG Chemical LUPOY EC5000A PC/ABS
Description: Injection Molding, PC/ABS, General Purpose, Anti-Static.Application: E&E (Housing)Information provided by LG Chemical
|
|||
| Specific Gravity | 1.18 g/cc | 1.18 g/cc | ASTM D792 |
|
Lubrizol Advanced Materials PEARLTHANE® 11T98 Thermoplastic Polyurethane Elastomer
PEARLTHANE® 11T98 is a polycaprolactone copolyester based TPU, supplied in form of translucent, colorless pellets, combining high hardness with excellent mechanical properties. It can be extruded..
|
|||
| Specific Gravity | 1.18 g/cc | 1.18 g/cc | |
|
Momentive Performance Materials Silplusâ„¢ 70 HS High Strength Heat Cured Rubber
Heat cured rubber is a high consistency product that can be molded, extruded or calendered using conventional rubber processing equipment to meet a wide range of cost, durability and performance sta..
|
|||
| Specific Gravity | 1.18 g/cc | 1.18 g/cc | ASTM D792 |
|
LG Chemical LUPOY GN5001RF PC/ABS, Halogen Free Flame Retardant
Description: Injection Molding, PC/ABS, Halogen Free Flame Retardant, Good FlowApplication: E&E (TV, Navigation Housing)CAS: 103598-77-2, 9003-56-9 and 181028-79-5Information provided by LG Chemical..
|
|||
| Specific Gravity | 1.18 g/cc | 1.18 g/cc | ASTM D792 |
|
Samsung Cheil Industries Starex® VE-0813 ABS, Unreinforced FR
Information provided by Samsung Cheil Industries.
|
|||
| Specific Gravity | 1.18 g/cc | 1.18 g/cc | ASTM D792 |
|
Samyang Trimma® FT6120 I[R] PMMA, Transparent
High transparency and high scratch resistance. Stable against weak acids, strong acids, weak alkalis and inorganic salts.Applications: Laptop, Monitor Front Cover - for high flow, high gloss and hi..
|
|||
| Specific Gravity | 1.18 g/cc | 1.18 g/cc | ASTM D792 |
|
Lubrizol Estane® ETE 75DT3 Thermoplastic Polyurethane, Easy-to-Extrude
Type: Estane® ETE 75DT3 is an aromatic polyether-based thermoplastic polyurethane (TPU).Features: Hard TPU with wide extrusion processing window and melt stability, low temperature flexibility, hig..
|
|||
| Specific Gravity | 1.18 g/cc | 1.18 g/cc | |
|
Dow Corning Z-1221 PHENYLMETHYLDICHLOROSILANE
Information provided by Dow Corning
|
|||
| Specific Gravity | 1.18 g/cc | 1.18 g/cc | DIN 53 479 |
|
Hippe PMMA
Components made of PMMA are brilliantly transparent. Outstanding aging stability and weathering resistance. Good surface hardness. Abrasion-resistant. Physiologically safe. High strength. Easi..
|
|||
| Specific Gravity | 1.18 g/cc | 1.18 g/cc | ASTM D792 |
|
DuPont Performance Polymers Hytrel® DYM500BK TPC-ET
(Unverified Data**)
Hytrel® DYM500BK is a medium modulus polyester alloy suited for injection molding of Air Bag Deployment Doors. It has a nominal durometer hardness of 55D and contains fine particle size carbon blac..
|
|||
| Specific Gravity | 1.18 g/cc | 1.18 g/cc | |
|
Colorite Polymers Vinylbond 95-950-65 PVC Compound
Description: Vinylbond 95-950 series compounds are flexible PVC alloys which are formulated specifically for the window market industry. These compounds offer excellent bonding characteristics to ri..
|
|||
| Specific Gravity | 1.18 g/cc | 1.18 g/cc | ASTM D792 |
|
C.O.I.M. LARIPUR® LPR5850 Modified Ester Polyurethane
Description: The products of the LARIPUR® line are thermoplastic polyurethanes. These products combine the technology of thermoplastic products with the features of polyurethanes:Excellent abrasion..
|
|||
| Specific Gravity | 1.18 g/cc | 1.18 g/cc | 23°C; ASTM D792 |
|
Teknor Apex APEX® 1700-50 Polyvinyl Chloride, Flexible
Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMFeatures-General Purpose, Low Gloss Uses-Appliance Components, Footwear, FurnitureForms-PelletsProcessing Met..
|
|||
| Specific Gravity | 1.18 g/cc | 1.18 g/cc | ASTM D792 |
|
PolyOne Syncure™ System S117FH Polyethylene, Crosslinked (XLPE)
NOTE: The above represents Typical Properties measured on 20 AWG with 16 mil wall. STORAGE AND HANDLING: Use within 48 hours once package is open to avoid self-curing and scrap.Information provided ..
|
|||