Polymer Property : Charpy Impact, Notched = 5.71 ft-lb/in² Product List

Mechanical Properties

Tips: 30 items are displayed at most.
Mechanical Properties Metric English Comments
Charpy Impact, Notched 1.20 J/cm²
<br>@Temperature -20.0 °C
5.71 ft-lb/in²
<br>@Temperature -4.00 °F
Plastcom SLOVAMID 66 GF 20 GB 10 HI PA66, improved strength
FeaturesModified with thermoplastic reactive caoutchouc, determined for mouldings with high toughness also at minus temperatures. Eligible application for ski-shoes, helmets for sport and other safe..
Charpy Impact, Notched 1.20 J/cm²
<br>@Temperature -20.0 °C
5.71 ft-lb/in²
<br>@Temperature -4.00 °F
ISO 179
Polykemi AB POLYabs P0P ABS, Plating Grade
Information provided by Polykemi AB
Charpy Impact, Notched 1.20 J/cm²
<br>@Temperature 23.0 °C
5.71 ft-lb/in²
<br>@Temperature 73.4 °F
ISO 179
Polykemi AB POLYfill PPHC GF3030 PD2 Polypropylene, Glass Fibre-Reinforced, Chemically Coupled
Information provided by Polykemi AB
Charpy Impact, Notched 1.20 J/cm²
<br>@Temperature -30.0 °C
5.71 ft-lb/in²
<br>@Temperature -22.0 °F
V-notch Edgew 80*10*3 sp=62mm; ISO 179/1eA
SABIC Innovative Plastics Lexan® 4301 PPC+PC (Asia Pacific)
Lexan 4301 is a high heat resistant poly (ester) carbonate resin for injection moldingThis data was supplied by SABIC-IP for the Asia Pacific region.
Charpy Impact, Notched 1.20 J/cm²
<br>@Temperature -30.0 °C
5.71 ft-lb/in²
<br>@Temperature -22.0 °F
Radici Radilon® A RV300RKC (cond.) Nylon 66
Radilon® A is a range of polyamide 66 (PA66) products obtained through the polymerization of hexamethylendiamine and adipic acid, and used for injection, extrusion and blow-molding.Information prov..
Charpy Impact, Notched 1.20 J/cm²
<br>@Temperature 23.0 °C
5.71 ft-lb/in²
<br>@Temperature 73.4 °F
50%RH; ISO 179/1eA
DuPont Performance Polymers Zytel® 79G13HSL BK039 Nylon 66 &nbsp;(Unverified Data**)
Zytel® 79G13HSL BK039 is a 13 % glass reinforced, heat stabilized, lubricated slightly toughened black polyamide 66 for injection molding. It has improved impact resistance.Information provided by ..
Charpy Impact, Notched 1.20 J/cm²
<br>@Temperature -30.0 °C
5.71 ft-lb/in²
<br>@Temperature -22.0 °F
ISO 179/1eA
DSM Akulon® K230-HPV8 Impact Modified Nylon 6 (European Grade) (Dry) &nbsp;(discontinued **)
The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier ..
Charpy Impact, Notched 1.20 J/cm²
<br>@Temperature -40.0 °C
5.71 ft-lb/in²
<br>@Temperature -40.0 °F
50%RH; ISO 179/1eA
DuPont Performance Polymers Zytel® 73G35HSL BK262 Nylon 6 &nbsp;(Unverified Data**)
Zytel® 73G35HSL BK262 is a 35% glass fiber reinforced, heat stabilized, black polyamide 6 resin for injection molding.Information provided by DuPont Performance Polymers
Charpy Impact, Notched 1.20 J/cm²
<br>@Temperature -30.0 °C
5.71 ft-lb/in²
<br>@Temperature -22.0 °F
ISO 179
LG Chemical HI-151 ABS, Middle Impact
Information Provided by LG Chem
Charpy Impact, Notched 1.20 J/cm²
<br>@Temperature 23.0 °C
5.71 ft-lb/in²
<br>@Temperature 73.4 °F
ISO 179/1eA
Lanxess Durethan® BKV 35 H2.0 EF 900116 Nylon 6, 35% Glass Fiber
PA 6, injection molding grade, 35% glass fibers, good heat-ageing resistance, good flowability (easy flow)
Charpy Impact, Notched 1.20 J/cm²
<br>@Temperature 23.0 °C
5.71 ft-lb/in²
<br>@Temperature 73.4 °F
ISO 179/1eA
Lanxess Pocan® B 4239 000000 PBT, 30% Glass Fiber
PBT, 30% glass fibers, injection molding, flame retardant
Charpy Impact, Notched 1.20 J/cm²
<br>@Temperature 23.0 °C
5.71 ft-lb/in²
<br>@Temperature 73.4 °F
ISO 179/1eA
Lanxess Durethan® BKV 330 H2.0 901510 Nylon 6, 30% Glass Fiber
PA 6, injection molding type, 30% glass fibers, branched/structural viscosity, good weldability (vibration or hot plate), good heat-ageing resistance
Charpy Impact, Notched 1.20 J/cm²
<br>@Temperature -30.0 °C
5.71 ft-lb/in²
<br>@Temperature -22.0 °F
ISO 179/1eA
Styrolution Terblend® N NM-21 EF Gray 38058 ABS+PA (Dry)
Description: Terblend® N NM-21 EF is an UV stabilized ABS/PA blend combining very high impact strength, even at low temperatures. The enhanced flowability enables excellent processability and sur..
Charpy Impact, Notched 1.20 J/cm²
<br>@Temperature -30.0 °C
5.71 ft-lb/in²
<br>@Temperature -22.0 °F
ISO 179/1eA
Styron CALIBREâ„¢ 200-14 Polycarbonate Resin
Overview: CALIBREâ„¢ 200-14 polycarbonate resin is a natural, FDA compliant, 14 melt flow rate general purpose polycarbonate resin with no mold release or UV stabilizer.Govt. and Industry Standar..
Charpy Impact, Notched 1.20 J/cm²
<br>@Temperature -30.0 °C
5.71 ft-lb/in²
<br>@Temperature -22.0 °F
Injection Molded; ISO 179/2
Styron MAGNUMâ„¢ 3904 Acrylonitrile Butadiene Styrene (ABS) Resin
Overview: MAGNUMâ„¢ 3904 is a resin with super-high impact. It is used in a wide range of technical applications. It can be processed by injection molding, extrusion or thermoforming. The mass (c..
Charpy Impact, Notched 1.20 J/cm²
<br>@Temperature -30.0 °C
5.71 ft-lb/in²
<br>@Temperature -22.0 °F
V-notch Edgew 80*10*4 sp=62mm; ISO 179/1eA
SABIC Innovative Plastics Noryl GTX GTX979 PPE+PA
NORYL GTX979 is a conductive, high heat material. It is especially designed for in- and on-line painted bodypanels and fenders in particular, with conductivity for electro-static painting in an uniq..
Charpy Impact, Notched 1.20 J/cm²
<br>@Temperature -30.0 °C
5.71 ft-lb/in²
<br>@Temperature -22.0 °F
ISO 179
Styrolution Novodur® H801 ABS / PC
Novodur H801 is a high heat injection molding grade with high impact strength and reduced emission.Information provided by Styrolution
Charpy Impact, Notched 1.20 J/cm²
<br>@Temperature -30.0 °C
5.71 ft-lb/in²
<br>@Temperature -22.0 °F
ISO 179
Styrolution Terblend® N NM-21 XP ABS+PA (Dry)
Information provided by STYROLUTION, which is a joint venture between BASF and INEOS
Charpy Impact, Notched 1.20 J/cm²
<br>@Thickness 3.00 mm,<br> Temperature -30.0 °C
5.71 ft-lb/in²
<br>@Thickness 0.118 in,<br> Temperature -22.0 °F
complete break; ISO 7391/b.o. ISO 179-1eA
Covestro Makrolon® 2258 Polycarbonate
Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Medical devices - bioc..
Charpy Impact, Notched 1.20 J/cm²
<br>@Thickness 3.00 mm,<br> Temperature -30.0 °C
5.71 ft-lb/in²
<br>@Thickness 0.118 in,<br> Temperature -22.0 °F
complete break; ISO 7391/b.o. ISO 179-1eA
Covestro Makrolon® Rx2435 Polycarbonate
Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Medical devices• Low..
Charpy Impact, Notched 1.20 J/cm²
<br>@Temperature -30.0 °C
5.71 ft-lb/in²
<br>@Temperature -22.0 °F
ISO 179/1eA
DSM Stanyl® TW200F8 Nylon 46-40% Glass Reinforced (European Grade) (Cond)
Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper..
Charpy Impact, Notched 1.20 J/cm²
<br>@Temperature -40.0 °C
5.71 ft-lb/in²
<br>@Temperature -40.0 °F
DAM; ISO 179/1eA
DuPont Performance Polymers Zytel® 77G33HS1L NC010 Nylon 612
Zytel® 77G33HS1L NC010 is a 33% glass fiber reinforced, heat stabilized polyamide 612 resin for injection molding.Information provided by DuPont Performance Polymers
Charpy Impact, Notched 1.20 J/cm²
<br>@Temperature -30.0 °C
5.71 ft-lb/in²
<br>@Temperature -22.0 °F
Edgew 80x10x4 sp=62; ISO 179/1eA
Eurostar Staramide BG7HU PA6, 35% Glass Fiber Filled, Heat and UV Stabilized, Injection Molded
Staramide BG7H is a Heat and UV Stabilized, 35% Glass Fiber Reinforced, Polyamide 6, Injection Molding ResinInformation provided by Eurostar.
Charpy Impact, Notched 1.20 J/cm²
<br>@Temperature -30.0 °C
5.71 ft-lb/in²
<br>@Temperature -22.0 °F
ISO 179/1eA
DSM Arnite® AV2 372 PET-35% Glass Reinforced (European and Asian Grade)
Arnite resins are engineered to provide specific performance in applications where DSM technology can offer value.Arnite Molding resins: Standard Unfilled and Reinforced materialsHigh modulus Flame ..
Charpy Impact, Notched 1.20 J/cm²
<br>@Temperature -30.0 °C
5.71 ft-lb/in²
<br>@Temperature -22.0 °F
ISO 179-1eA
Barlog Plastics KEBATER BF250 PBT, 50% glass fiber reinforced, food grade
PBT-GF50Information provided by BARLOG plastics GmbH.
Charpy Impact, Notched 1.20 J/cm²
<br>@Temperature 23.0 °C
5.71 ft-lb/in²
<br>@Temperature 73.4 °F
ISO 179
Ascend Performance Materials Vydyne® R540H Nylon 66, 40% Glass Reinforced, DAM
Vydyne® R540H is general-purpose, heat-stabilized, hydrolysis-resistant, 40% glass-fiber reinforced PA66 resin. Available in natural, it is specifically designed to maximize the retention of physic..
Charpy Impact, Notched 1.20 J/cm²
<br>@Temperature 23.0 °C
5.71 ft-lb/in²
<br>@Temperature 73.4 °F
ISO 179/1eA
BASF Ultraform® N2650 Z2 (LEV) POM
Description: Is a POM + PUR, elastomer-modified injection-molding grades with high impact strength for clips, snap and fastening elements, also for components subject to impact stress.Information pr..
Charpy Impact, Notched 1.20 J/cm²
<br>@Temperature -30.0 °C
5.71 ft-lb/in²
<br>@Temperature -22.0 °F
ISO 179/eA
Eurotec® Tecodur® PB70 GR45 NL PBT 45% glass fiber reinforced
Excellent stiffness and hardnessGood mechanical strengthGood creep and fatigue behaviorVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance..
Charpy Impact, Notched 1.20 J/cm²
<br>@Temperature -30.0 °C
5.71 ft-lb/in²
<br>@Temperature -22.0 °F
ISO 179
Ascend Performance Materials Vydyne® R533 Nylon 66, 33% Glass Filled, Conditioned (2.5% Moisture)
Vydyne® R533 is general-purpose, 33% glass-reinforced PA66 resin. Available in natural, it is an injection-molding grade resin that is lubricated for good machine feed, flow, and mold release. Glas..
Charpy Impact, Notched 1.20 J/cm²
<br>@Temperature 23.0 °C
5.71 ft-lb/in²
<br>@Temperature 73.4 °F
50%RH; ISO 179/1eA
DuPont Performance Polymers Zytel® EFE1068 NC010T Nylon 66 &nbsp;(Unverified Data**)
Zytel® EFE1068 NC010T is a lubricated polyamide 66 for injection molding. It has excellent flow characteristics and was developed for fast production cycles and high productivity applications.Info..