Material Notes:
A high purity, ultrafine, wet ground natural calcium carbonate available in dry or slurry form.Applications: Plastic applications such as rigid PVC and flexible PVC. Paint applications such as water based, solvent based, and high gloss powder coatings.Information supplied by Omya North America.
Physical Properties Metric English Comments
Specific Gravity 1.90 g/cc
1.90 g/cc
Slurry
2.70 g/cc
2.70 g/cc
dry
Density 1.898 g/cc
0.06857 lb/in³
Slurry
Solids Content 75 %
75 %
Slurry
Brightness 96 %
96 %
Y - Brightness (dry)
Moisture Absorption at Equilibrium 0.070 %
0.070 %
Moisture Loss at 110°C % (dry)
Particle Size 1.4 µm
1.4 µm
Median Diameter
Specific Surface Area 7.0 m²/g
7.0 m²/g
Brookfield Viscosity 200 cP
200 cP
dry
Optical Properties Metric English Comments
Refractive Index 1.57
1.57
dry
Descriptive Properties Value Comments
Calcium Carbonate % 98
FDA 21 CFR 174.5, 175.300, 178.3297
Hegman (dry) 6
Magnesium Carbonate % 1
Percent Finer than 1 Microns 40
Percent Finer than 2 Microns 60
Pounds Pigment/gallon (slurry) 11.88
Pounds Pigment/Solid Gallon (dry) 22.6
Retained in 325 mesh (dry) ppm 7