Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Strength, Yield = 42.2 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 42.2 MPa
6120 psi
ASTM D638
Hyosung Topilene HJ700 PP
HJ700 High Isostatic PP HomopolymerApplications:CompoundingElectric applianceAutomobile partsCharacteristics:High stiffnessHeat resistanceInformation provided by Hyosung Corporation
Tensile Strength, Yield 42.2 MPa

@Thickness 3.20 mm
6120 psi

@Thickness 0.126 in
50 mm/min; ASTM D638
LG Chemical AF312B ABS, Flame Retardant
Feature: Injection Molding, Flame RetardantApplication: Electric/Electronic Applications (TV, Monitor Housing) IT/OA deviceCAS No. 9003-56-9, 79-94-7 and 1309-64-4Information provided by LG Chemical..
Tensile Strength, Yield 42.2 MPa

@Thickness 3.20 mm
6120 psi

@Thickness 0.126 in
50 mm/min; ASTM D638
LG Chemical AF312C ABS, Flame Retardant
Feature: Injection Molding, Flame RetardantApplication: Electric/Electronic Applications (TV, Monitor Housing) IT/OA deviceCAS No. 9003-56-9, 79-94-7 and 1309-64-4Information provided by LG Chemical..
Tensile Strength, Yield 42.2 MPa

@Thickness 3.20 mm
6120 psi

@Thickness 0.126 in
50 mm/min; ASTM D638
LG Chemical AF312T ABS, Flame Retardant
Feature: Injection Molding, Flame RetardantApplication: Electric/Electronic Applications (TV, Monitor Housing) IT/OA deviceCAS No. 9003-56-9, 79-94-7 and 1309-64-4Information provided by LG Chemical..
Tensile Strength, Yield 42.2 MPa

@Thickness 3.20 mm
6120 psi

@Thickness 0.126 in
50 mm/min; ASTM D638
LG Chemical AF360S ABS, TBBA-free Flame Retardant, Low Flow
Feature: Injection Molding, TBBA-free Flame Retardant, Low FlowApplication: Electric/Electronic Applications (TV, Monitor Housing) IT/OA deviceCAS No. 9003-56-9, 84852-53-9 and 1309-64-4Information ..
Tensile Strength, Yield 42.2 MPa

@Thickness 3.20 mm
6120 psi

@Thickness 0.126 in
50 mm/min; ASTM D638
LG Chemical HF380NS ABS, High Flow, General Anti-Static
Feature: Injection Molding, High Flow, General Anti-StaticApplication: Electric & Electronic Products, Miscellaneous goods)CAS No. 9003-56-9Information provided by LG Chemical
Tensile Strength, Yield 42.2 MPa

@Thickness 3.20 mm
6120 psi

@Thickness 0.126 in
50 mm/min; ASTM D638
LG Chemical TR300 MABS, Flame Retardant, Transparency
Feature: Injection Molding, Flame Retardant, TransparencyApplication: Electric/Electronic Applications (TV, Monitor Housing) IT/OA deviceCAS No. 9010-94-0 and 25713-60-4Information provided by LG Ch..
Tensile Strength, Yield 42.2 MPa

@Thickness 3.20 mm
6120 psi

@Thickness 0.126 in
50 mm/min; ASTM D638
LG Chemical MA221 ABS, High Impact, Low Gloss
Feature: Injection Molding, Extrusion Molding, High Impact, Low GlossApplication: Automotive Sheet, Semi-Conductor TrayCAS No. 9003-56-9Information provided by LG Chemical
Tensile Strength, Yield 42.2 MPa
6120 psi
50 mm/min; ASTM D638
Samsung Cheil Industries Starex® BM-0320 J ABS, Unreinforced
Heat resistantInformation provided by Samsung Cheil Industries.
Tensile Strength, Yield 42.2 MPa
6120 psi
5 mm/min; ASTM D638
Samsung Cheil Industries Starex® CM-0140UV ABS, Unreinforced
Information provided by Samsung Cheil Industries.
Tensile Strength, Yield 42.2 MPa
6120 psi
5 mm/min; ASTM D638
Samsung Cheil Industries Starex® SF-0950S MABS, Unreinforced Scratch Resistant
Information provided by Samsung Cheil Industries.
Tensile Strength, Yield 42.2 MPa
6120 psi
5 mm/min; ASTM D638
Samsung Cheil Industries Starex® SR-0320BM ABS, Unreinforced Heat Resistant
Information provided by Samsung Cheil Industries.
Tensile Strength, Yield 42.2 MPa
6120 psi
5 mm/min; ASTM D638
Samsung Cheil Industries Starex® WR-9700S ASA, Unreinforced
Used in golf cart roof etc.Information provided by Samsung Cheil Industries.
Tensile Strength, Yield 42.2 MPa
6120 psi
5 mm/min; ASTM D638
Samsung Cheil Industries Starex® WX-9700 ASA, Unreinforced Extrusion Grade
Information provided by Samsung Cheil Industries.
Tensile Strength, Yield 42.2 MPa
6120 psi
50 mm/min; ASTM D638
Samsung Cheil Industries Starex® BM-0320 J ABS, Unreinforced
Heat resistantInformation provided by Samsung Cheil Industries.
Tensile Strength, Yield 42.2 MPa
6120 psi
5 mm/min; ASTM D638
Samsung Cheil Industries Starex® CM-0140UV ABS, Unreinforced
Information provided by Samsung Cheil Industries.
Tensile Strength, Yield 42.2 MPa
6120 psi
5 mm/min; ASTM D638
Samsung Cheil Industries Starex® SR-0320BM ABS, Unreinforced Heat Resistant
Information provided by Samsung Cheil Industries.
Tensile Strength, Yield 42.2 MPa
6120 psi
5 mm/min; ASTM D638
Samsung Cheil Industries Starex® WR-9700S ASA, Unreinforced
Used in golf cart roof etc.Information provided by Samsung Cheil Industries.
Tensile Strength, Yield 42.2 MPa
6120 psi
ASTM D412
C.O.I.M. LARIPUR® LPR7560 PTMG Polyether Polyurethane
Description: The products of the LARIPUR® line are thermoplastic polyurethanes. These products combine the technology of thermoplastic products with the features of polyurethanes:Excellent abrasion..
Tensile Strength, Yield 42.2 MPa

@Thickness 3.20 mm
6120 psi

@Thickness 0.126 in
Type 1, 5 mm/min; ASTM D-638
Bhansali Engineering Abstron HR-105 ABS Super Heat Resistant
High Heat Resistant Grades with Better Flow characteristicInformation provided by Bhansali
Tensile Strength, Yield 42.2 MPa

@Thickness 3.20 mm
6120 psi

@Thickness 0.126 in
Type 1, 5 mm/min; ASTM D-638
Bhansali Engineering Abstron HR-59(M) ABS Heat Resistant
High, Medium Impact Heat Resistant Grades with good flowInformation provided by Bhansali
Tensile Strength, Yield 42.2 MPa

@Thickness 3.20 mm
6120 psi

@Thickness 0.126 in
Type I, 5 mm/min; ASTM D638
Bhansali Engineering Abstron IM17A TT ABS Injection Molding Grade
High Flow, Medium ImpactInformation provided by Bhansali
Tensile Strength, Yield 42.2 MPa

@Thickness 3.20 mm
6120 psi

@Thickness 0.126 in
Type I, 5 mm/min; ASTM D638
Bhansali Engineering Abstron IMC25 ABS-PC Alloy
Medium FlowInformation provided by Bhansali
Tensile Strength, Yield 42.2 MPa

@Thickness 3.20 mm
6120 psi

@Thickness 0.126 in
Type I, 5 mm/min; ASTM D638
Bhansali Engineering Abstron TIM 300 MMA- ABS
High Impact(Transparent ABS)Information provided by Bhansali
Tensile Strength, Yield 42.2 MPa

@Thickness 3.20 mm
6120 psi

@Thickness 0.126 in
Type I, 5 mm/min; ASTM D638
Bhansali Engineering Abstron TIM 300 MMA- ABS
High Impact(Transparent ABS)Information provided by Bhansali
Tensile Strength, Yield 42.2 MPa
6120 psi
at 300% elongation; ASTM D412
Lubrizol Estane® S375D Thermoplastic Polyurethane
Type: Estane® S375D is a Shore 78D, polyester based thermoplastic polyurethane (TPU) with excellent transparency. FDA approved (21 CFR 177.2600, 177.1680).Uses: Injection Molding.Availability: Asi..
Tensile Strength, Yield 42.2 MPa

@Thickness 3.20 mm
6120 psi

@Thickness 0.126 in
Type 1, 5 mm/min; ASTM D-638
Bhansali Engineering Abstron HR-105 ABS Super Heat Resistant
High Heat Resistant Grades with Better Flow characteristicInformation provided by Bhansali
Tensile Strength, Yield 42.2 MPa

@Thickness 3.20 mm
6120 psi

@Thickness 0.126 in
Type I, 5 mm/min; ASTM D638
Bhansali Engineering Abstron KU600N ABS Heat Resistant
High ImpactInformation provided by Bhansali
Tensile Strength, Yield 42.2 MPa

@Thickness 3.20 mm
6120 psi

@Thickness 0.126 in
Type I, 5 mm/min; ASTM D638
Bhansali Engineering Abstron IM17A TT ABS Injection Molding Grade
High Flow, Medium ImpactInformation provided by Bhansali
Tensile Strength, Yield 42.2 MPa

@Thickness 3.20 mm
6120 psi

@Thickness 0.126 in
Type I, 5 mm/min; ASTM D638
Bhansali Engineering Abstron IMC25 ABS-PC Alloy
Medium FlowInformation provided by Bhansali
Copyright © lookpolymers.com All Rights Reserved