| Category | Polymer , Thermoplastic , Polycarbonate (PC) , Polycarbonate, Unreinforced, Flame Retardant |
| Manufacturer | LG Chemical |
| Trade Name | LUPOY |
| Port | Ningbo port,China |
| Trade Terms | FOB, CFR, CIF |
| Payment Terms | L/C, T/T, Western Union |
| Download PDF | LG Chemical LUPOY GN1006FMR PC, Halogen Free, Flame Retardant, Transparency.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.20 g/cc | 1.20 g/cc | ASTM D792 |
| Maximum Moisture Content | 0.020 | 0.020 | Injection Molding |
| Linear Mold Shrinkage, Flow | 0.0050 - 0.0070 cm/cm @Thickness 3.20 mm |
0.0050 - 0.0070 in/in @Thickness 0.126 in |
ASTM D955 |
| Melt Flow | 10 g/10 min @Load 1.20 kg, Temperature 300 °C |
10 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Rockwell R | 118 | 118 | ASTM D785 |
| Tensile Strength, Yield | 61.8 MPa @Thickness 3.20 mm |
8960 psi @Thickness 0.126 in |
50mm/min; ASTM D638 |
| Elongation at Break | >= 100 % @Thickness 3.20 mm |
>= 100 % @Thickness 0.126 in |
50mm/min; ASTM D638 |
| Flexural Yield Strength | 91.2 MPa @Thickness 3.20 mm |
13200 psi @Thickness 0.126 in |
10mm/min; ASTM D790 |
| Flexural Modulus | 2.26 GPa @Thickness 3.20 mm |
327 ksi @Thickness 0.126 in |
10mm/min; ASTM D790 |
| Izod Impact, Notched | >= 7.16 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
>= 13.4 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Deflection Temperature at 1.8 MPa (264 psi) | >= 130 °C @Thickness 6.40 mm |
>= 266 °F @Thickness 0.252 in |
Unannealed; ASTM D648 |
| Vicat Softening Point | 141 °C @Load 5.00 kg |
286 °F @Load 11.0 lb |
50°C/h; ASTM D1525 |
| UL RTI, Electrical | 120 °C @Thickness >=1.50 mm |
248 °F @Thickness >=0.0591 in |
|
| 120 °C @Thickness >=2.00 mm |
248 °F @Thickness >=0.0787 in |
||
| 120 °C @Thickness >=2.50 mm |
248 °F @Thickness >=0.0984 in |
||
| 120 °C @Thickness >=3.00 mm |
248 °F @Thickness >=0.118 in |
||
| UL RTI, Mechanical with Impact | 110 °C @Thickness >=1.50 mm |
230 °F @Thickness >=0.0591 in |
|
| 110 °C @Thickness >=2.00 mm |
230 °F @Thickness >=0.0787 in |
||
| 110 °C @Thickness >=2.50 mm |
230 °F @Thickness >=0.0984 in |
||
| 110 °C @Thickness >=3.00 mm |
230 °F @Thickness >=0.118 in |
||
| UL RTI, Mechanical without Impact | 120 °C @Thickness >=1.50 mm |
248 °F @Thickness >=0.0591 in |
|
| 120 °C @Thickness >=2.00 mm |
248 °F @Thickness >=0.0787 in |
||
| 120 °C @Thickness >=2.50 mm |
248 °F @Thickness >=0.0984 in |
||
| 120 °C @Thickness >=3.00 mm |
248 °F @Thickness >=0.118 in |
||
| Flammability, UL94 | V-2 @Thickness >=1.50 mm |
V-2 @Thickness >=0.0591 in |
|
| V-1 @Thickness >=2.00 mm |
V-1 @Thickness >=0.0787 in |
||
| V-0 @Thickness >=2.50 mm |
V-0 @Thickness >=0.0984 in |
||
| V-0 @Thickness >=3.00 mm |
V-0 @Thickness >=0.118 in |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Arc Resistance | 0.00 - 60 sec | 0.00 - 60 sec | ASTM D495 |
| Comparative Tracking Index | 175 - 250 V | 175 - 250 V | |
| High Voltage Arc-Tracking Rate, HVTR | 80.0 - 150 mm/min | 3.15 - 5.91 in/min |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Rear Barrel Temperature | 260 - 280 °C | 500 - 536 °F | Injection Molding |
| Middle Barrel Temperature | 280 - 300 °C | 536 - 572 °F | Injection Molding |
| Front Barrel Temperature | 300 - 320 °C | 572 - 608 °F | Injection Molding |
| Nozzle Temperature | 300 - 320 °C | 572 - 608 °F | Injection Molding |
| Melt Temperature | 300 - 320 °C | 572 - 608 °F | Injection Molding |
| Mold Temperature | 80.0 - 120 °C | 176 - 248 °F | Injection Molding |
| Drying Temperature | 100 - 120 °C | 212 - 248 °F | Injection Molding |
| Dry Time | 3.00 - 5.00 hour | 3.00 - 5.00 hour | Injection Molding |
| Back Pressure | 0.981 - 3.92 MPa | 142 - 569 psi | Injection Molding |
| Screw Speed | 40 - 70 rpm | 40 - 70 rpm | Injection Molding |