Processing Properties | Metric | English | Comments |
---|---|---|---|
Back Pressure | 0.981 - 3.92 MPa | 142 - 569 psi | Injection Molding |
LG Chemical LUCON CP510F PC/ABS+CNT Description Injection Molding Grade, PC/ABS+CNT, Electrostatic Dissipation, High Flow, Good ProcessabilityApplication: Copy Machine Paper GuideCAS No. 103598-77-2 and 7440-44-0Information provided b.. |
|||
Back Pressure | 0.981 - 3.92 MPa | 142 - 569 psi | Injection Molding |
LG Chemical LUCON PN9008 PPS+MF+GF Injection Molding Grade, PPS+MF+GF, High Thermal Conductivity, Chemical Resistance, High Heat ResistanceApplication: Electrical or Electronic Parts (Heat sink, LED etc.), Motor HousingsCAS No. 25212.. |
|||
Back Pressure | 0.981 - 1.96 MPa | 142 - 284 psi | Injection Molding |
LG Chemical LUMIPLAS LD590T Light diffusion ABS Description: Extrusion, Light diffusion, High ImpactApplication: (LED) Lamp Cover, Signboard Lighting Decoration of Electronic DeviceCAS No. 9010-94-0Information provided by LG Chemical |
|||
Back Pressure | 0.981 - 3.92 MPa | 142 - 569 psi | Injection Molding |
LG Chemical LUPOS GP2100 ABS+GF10%, General Purpose Feature: Injection Molding, ABS+GF10%, General PurposeApplication: Electric & Electronic (Housing, Components)CAS No. 9003-56-9, 9003-54-7 and 65997-17-3Information provided by LG Chemical |
|||
Back Pressure | 0.981 - 3.92 MPa | 142 - 569 psi | Injection Molding |
LG Chemical LUPOY EC5000A PC/ABS Description: Injection Molding, PC/ABS, General Purpose, Anti-Static.Application: E&E (Housing)Information provided by LG Chemical |
|||
Back Pressure | 0.981 - 3.92 MPa | 142 - 569 psi | Injection Molding |
LG Chemical LUPOY EF5001RFT PC/ABS Description: Injection Molding, PC/ABS, Halogen Free Flame Retardant, EU Eco-Label compliantApplication: Display housingCAS: 103598-77-2, 9003-56-9 and 125997-21-9Information provided by LG Chemical.. |
|||
Back Pressure | 0.981 - 3.92 MPa | 142 - 569 psi | Injection Molding |
LG Chemical LUPOY GN1000F PC, Halogen Free, Flame Retardant, Transparency Description: Injection Molding, PC, Halogen Free Flame Retardant, TransparencyApplication: IT/OA, Electric & Electronic Housing and ComponentsCAS: 103598-77-2 and 181028-79-5Information provided by .. |
|||
Back Pressure | 0.981 - 3.92 MPa | 142 - 569 psi | Injection Molding |
LG Chemical LUPOY GN1000FA PC, Halogen Free, Flame Retardant, Transparency Description: Injection Molding, PC, Halogen Free Flame Retardant, TransparencyApplication: IT/OA, Electric & Electronic Housing and ComponentsCAS: 103598-77-2 and 181028-79-5Information provided by .. |
|||
Back Pressure | 0.981 - 3.92 MPa | 142 - 569 psi | Injection Molding |
LG Chemical LUPOY GN1006FMR PC, Halogen Free, Flame Retardant, Transparency Description: Injection Molding, PC, Halogen Free Flame Retardant, Transparency, Mold ReleaseApplication: IT/OA, Electric & Electronic Housing and ComponentsCAS: 103598-77-2Information provided by LG.. |
|||
Back Pressure | 0.981 - 1.96 MPa | 142 - 284 psi | Injection Molding |
LG Chemical LUPOY GN1008RF PC, Halogen Free, Flame Retardant, High impact strength Description: Injection Molding, PC, Halogen Free Flame Retardant, High impact strengthApplication: IT&OA (Notebook PC battery pack housing)CAS: 103598-77-2, 137050-02-03 and 139189-30-3Information p.. |
|||
Back Pressure | 0.981 - 3.92 MPa | 142 - 569 psi | Injection Molding |
LG Chemical LUPOY GP1000L PC, Transparent Description: Injection Molding, PC, General Purpose, Transparency, High FlowApplication: IT/OA, E&E Housing and Components Automotive InteriorCAS: 103598-77-2Information provided by LG Chemical |
|||
Back Pressure | 0.981 - 3.92 MPa | 142 - 569 psi | Injection Molding |
LG Chemical LUPOY GP5006AF PC/ABS, Flame Retardant Description: Injection Molding, PC/ABS, Flame RetardantApplication: Electric and Electronic Housing and ComponentsCAS: 103598-77-2, 9003-56-9, 68928-70-1 and 1309-64-4Information provided by LG Chem.. |
|||
Back Pressure | 0.981 - 3.92 MPa | 142 - 569 psi | Injection Molding |
LG Chemical LUPOY SC1004AU PC, High Impact Description: Injection Molding, PC, High Impact, High Flow, Good WeatherabilityApplication: Electric & Electronic HousingCAS: 103598-77-2 and 143106-82-5Information provided by LG Chemical |
|||
Back Pressure | 0.981 - 3.92 MPa | 142 - 569 psi | Injection Molding |
LG Chemical LUPOY SC2202 PC+GF20%, High Impact Description: Injection Molding, PC+GF20%, Good Toughness, Good Impact, Chemical ResistanceApplication: Mobile Phone HousingCAS: 103598-77-2 and 65997-17-3Information provided by LG Chemical |
|||
Back Pressure | 0.981 - 3.92 MPa | 142 - 569 psi | Injection Molding |
LG Chemical LUPOY SC2302 PC+GF30%, High Impact Description: Injection Molding, PC+GF30%, Good Toughness, Good Impact, Chemical ResistanceApplication: Mobile Phone HousingCAS: 103598-77-2 and 65997-17-3Information provided by LG Chemical |
|||
Back Pressure | 0.981 - 3.92 MPa | 142 - 569 psi | Injection Molding |
LG Chemical LUPOY SR3108FC PC, Halogen Free Flame Retardance Description: Injection Molding, PC, Halogen Free Flame Retardance, Light Reflectance, White Color OnlyApplication: LCD Back Light Unit partsCAS: 103598-77-2, 9003-56-9 and 13463-67-1Information prov.. |
|||
Back Pressure | 0.981 - 3.92 MPa | 142 - 569 psi | Injection Molding |
LG Chemical LUPOY SR3108FM PC, Halogen Free Flame Retardance Description: Injection Molding, PC, Halogen Free Flame Retardance, Light Reflectance, White Color OnlyApplication: LCD Back Light Unit partsCAS: 103598-77-2, 9003-56-9 and 13463-67-1Information prov.. |
|||
Back Pressure | 0.981 - 3.92 MPa | 142 - 569 psi | Injection Molding |
LG Chemical LUPOY SR3108L PC, High Impact Description: Injection Molding, PC, High Flow, High Impact, White Color OnlyApplication: BLU Mold frame for Mobile DevicesCAS: 103598-77-2 and 13463-67-1Information provided by LG Chemical |
|||
Back Pressure | 0.981 - 3.92 MPa | 142 - 569 psi | Injection Molding |
LG Chemical LUPOY GN1002FL PC, Halogen Free, Flame Retardant, High Flow Description: Injection Molding, PC, Halogen Free Flame Retardant, High Flow, High ImpactApplication: IT/OA (M/P Battery Inner Pack Housing)CAS: 103598-77-2, 25232-40-0 and 139189-30-3Information pro.. |
|||
Back Pressure | 0.981 - 3.92 MPa | 142 - 569 psi | Injection Molding |
LG Chemical LUPOY GN1002FS PC, Halogen Free, Flame Retardant, High Impact Description: Injection Molding, PC, Halogen Free Flame Retardant, High Impact, Chemical ResistanceApplication: IT/OA (M/P Battery Housing)CAS: 103598-77-2, 25232-40-0 and 139189-30-3Information prov.. |
|||
Back Pressure | 0.981 - 3.92 MPa | 142 - 569 psi | Injection Molding |
LG Chemical LUPOY GN2301F PC+GF30%, Halogen Free, Flame Retardant, Heat Resistance Description: Injection Molding, PC+GF30%, Halogen Free Flame Retardant, Heat ResistanceApplication: IT/OA, Electric & Electronic Housing and ComponentsCAS: 103598-77-2 and 65997-17-3Information prov.. |
|||
Back Pressure | 0.981 - 3.92 MPa | 142 - 569 psi | Injection Molding |
LG Chemical LUPOY GP1000MR PC, Transparent Description: Injection Molding, PC, General Purpose, Transparency, Mold ReleaseApplication: IT/OA Housing and Components, Automotive InteriorCAS: 103598-77-2Information provided by LG Chemical |
|||
Back Pressure | 0.981 - 3.92 MPa | 142 - 569 psi | Injection Molding |
LG Chemical LUPOY GP1000MU PC, Transparent Description: Injection Molding, PC, General Purpose, Transparency, UV StabilityApplication: IT/OA Housing and Components, Automotive Exterior and InteriorCAS: 103598-77-2Information provided by LG C.. |
|||
Back Pressure | 0.981 - 3.92 MPa | 142 - 569 psi | Injection Molding |
LG Chemical LUPOY GP1000SW PC, Transparent Description: Injection Molding, PC, General Purpose, TransparencyApplication: Keypad for Mobile Phone, Automotive (Interior)CAS: 103598-77-2Information provided by LG Chemical |
|||
Back Pressure | 0.979 - 1.96 MPa | 142 - 284 psi | |
Samsung Cheil Industries Starex® WR-9140 General Purpose ABS Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Back Pressure | 0.979 - 1.96 MPa | 142 - 284 psi | |
Samsung Cheil Industries Starex® WR-9330I Heat Resistant Grade ABS Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Back Pressure | 0.979 - 1.96 MPa | 142 - 284 psi | |
Samsung Cheil Industries TRANEX® TX-0520T Transparent Grade ABS Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Back Pressure | 0.979 - 1.96 MPa | 142 - 284 psi | |
Samsung Cheil Industries Starex® WR-9330I Heat Resistant Grade ABS Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Back Pressure | 0.979 - 1.96 MPa | 142 - 284 psi | |
Samsung Cheil Industries TRANEX® TX-0520T Transparent Grade ABS Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Back Pressure | 0.981 - 3.92 MPa | 142 - 569 psi | Injection Molding |
LG Chemical LUPOY GP2100 PC+GF10%, Heat Resistance Description: Injection Molding, PC+GF10%, General Purpose, Heat ResistanceApplication: IT/OA, E&E Housing and Components, Automotive (Interior)CAS: 103598-77-2 and 65997-17-3Information provided by .. |