| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.39 g/cc | 1.39 g/cc | ASTM D792 |
|
PolyOne Geon™ Vinyl Wire & Cable MJF114A Polyvinyl Chloride, Flexible (PVC, Flexible)
Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne
|
|||
| Specific Gravity | 1.39 g/cc | 1.39 g/cc | ASTM D792 |
|
PolyOne Nymax™ ND 1233 GF Natural Polyamide 66 (Nylon 66)
The Nymax® GF 1200 Series of glass fiber-reinforced nylon 6/6 compounds have been specifically formulated for applications requiring high stiffness, tensile properties, heat resistance, and durabil..
|
|||
| Specific Gravity | 1.39 g/cc | 1.39 g/cc | ASTM D-792 |
|
PlastiComp Velocity® LCF50-PA6 High Flow Nylon 6, 50% Long Carbon Fiber
This compound complies with European Union Directive 2002/95/EC Restriction of Hazardous Substances (RoHS).Information provided by PlastiComp, Inc.
|
|||
| Specific Gravity | 1.39 g/cc | 1.39 g/cc | ASTM D792 |
|
Ravago Manufacturing Americas Hylon® N1233HL BK Nylon 6/6
Available in North America Filler: Glass Fiber Reinforcement, 33% Filler by WeightAdditive: Heat Stabilizer and Lubricant Features: Lubricated and Heat StabilizedRoHS CompliantAuto Specifications: ..
|
|||
| Specific Gravity | 1.39 g/cc | 1.39 g/cc | ASTM D3763 |
|
Parker Chomerics PREMIER™ A230-FRHF EMI Shielding Plastic
Description: PREMIER™ is the world’s first and most versatile commercially available conductive thermoplastic for real world EMI shielding solutions. It is a blend of PC/ABS thermoplastic polymer ..
|
|||
| Specific Gravity | 1.39 - 1.41 g/cc | 1.39 - 1.41 g/cc | PEPL-10-W-21 |
|
Pearl Engineering PEPLPET B-07C PET Bottle Grade
A co-polymer used mostly for containers.
|
|||
| Specific Gravity | 1.39 g/cc | 1.39 g/cc | ASTM D792 |
|
Kolon KOCETAL® UR302 Toughened Grade Acetal Resin
TPU added, improved toughness. Applications: Impact resistant, flexible products. Information provided by API-Kolon
|
|||
| Specific Gravity | 1.39 g/cc | 1.39 g/cc | ISO 1183 |
|
Lanxess Pocan® TP 740-202 901510 PBT+ASA, 20% Glass Fiber
PBT + ASA, 20% glass fibers, injection molding, low tendency to warp, improved surface finishInformation provided by LANXESS.
|
|||
| Specific Gravity | 1.39 g/cc | 1.39 g/cc | ASTM D792 |
|
Teknor Apex APEX® 4130 Polyvinyl Chloride, Flexible
Notes: 75°C Jacket; RoHS Compliant Features: Good UV Resistance; Sunlight Resistant (720 hours) Uses: Flexible Cord Jacketing Forms: Pellets Agency Ratings: UL QMTT2 .E73402 Wire Types: SJTW; STW..
|
|||
| Specific Gravity | 1.39 g/cc | 1.39 g/cc | ASTM D792 |
|
SABIC Innovative Plastics LNP THERMOCOMP RX06421S PA 66
LNP* Thermocomp* RX06421S is a compound based on Nylon 66 resin containing Glass Fiber. Added features of this material include: Easy Molding.
|
|||
| Specific Gravity | 1.39 g/cc | 1.39 g/cc | ASTM D792 |
|
SABIC Innovative Plastics LNP THERMOCOMP EC006APQ PEI
LNP* Thermocomp EC006APQ is a compound based on Polyetherimide containing 30% Carbon Fiber. Added features include: Electrically Conductive, High Flow.
|
|||
| Specific Gravity | 1.39 g/cc | 1.39 g/cc | ASTM D792 |
|
Chase Plastics CP Pryme® N233GL (DAM) Nylon 6, 33% Glass Fiber Reinforced, Internally Lubricated
Information provided by Chase Plastics.
|
|||
| Specific Gravity | 1.39 g/cc | 1.39 g/cc | ASTM D792 |
|
Chase Plastics CP Pryme® N333GL (COND, 50% RH) Nylon 6 (Utility Grade), 33% Glass Fiber Reinforced, Internally Lubricated
Information provided by Chase Plastics.
|
|||
| Specific Gravity | 1.39 g/cc | 1.39 g/cc | ASTM D792 |
|
A. Schulman POLYBATCH™ Navajo 10275U/4 Concentrate Based In LDPE
DescriptionPOLYBATCH® 10275U/4 is a navajo color concentrate containing an optimized blend of color and UV stabilizer based in LLDPE. This concentrate was designed to provide color and UV stabili..
|
|||
| Specific Gravity | 1.39 g/cc | 1.39 g/cc | ASTM D792 |
|
A. Schulman POLYBATCH™ Blue 4535 Concentrate Based In Polyethylene
DescriptionPOLYBATCH® 4535 is a blue color concentrate based in polyethylene . This concentrate was designed to provide color in polyolefin film and molding applications. POLYBATCH® 4535 is typi..
|
|||
| Specific Gravity | 1.39 g/cc | 1.39 g/cc | ASTM D792 |
|
A. Schulman SCHULAMID® 6 GF35 35% Glass Fiber Reinforced Nylon 6
Information provided by A. Schulman.
|
|||
| Specific Gravity | 1.39 g/cc | 1.39 g/cc | ASTM D792 |
|
A. Schulman SCHULAMID® 6 GF35 35% Glass Fiber Reinforced Nylon 6
Information provided by A. Schulman.
|
|||
| Specific Gravity | 1.39 g/cc | 1.39 g/cc | ASTM D792 |
|
Diamond Polymers NPP 60-3301 Clear Polyester Copolymer
Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc.
|
|||
| Specific Gravity | 1.39 g/cc | 1.39 g/cc | ASTM D792 |
|
Colorite Polymers CS8039UL Non Lead Wire and Cable Vinyl Compound
Description: Colorite specialty wire and cable compounds feature low smoke properties, excellent flame retardance, low temperature flexibility, and resistance to abrasion and chemicals. All are avai..
|
|||
| Specific Gravity | 1.39 g/cc | 1.39 g/cc | ASTM D792 |
|
Colorite Polymers CS9039GP Wire and Cable Insulation Vinyl Compound
Description: Colorite specialty wire and cable compounds feature low smoke properties, excellent flame retardance, low temperature flexibility, and resistance to abrasion and chemicals. All are avai..
|
|||
| Specific Gravity | 1.39 - 1.43 g/cc | 1.39 - 1.43 g/cc | ASTM D-792 |
|
Axiall 13821 Wire & Cable Flexible PVC
Non-lead stabilized, 720 hour sunlight resistant, TW insulation compound also recommended for 75C Class 43 applications or outdoor jacket applications.Information provided by Georgia GulfGeorgia Gul..
|
|||
| Specific Gravity | 1.39 g/cc | 1.39 g/cc | Dry; ASTM D792 |
|
Asahi Kasei Leona® 90G33 33% Glass Filled Nylon 66
Enhanced strength and stiffness; with 33% GF. Superior fluidity and appearance.Applications:Automotive parts Information provided by Asahi Kasei
|
|||
| Specific Gravity | 1.39 g/cc | 1.39 g/cc | ASTM D792 |
|
Teknor Apex APEX® 80118-Y Polyvinyl Chloride, Flexible
Notes: 60°C Insulation; RoHS Compliant Features: Good UV Resistance Uses: Cable Jacketing; InsulationAgency Ratings: UL 1063; UL 1581; UL 62; UL 83 Forms: Pellets Wire Types: TWInformation Provided..
|
|||
| Specific Gravity | 1.39 g/cc | 1.39 g/cc | DAM; ASTM D792 |
|
DuPont Performance Polymers Zytel® 74G33W BK196 Nylon 66
(Unverified Data**)
Zytel® 74G33W BK196 is a high gloss automotive weatherable black 33% glass reinforced nylon 66 and nylon 6 comelt resin.Information provided by DuPont Performance Polymers
|
|||
| Specific Gravity | 1.39 g/cc | 1.39 g/cc | ASTM D792 |
|
PolyOne Geon™ Vinyl Wire & Cable W1100L-xx92FRD Polyvinyl Chloride, Flexible (PVC, Flexible)
Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications. Provisional Product Information - Physical and Mechanical properties based on initial production.Information provide..
|
|||
| Specific Gravity | 1.39 g/cc | 1.39 g/cc | ASTM D792 |
|
PolyOne Geon™ Vinyl Wire & Cable 1721-xx14E Polyvinyl Chloride, Flexible (PVC, Flexible)
Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne
|
|||
| Specific Gravity | 1.39 g/cc | 1.39 g/cc | ASTM D792 |
|
PolyOne Edgetek® UR-20GF/000 Thermoplastic Elastomer - TPU, Glass Filled
(discontinued **)
Description/Features:Glass Fiber ReinforcedUL 94 HBPolyOne First ChoiceInformation provided by PolyOne Corporation.
|
|||