| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Middle Barrel Temperature | 250 - 265 °C | 482 - 509 °F | |
|
Parker Chomerics PREMIER™ A220-FR EMI Shielding Plastic
Description: PREMIER™ is the world’s first and most versatile commercially available conductive thermoplastic for real world EMI shielding solutions. It is a blend of PC/ABS thermoplastic polymer ..
|
|||
| Middle Barrel Temperature | 245 - 265 °C | 473 - 509 °F | Start Point: 250°C |
|
Kingfa PET-RG20 Flame Retardant, 20% Glass Fiber Reinforced PET
Features:Flame retardantHigh strengthGood heat resistanceOutstanding electrical propertiesApplications:Injection moldingConnectorsRelayBobbinsSocketsE & E partsInformation Provided by Kingfa Sci. & ..
|
|||
| Middle Barrel Temperature | 245 - 265 °C | 473 - 509 °F | Start Point: 250°C |
|
Kingfa PET-RG30 Flame Retardant, 30% Glass Fiber Reinforced PET
Features:Flame retardantHigh strengthGood heat resistanceOutstanding electrical propertiesApplications:Injection moldingConnectorsRelayBobbinsSocketsE & E partsInformation Provided by Kingfa Sci. & ..
|
|||
| Middle Barrel Temperature | 245 - 265 °C | 473 - 509 °F | Injection Molding |
|
LG Chemical LUMID GP2151AF PA6+GF15%, Flame Retardant
Feature: Injection Molding, PA6+GF15%, Flame RetardantApplication: ConnectorsCAS No. 25038-54-4, 65997-17-3, 88497-56-7, 1309-64-4 and 138265-88-0Information provided by LG Chemical
|
|||
| Middle Barrel Temperature | 240 - 265 °C | 464 - 509 °F | Injection Molding |
|
LG Chemical LUMID LW4203A(W) PA6+GF/MF20%, Low Warpage
Feature: Injection Molding, PA6+GF/MF20%, Low WarpageApplication: Automotive Parts (Engine Cover)CAS No. 25038-54-4, 13983-17-0 and 65997-17-3Information provided by LG Chemical
|
|||
| Middle Barrel Temperature | 245 - 265 °C | 473 - 509 °F | Injection Molding |
|
LG Chemical LUPOY ER5151RFA PC/ABS Mineral Filler, Halogen Free Flame Retardant
Description: Injection Molding, PC/ABS, Halogen Free Flame Retardant, High strength, EPEATApplication: IT&OA (Notebook PC housing)CAS: 103598-77-2, 9003-56-9, 181028-79-5 and 14807-96-6Information p..
|
|||
| Middle Barrel Temperature | 250 - 265 °C | 482 - 509 °F | Injection Molding |
|
LG Chemical LUPOY GN1000F PC, Halogen Free, Flame Retardant, Transparency
Description: Injection Molding, PC, Halogen Free Flame Retardant, TransparencyApplication: IT/OA, Electric & Electronic Housing and ComponentsCAS: 103598-77-2 and 181028-79-5Information provided by ..
|
|||
| Middle Barrel Temperature | 245 - 265 °C | 473 - 509 °F | Injection Molding |
|
LG Chemical LUPOY GN5151RFA PC/ABS Mineral Filler
Description: Injection Molding, PC/ABS Mineral Filler, General Purpose, High Stiffness, Halogen Free Flame RetardantApplication: IT&OA (Notebook PC housingCAS: 103598-77-2, 9003-56-9, 181028-79-5 an..
|
|||
| Middle Barrel Temperature | 235 - 265 °C | 455 - 509 °F | Injection Molding |
|
LG Chemical LUPOY HI5002A PC/ABS, High Impact
Description: Injection Molding, PC/ABS, General Purpose, High Flow, High ImpactApplication: E&E (housing)CAS: 103598-77-2 and 9003-56-9Information provided by LG Chemical
|
|||
| Middle Barrel Temperature | 235 - 265 °C | 455 - 509 °F | Injection Molding |
|
LG Chemical LUPOY MP5000AM PC/ABS
Description: Injection Molding, PC/ABS, General Purpose, Metal PlatingApplication: Automotive (Exterior), E&E (Housing)CAS: 103598-77-2 and 9003-56-9Information provided by LG Chemical
|
|||
| Middle Barrel Temperature | 250 - 265 °C | 482 - 509 °F | |
|
Lavergne VYPET 2130 Polyester Alloy Resin, 30% Fiberglass Reinforced
Vypet 2130 is a 30% fiberglass reinforced, toughened Modified PBT injection molding compound designed for structural and electrical applications.Features: High temperature performances; Excellent di..
|
|||
| Middle Barrel Temperature | 245 - 265 °C | 473 - 509 °F | Start Point: 250°C |
|
Kingfa PET-G15 15% Glass Fiber Reinforced PET
Features:High strengthGood heat resistanceApplications:Injection moldingApplication partsAuto partsInformation Provided by Kingfa Sci. & Tech. Co., Ltd.
|
|||
| Middle Barrel Temperature | 245 - 265 °C | 473 - 509 °F | Start Point: 250°C |
|
Kingfa PET-G30 30% Glass Fiber Reinforced PET
Features:High strengthGood heat resistanceApplications:Injection moldingApplication partsAuto partsInformation Provided by Kingfa Sci. & Tech. Co., Ltd.
|
|||
| Middle Barrel Temperature | 245 - 265 °C | 473 - 509 °F | Start Point: 250°C |
|
Kingfa PET-RG15 Flame Retardant, 15% Glass Fiber Reinforced PET
Features:Flame retardantHigh strengthGood heat resistanceOutstanding electrical propertiesApplications:Injection moldingConnectorsRelayBobbinsSocketsE & E partsInformation Provided by Kingfa Sci. & ..
|
|||
| Middle Barrel Temperature | 245 - 265 °C | 473 - 509 °F | Injection Molding |
|
LG Chemical LUPOY GN5151RF PC/ABS Mineral Filler
Description: Injection Molding, PC/ABS Mineral Filler, General Purpose, High Stiffness, Halogen Free Flame RetardantApplication: E&E (Housing), IT/OA (Notebook PC Housing)CAS: 103598-77-2, 9003-56-9..
|
|||
| Middle Barrel Temperature | 230 - 265 °C | 446 - 509 °F | Cylinder Temperature |
|
Asia International Enterprise (Hong Kong) 30G3F Polybutylene terephthalate, 15% Glass Fiber Filled
Information provided by Asia International Enterprise (Hong Kong) Ltd.
|
|||
| Middle Barrel Temperature | 230 - 265 °C | 446 - 509 °F | Cylinder Temperature |
|
Asia International Enterprise (Hong Kong) 30G3 Polybutylene terephthalate, 15% Glass Fiber Filled
Information provided by Asia International Enterprise (Hong Kong) Ltd.
|
|||
| Middle Barrel Temperature | 260 - 265 °C | 500 - 509 °F | |
|
Beijing Chemical Industry KAIFA® MN301-M30 Nylon 66 Resin
Mineral filled, Good flowInformation provided by Beijing Chemical Industry Research Institute (Group)
|
|||
| Middle Barrel Temperature | 230 - 265 °C | 446 - 509 °F | Cylinder Temperature |
|
Asia International Enterprise (Hong Kong) 30G6 Polybutylene terephthalate, 30% Glass Fiber Filled
Information provided by Asia International Enterprise (Hong Kong) Ltd.
|
|||
| Middle Barrel Temperature | 230 - 265 °C | 446 - 509 °F | Cylinder Temperature |
|
Asia International Enterprise (Hong Kong) 30G6F Polybutylene terephthalate, 30% Glass Fiber Filled
Information provided by Asia International Enterprise (Hong Kong) Ltd.
|
|||
| Middle Barrel Temperature | 260 - 265 °C | 500 - 509 °F | |
|
Beijing Chemical Industry KAIFA® MN101 Nylon 66 Resin
Good flow, High impactInformation provided by Beijing Chemical Industry Research Institute (Group)
|
|||
| Middle Barrel Temperature | 260 - 265 °C | 500 - 509 °F | |
|
Beijing Chemical Industry KAIFA® MN301-G0 Nylon 66 Resin
High flame retardant, Good flowInformation provided by Beijing Chemical Industry Research Institute (Group)
|
|||
| Middle Barrel Temperature | 245 - 265 °C | 473 - 509 °F | Injection Molding |
|
LG Chemical LUPOY GN5201F PC/ABS+GF20%, Halogen Free Flame Retardant
Description: Injection Molding, PC/ABS+GF20%, Halogen Free Flame Retardant, High StiffnessApplication: E&E (Housing, OA Frame)CAS: 103598-77-2, 9003-56-9, 181028-79-5 and 65997-17-3Information provi..
|
|||