Polymer Property : Middle Barrel Temperature = 235 °C Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Middle Barrel Temperature 235 °C
455 °F
For high temperature coextrusions.
DuPont Bynel® 41E623 Adhesive Resin  (discontinued **)
Bynel® Series 4100 resins are anhydride-modified linear low-density polyethylene (LLDPE) resins. They are available in pellet form for use in conventional extrusion and coextrusion equipment design..
Middle Barrel Temperature 235 - 260 °C
455 - 500 °F
Start Point: 245°C
Kingfa JH710 G15 Flame Retardant & 15% Glass Fiber Reinforced PC
Features:Environmental friendly flame retardantUL V-0 @ 1.6mmHigh mechanical strengthGood size stability, good surfaceSuitable for exact moldingApplications:CD-ROM, DVDPrinter, photocopier cabinetSc..
Middle Barrel Temperature 235 - 255 °C
455 - 491 °F
Start Point: 245°C
Kingfa PBT-RG301 Flame Retardant, 30% Glass Fiber Reinforced PBT
Features:Flame retardantHigh mechanical strengthHigh heat resistanceGood electric propertiesNo bloomingApplications:Injection moldingHousehold appliance partsBobbinLighting partsRelayLinkerInformati..
Middle Barrel Temperature 235 - 255 °C
455 - 491 °F
Start Point: 245°C
Kingfa PBT-RG302 Flame Retardant, 30% Glass Fiber Reinforced PBT
Features:Flame retardantHigh strengthHigh temperature propertiesHigh glossyGood surfaceNo bloomingApplications:Injection moldingConnectorsRelayBobbinsPlugsE & E partsInformation Provided by Kingfa S..
Middle Barrel Temperature 235 - 245 °C
455 - 473 °F
Injection Molding
LG Chemical Lupox® GP1000H PBT
Description: Injection Molding, PBT, High Flow, High ImpactApplication: Automotive (Connector)CAS No. 155123-66-3 and 24968-12-5Information provided by LG Chemical
Middle Barrel Temperature 235 - 245 °C
455 - 473 °F
Injection Molding
LG Chemical Lupox® GP1000W PBT
Description: Injection Molding, PBT, Anti-HydrolysisApplication: IT/OA, Automotive (Connector)CAS No. 24968-12-5Information provided by LG Chemical
Middle Barrel Temperature 235 - 250 °C
455 - 482 °F
LG Chemical Lupox® PBT-GP-2300 30% GFR PBT
Information provided by US distributor Polymer Technology and Services, LLC (PTS).
Middle Barrel Temperature 235 - 250 °C
455 - 482 °F
LG Chemical Lupox® PBT-GP-2306FA 30% GFR Flame Retardant, UV Stabilized PBT
Information provided by US distributor Polymer Technology and Services, LLC (PTS).
Middle Barrel Temperature 235 - 250 °C
455 - 482 °F
LG Chemical Lupox® PBT-LW5303 30% Glass Filled Low Warp PBT
Low Warpage. Information provided by US distributor Polymer Technology and Services, LLC (PTS).
Middle Barrel Temperature 235 - 250 °C
455 - 482 °F
LG Chemical Lupox® SG-4405 Surface Gloss PBT, 40% Glass Fiber/Mineral Reinforced, Dimensional Stability
LUPOX semi-crystalline thermoplastic PBT resins exhibit properties including high strength, rigidity and good resistance to fatigue and creep at elevated temperatures. Furthermore, LUPOX resins sho..
Middle Barrel Temperature 235 °C
455 °F
For high temperature coextrusions.
DuPont Bynel® 4157 Adhesive Resin
Bynel® Series 4100 resins are anhydride-modified linear low-density polyethylene (LLDPE) resins. They are available in pellet form for use in conventional extrusion and coextrusion equipment design..
Middle Barrel Temperature 235 °C
455 °F
For high temperature coextrusions.
DuPont Bynel® 41E687 Adhesive Resin
Bynel® Series 4100 resins are anhydride-modified linear low-density polyethylene (LLDPE) resins. They are available in pellet form for use in conventional extrusion and coextrusion equipment design..
Middle Barrel Temperature 235 - 245 °C
455 - 473 °F
Beijing Chemical Industry KAIFA® HN301-G30 PA6 Resin
30% glass fiber reinforced, flame retardantInformation provided by Beijing Chemical Industry Research Institute (Group)
Middle Barrel Temperature 235 - 266 °C
455 - 511 °F
A. Schulman ComAlloy Hiloy® 243 SAN, Glass Reinforced
Data provided by the manufacturer, ComAlloy International Company.30% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line.
Middle Barrel Temperature 235 - 249 °C
455 - 480 °F
A. Schulman ComAlloy Hiloy® 431 Glass Reinforced, PBT Alloy
Data provided by the manufacturer, ComAlloy International Company.15% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line.
Middle Barrel Temperature 235 - 249 °C
455 - 480 °F
A. Schulman ComAlloy Hiloy® 436 Glass/Mineral Reinforced, PBT Alloy
Data provided by the manufacturer, ComAlloy International Company.20% Glass/Mineral Reinforced.The ComAlloy product line has been integrated into the A Schulman product line.
Middle Barrel Temperature 235 - 249 °C
455 - 480 °F
A. Schulman ComAlloy Voloy® 411 Mineral Reinforced, PBT Alloy, Flame Retardant, UL
Data provided by the manufacturer, ComAlloy International Company.25% Mineral Reinforced.The ComAlloy product line has been integrated into the A Schulman product line.
Middle Barrel Temperature 235 - 249 °C
455 - 480 °F
A. Schulman ComAlloy Voloy® 417 Polyester - PBT, Glass/Mineral Reinforced, Flame Retardant, UL
Data provided by the manufacturer, ComAlloy International Company.43% Glass/Mineral Reinforced.The ComAlloy product line has been integrated into the A Schulman product line.
Middle Barrel Temperature 235 - 249 °C
455 - 480 °F
A. Schulman ComAlloy Hiloy® 432 Glass Reinforced, PBT Alloy
Data provided by the manufacturer, ComAlloy International Company.33% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line.
Middle Barrel Temperature 235 - 249 °C
455 - 480 °F
A. Schulman ComAlloy Hiloy® 462 Glass Reinforced, PBT Alloy
Data provided by the manufacturer, ComAlloy International Company.15% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line.
Middle Barrel Temperature >= 235 °C
>= 455 °F
Borealis Borstar® HE6062 HDPE Black Jacketing Compound
Borstar HE6062 is a black, bimodal co-polymer high density polyethylene (HDPE) compound produced using the Borealis Borstar process. It is characterized by balanced properties important in jacketin..