Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 30.0 kV/mm | 762 kV/in | |
Plastcom SLOVASTER® B GF 6 FRL 4 PBT, 6% glass fibre, flame retarder FeaturesPBT with the content of 6 % chemically bound glass fibre and with the flame retardant on the basis of bromine hydrocarbons. Anisotropy of shrinkage enables the injection moulding of round, c.. |
|||
Dielectric Strength | 30.0 kV/mm | 762 kV/in | Dry; IEC 60243 |
Polimeri Europa Sinkral® B 532/E ABS Resin Sinkral B 532/E is an extrusion grade, which combines high toughness with good rigidity. Its rheological characteristics and good thermal stability are required for the production of large extruded .. |
|||
Dielectric Strength | 30.0 kV/mm | 762 kV/in | |
Polimeri Europa SINKRAL B153/V4 ABS, Heat Stabilized, 17% Glass Fiber
(discontinued **) Symbol according to ISO 1043-1-2: ABS (GF) Grade designation according to ISO 2580-ABS 1,MG,105-04-09-30,GF15 17% glass fibre reinforced injection moulding grade, with high stiffness and good proc.. |
|||
Dielectric Strength | 30.0 kV/mm | 762 kV/in | |
Polimeri Europa SINKRAL B633/E ABS, Impact & Heat Stabilized Grade
(discontinued **) Symbol according to ISO 1043-1: ABS Grade designation according to ISO 2580-ABS 1,EG,105-04-25-20 High impact extrusion grade with excellent stiffness, good processability and high thermal stabili.. |
|||
Dielectric Strength | 30.0 kV/mm | 762 kV/in | |
Covestro Bayblend® R-FR 390 Polycarbonate/ABS Blend
(discontinued **) FR-recycled grades with variable recycled content.Applications: Housings for office equipment, electrical engineering, computer sectors.Information provided by Bayer.As of 1 September 2015, Bayer Ma.. |
|||
Dielectric Strength | 30.0 kV/mm | 762 kV/in | IEC 60243-1 |
Menzolit Menzolit® BMC 0410 Unsaturated Polyester UP BMC 0410 is a low profile BMC with zero shrinkage and low coefficient of thermal expansion. It is especially suited for precision mouldings in office and communication equipment. The combination of .. |
|||
Dielectric Strength | 30.0 kV/mm | 762 kV/in | Conditioned; IEC 60243-1 |
Lanxess Durethan® A 30 S 000000 Nylon 66 PA 66 standard injection molding-grade, non-reinforced, good demolding, very rapid solidificationApplication Examples: plug connectors, terminal blocks, cable clips, bobbins |
|||
Dielectric Strength | 30.0 kV/mm | 762 kV/in | JIS K2111 |
Toyobo PELPRENE™ P90BD Polyester TPE, High Viscous, High Durability Features: Polyester TPE, High Viscous, High DurabilityInformation provided by Toyobo. |
|||
Dielectric Strength | 30.0 kV/mm | 762 kV/in | VDE 0303/4 |
Polyram RamTough PZ300G3 Polycarbonate, 15% Glass Fiber 15% Glass fiber reinforced polycarbonate for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Dielectric Strength | 30.0 kV/mm | 762 kV/in | IEC 60250 |
Polyram RamTough PZ305G4 Polycarbonate, 20% Glass Fiber 20% glass fiber reinforced polycarbonate for injection molding applications.Information provided by Polyram. |
|||
Dielectric Strength | 30.0 kV/mm | 762 kV/in | ASTM D149 |
Chengdu Polyster KLX-G42 PC Film & Sheet PC film, high transparency, one side is velvet the other side is matte.Information provided by Chengdu Polyster Co., Ltd. |
|||
Dielectric Strength | 30.0 kV/mm | 762 kV/in | |
Covestro Apec® HT KU 1-9354 High-Heat Polycarbonate Only opaque colors available, flame retardant.Applications: Lighting, electrical parts.Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and off.. |
|||
Dielectric Strength | 30.0 kV/mm | 762 kV/in | IEC 60243-1 |
DSM Akulon® K224-LGM35 (Cond.) 15% Glass Reinforced, 25% Mineral Reinforced Nylon 6 (North America) Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis.. |
|||
Dielectric Strength | 30.0 kV/mm | 762 kV/in | IEC 60243-1 |
DSM Akulon® S223-G4U (Cond.) 23% Glass Reinforced Nylon 66 (North America) Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis.. |
|||
Dielectric Strength | 30.0 kV/mm | 762 kV/in | |
Covestro Makrolon® 2405 Polycarbonate, Injection Grade Very easy flowing injection molding grade with easy mold release, Makrolon grade 2458 for food contact applications.Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience was se.. |
|||
Dielectric Strength | 30.0 kV/mm | 762 kV/in | |
Covestro Makrolon® 6385 Polycarbonate, Injection Grade Low viscosity, flame retardant injection molding grade with easy mold release, not available in transparent colors.Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience was sep.. |
|||
Dielectric Strength | 30.0 kV/mm | 762 kV/in | No thickness given |
ConocoPhillips Hydroclear® 1 Ultra-clean multi-purpose R&O Oil, AGMA Lubricant No. 1 Description: Conoco Hydroclear Ultra-Clean Multipurpose R&O Oil is a rust- and oxidation-inhibited industrial oil with ashless wear protection formulated from premium Conoco hydrocracked base stocks.. |
|||
Dielectric Strength | 30.0 kV/mm | 762 kV/in | |
Covestro Makrolon® KU 1-1216 Polycarbonate, UV-Stabilized UV-stabilized injection molding grade, good flow, suitable for spectacle glasses (LQ = Lens-Quality).Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience was separated from Ba.. |
|||
Dielectric Strength | 30.0 kV/mm | 762 kV/in | |
Arkema Group Rilsan® Powder ESY Black X 7260 Nylon 11, Coating Grade Powder ESY BLACK X 7260 - RILSAN POLYAMIDE 11 (PA11) POWDERMelt mix black powder for coating of metallic parts by electrostatic spray, and post fused in an oven.There is a wide range of colors.The p.. |
|||
Dielectric Strength | 30.0 kV/mm | 762 kV/in | IEC 60243 |
Azoty Tarnow™ TARNOFORM 300 GF7 POM 35% glass fiber reinforced injection molding grade, suitable for applications where increased strength and stiffness is required.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A... |
|||
Dielectric Strength | 30.0 kV/mm @Thickness 2.00 mm |
762 kV/in @Thickness 0.0787 in |
Short time; ASTM D149 |
Asahi Kasei Xyron® SZ800 Modified Polyphenylene Ether High-Heat ResistantInformation provided by Asahi Kasei |
|||
Dielectric Strength | 30.0 kV/mm | 762 kV/in | in transformer oil; IEC 60243-1 |
CENTROPLAST CENTRO HPM Polysulfone This plastic has good hydrolysis, chemical and radiation resistance, and can operate at high temperatures. It is used in food processing industry, pumps and valves, and medical equipment.Informatio.. |
|||
Dielectric Strength | 30.0 kV/mm | 762 kV/in | dry; IEC 243-1 |
Azoty Tarnow™ Tarnamid® T-27 MCS 850 Polyamide 6 - Flame Retarded, Unreinforced Glow wire resistance 850°C, bromine and red phosphorus free, medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.Tarnamid® has .. |
|||
Dielectric Strength | 30.0 kV/mm | 762 kV/in | IEC 243-1 |
Azoty Tarnow™ Tarnamid® T-27 MHLS Polyamide 6 - Colored Heat and UV light stabilized grade. Medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.Tarnamid® has the following main proper.. |
|||
Dielectric Strength | 30.0 kV/mm | 762 kV/in | No thickness given. |
ConocoPhillips Hydroclear® 3 Ultra-clean multi-purpose R&O Oil, AGMA Lubricant No. 3 Description: Conoco Hydroclear Ultra-Clean Multipurpose R&O Oil is a rust- and oxidation-inhibited industrial oil with ashless wear protection formulated from premium Conoco hydrocracked base stocks.. |
|||
Dielectric Strength | 30.0 kV/mm | 762 kV/in | IEC 243-1 |
CP-Polymer-Technik Wellamid® 6600 HWCP Nylon 66, Heat Stabilized, Dry Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Dielectric Strength | 30.0 kV/mm | 762 kV/in | conditioned; IEC 60243-1 |
EMS-Grivory Grivory® HT1V-3 HY black 9205 PA6T/6I-GF30 Product description: Grivory HT1V-3 HY black 9205 is a 30% glass fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. Grivory HT1V-3 HY bl.. |
|||
Dielectric Strength | 30.0 kV/mm | 762 kV/in | |
Polimeri Europa SINKRAL F233 ABS, Heat Stabilized
(discontinued **) Symbol according to ISO 1043-1: ABS Grade designation according to ISO 2580-ABS 1,MG,105-15-16-25 Medium heat injection moulding grade having high flow and good thermal stability during processing.. |
|||
Dielectric Strength | 30.0 kV/mm | 762 kV/in | |
Polimeri Europa KOBLEND PCA 53 PC+ABS
(discontinued **) Symbol according to ISO 1043/1: PC+ABS Injection moulding grade with flame retardant properties ( UL 94 V-0 at 1.6mm thickness ) and good light resistance. Vicat/B50 = 110°C Main application fiel.. |
|||
Dielectric Strength | 30.0 kV/mm @Thickness 1.00 mm |
762 kV/in @Thickness 0.0394 in |
IEC 60243-P1 |
Hexion Bakelite™ PF 4155 Phenolic Formaldehyde Resin, Resistant to High Temperatures, Improved Electrical Properties, Low Shrinkage, High Mechanical Strength Phenolic molding compound, inorganically filled, glass fiber reinforced, good media and temperature resistance. Conditioned Cu-adhesion.Application areas: Commutators (fuel pumps, actuators, starte.. |