Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Ascend Performance Materials Vydyne® R633 Nylon 66 Copolymer, 33% Glass Filled, Dry as Molded

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, 30% Glass Fiber Filled
Manufacturer Ascend Performance Materials (formerly Solutia)
Trade Name VYDYNE®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ascend Performance Materials Vydyne® R633 Nylon 66 Copolymer, 33% Glass Filled, Dry as Molded.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Vydyne® R633 is 33% glass-fiber reinforced, PA66/6 copolymer resin for superior surface appearance. Available in natural, this injection-molding grade resin is lubricated for machine feed and mold release. Vydyne R633 has tensile strength and modulus properties just below aluminum and zinc and can replace these metals in numerous applications due to an excellent balance of properties. Reduction in production costs, energy/consumption, and part weight are key advantages of Vydyne glass-reinforced PA66/6 resins over aluminum and/or zinc die-cast parts. Typical Applications/End Uses: Vydyne R633 has been used for many under-the-hood automotive applications, motor housings for power tools, and garden appliances. These resins have also been used in miscellaneous brackets, gears and clips that require high rigidity and strength.Availability:Asia PacificEuropeNorth AmericaAdditive: Lubricant Features:CopolymerGood Mold ReleaseGood Surface FinishHigh RigidityHigh StrengthHigh Tensile Strength LubricatedUses:GearsHousingsLawn and Garden EquipmentMetal ReplacementPower/Other ToolsAppearance: Natural ColorForms: PelletsProcessing Method: Injection Molding
Physical Properties Metric English Comments
Specific Gravity 1.39 g/cc
1.39 g/cc
ISO 1183
Water Absorption 1.3 %

@Time 86400 sec
1.3 %

@Time 24.0 hour
ISO 62
Moisture Absorption at Equilibrium 2.3 %
2.3 %
50% RH; ISO 62
Linear Mold Shrinkage 0.0040 cm/cm

@Thickness 2.00 mm
0.0040 in/in

@Thickness 0.0787 in
ISO 294-4
Linear Mold Shrinkage, Transverse 0.0090 cm/cm

@Thickness 2.00 mm
0.0090 in/in

@Thickness 0.0787 in
ISO 294-4
Mechanical Properties Metric English Comments
Tensile Strength at Break 184 MPa
26700 psi
ISO 527-2
Elongation at Break 4.0 %
4.0 %
ISO 527-2
Tensile Modulus 10.8 GPa
1570 ksi
ISO 527-2
Flexural Strength 255 MPa
37000 psi
ISO 178
Flexural Modulus 8.80 GPa
1280 ksi
ISO 178
Poissons Ratio 0.42
0.42
ISO 527-2
Izod Impact, Notched (ISO) 13.0 kJ/m²
6.19 ft-lb/in²
ISO 180
12.0 kJ/m²

@Temperature -30.0 °C
5.71 ft-lb/in²

@Temperature -22.0 °F
ISO 179
Charpy Impact Unnotched 4.40 J/cm²

@Temperature -30.0 °C
20.9 ft-lb/in²

@Temperature -22.0 °F
ISO 179
5.10 J/cm²

@Temperature 23.0 °C
24.3 ft-lb/in²

@Temperature 73.4 °F
ISO 179
Charpy Impact, Notched 1.10 J/cm²

@Temperature -30.0 °C
5.24 ft-lb/in²

@Temperature -22.0 °F
ISO 179
1.20 J/cm²

@Temperature 23.0 °C
5.71 ft-lb/in²

@Temperature 73.4 °F
ISO 179
Thermal Properties Metric English Comments
CTE, linear 1.50 µm/m-°C

@Thickness 2.00 mm,
Temperature 23.0 - 55.0 °C
0.833 µin/in-°F

@Thickness 0.0787 in,
Temperature 73.4 - 131 °F
ISO 11359-2
CTE, linear, Transverse to Flow 10.0 µm/m-°C

@Thickness 2.00 mm,
Temperature 23.0 - 55.0 °C
5.56 µin/in-°F

@Thickness 0.0787 in,
Temperature 73.4 - 131 °F
ISO 11359-2
Melting Point 233 °C
451 °F
ISO 11357-3
Deflection Temperature at 0.46 MPa (66 psi) 230 °C
446 °F
ISO 75-2/B
Deflection Temperature at 1.8 MPa (264 psi) 220 °C
428 °F
ISO 75-2/A
UL RTI, Mechanical with Impact 65.0 °C

@Thickness 3.00 mm
149 °F

@Thickness 0.118 in
UL 746B
Processing Properties Metric English Comments
Processing Temperature 285 - 305 °C
545 - 581 °F
Melt
Rear Barrel Temperature 280 - 310 °C
536 - 590 °F
Middle Barrel Temperature 280 - 310 °C
536 - 590 °F
Front Barrel Temperature 280 - 310 °C
536 - 590 °F
Nozzle Temperature 280 - 310 °C
536 - 590 °F
Mold Temperature 65.0 - 95.0 °C
149 - 203 °F
Drying Temperature 80.0 °C
176 °F
Dry Time 4.00 hour
4.00 hour
Descriptive Properties Value Comments
Suggested Max Regrind 25%