Processing Properties | Metric | English | Comments |
---|---|---|---|
Middle Barrel Temperature | 260 - 280 °C | 500 - 536 °F | |
PolyOne Trilliant™ HC THC-02 1200 IL Natural Polyamide 66 (Nylon 66) The Trilliant® HC specialty compounds offer a complete system of specialty engineered materials, certified processes, services and technical support that enable healthcare OEM's to get to market ah.. |
|||
Middle Barrel Temperature | 260 °C | 500 °F | Zone 4; Cylinder |
Premix Thermoplastics PRE-ELEC® PC 1431 PRE-ELEC PC 1431 is a conductive thermoplastic compound based on polycarbonate. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-ELE.. |
|||
Middle Barrel Temperature | 260 - 282 °C | 500 - 540 °F | |
Polymer Resources PC-FD4-[color]-1 Polycarbonate, FDA-compliant Feedstocks, Easy Flow with Mold Release, Gamma Resistant Polycarbonate, FDA-compliant Feedstocks, Easy Flow with Mold Release, Gamma ResistantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pig.. |
|||
Middle Barrel Temperature | 260 - 282 °C | 500 - 540 °F | |
Polymer Resources PC-GP4 Polycarbonate, General Purpose, Easy Flow Polycarbonate, General Purpose, Easy FlowFeatures: • High Impact Resistance • Self Extinguishing • High FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conduc.. |
|||
Middle Barrel Temperature | 260 - 282 °C | 500 - 540 °F | |
Polymer Resources PC-GP4-[color]-1 Polycarbonate, General Purpose, Easy Flow with Mold Release Polycarbonate, General Purpose, Easy Flow with Mold ReleaseProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Infor.. |
|||
Middle Barrel Temperature | 260 - 282 °C | 500 - 540 °F | |
Polymer Resources PC-GP4-[color]-5 Polycarbonate, FDA-compliant Feedstocks, Easy Flow Polycarbonate, FDA-compliant Feedstocks, Easy FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information pr.. |
|||
Middle Barrel Temperature | 260 - 304 °C | 500 - 580 °F | |
Polymer Resources PPX-FRG20 Modified-PPO, V-1 Flame Retardant, 20% Glass Reinforced Modified-Polyphenylene Oxide, V-1 Flame Retardant, 20% Glass ReinforcedFeatures: • Bromine Free • Chlorine FreeProcess: Injection MoldingNotes: All physical, mechanical and thermal testing condu.. |
|||
Middle Barrel Temperature | 260 - 304 °C | 500 - 580 °F | |
Polymer Resources PPX-GP2 Modified-PPO, General Purpose Modified-Polyphenylene Oxide, General Purpose, 250F HDTProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informati.. |
|||
Middle Barrel Temperature | 260 - 304 °C | 500 - 580 °F | |
Polymer Resources PPX-GP4-IM Modified-PPO, Impact Modified Modified-Polyphenylene Oxide, Impact Modified, 210F HDTProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informati.. |
|||
Middle Barrel Temperature | 260 - 280 °C | 500 - 536 °F | |
PolyOne Nymax™ 1200 IL Natural Polyamide 66 (Nylon 66) The Nymax® 1200 IL is an internally lubricated, unfilled nylon 6/6 designed for exceptional processing and mold release. This grade is intended primarily for injection molded applications where a g.. |
|||
Middle Barrel Temperature | 260 - 282 °C | 500 - 540 °F | |
Polymer Resources PC-FD4 Polycarbonate, FDA-compliant Feedstocks, Easy Flow, Gamma Resistant Polycarbonate, FDA-compliant Feedstocks, Easy Flow, Gamma ResistantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test sampl.. |
|||
Middle Barrel Temperature | 260 - 271 °C | 500 - 520 °F | |
PTS Tristar® PC-15R-113 15 MFI Clear Utility Grade Polycarbonate With Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Middle Barrel Temperature | 260 - 300 °C | 500 - 572 °F | |
Hybrid Plastics PO6C81.01 Nanoreinforced® Polyphenylene Oxide (PPO) PPO available on the market today is typically mixed with polystyrene or other polymers to make it processable. However, these resins degrade the excellent mechanical and flammability properties of .. |
|||
Middle Barrel Temperature | 260 - 280 °C | 500 - 536 °F | Injection Molding |
LG Chemical LUMID GP2259AFL PA6+GF25%, Flame Retardant Feature: Injection Molding, PA6+GF25%, Flame RetardantApplication: IT/OA (Connector)CAS No. 25038-54-4, 65997-17-3, 1163-19-5, 1309-64-4 and 138265-88-0Information provided by LG Chemical |
|||
Middle Barrel Temperature | 260 - 275 °C | 500 - 527 °F | Injection Molding |
LG Chemical LUPOY GN1008RF PC, Halogen Free, Flame Retardant, High impact strength Description: Injection Molding, PC, Halogen Free Flame Retardant, High impact strengthApplication: IT&OA (Notebook PC battery pack housing)CAS: 103598-77-2, 137050-02-03 and 139189-30-3Information p.. |
|||
Middle Barrel Temperature | 260 - 282 °C | 500 - 540 °F | |
MRC Polymers EMAREXâ„¢ 300 GF43 Nylon 6, 43% Glass Fiber Filled Available in Black onlyCan be UV and Heat StabilizedProperty data for DAM samples.Information provided by MRC Polymers Inc. |
|||
Middle Barrel Temperature | 260 - 277 °C | 500 - 530 °F | |
MRC Polymers NAXALOYâ„¢ 770 ABS + PC Alloy Impact modifiedAvailable in Natural, Black, and GrayCan be Colored (Masterbatch)Low temperature ductility and impact modifiedCan be UV StabilizedInternal and external lubricant can be addedInformati.. |
|||
Middle Barrel Temperature | 260 - 280 °C | 500 - 536 °F | Mid-2. Region Temperature |
Tisan TISLAMID® 66 15% Glass Fiber Reinforced Nylon 66 TISLAMID has a wide area of application in electric/electronic, automotive, durable goods and telecommunications industries. It demonstrates characteristics such as Excellent chemical resistanceElec.. |
|||
Middle Barrel Temperature | 260 - 280 °C | 500 - 536 °F | Mid-2. Region Temperature |
Tisan TISLAMID® 66 25% Glass Fiber Reinforced Flame Retardant (V0). Heat Stabilized Nylon 66 TISLAMID has a wide area of application in electric/electronic, automotive, durable goods and telecommunications industries. It demonstrates characteristics such as Excellent chemical resistanceElec.. |
|||
Middle Barrel Temperature | 260 - 280 °C | 500 - 536 °F | Mid-2. Region Temperature |
Tisan TISLAMID® 66 Flame Retardant (V0). Halogen Free Heat Stabilized Nylon 66 TISLAMID has a wide area of application in electric/electronic, automotive, durable goods and telecommunications industries. It demonstrates characteristics such as Excellent chemical resistanceElec.. |
|||
Middle Barrel Temperature | 260 - 280 °C | 500 - 536 °F | Mid-2. Region Temperature |
Tisan TISLAMID® 66 Flame Retardant (V0). Heat Stabilized Nylon 66 TISLAMID has a wide area of application in electric/electronic, automotive, durable goods and telecommunications industries. It demonstrates characteristics such as Excellent chemical resistanceElec.. |
|||
Middle Barrel Temperature | 260 - 266 °C | 500 - 510 °F | |
Diamond Polymers ASA M-523 Description: ASA Weatherable Polymer, Injection Molding Grade, High HeatInformation provided by Diamond Polymers, Inc. |
|||
Middle Barrel Temperature | 260 - 288 °C | 500 - 550 °F | |
Clariant PA131G2GN-91 Green Nylon 66, Highly Toughened Data provided by Clariant Masterbatches |
|||
Middle Barrel Temperature | 260 - 271 °C | 500 - 520 °F | |
A. Schulman ComAlloy Hiloy® 610 Nylon 6, Glass/Mineral Reinforced, UL Data provided by the manufacturer, ComAlloy International Company.45% Glass/Mineral Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Middle Barrel Temperature | 260 - 265 °C | 500 - 509 °F | |
Beijing Chemical Industry KAIFA® MN301-M30 Nylon 66 Resin Mineral filled, Good flowInformation provided by Beijing Chemical Industry Research Institute (Group) |
|||
Middle Barrel Temperature | 260 - 304 °C | 500 - 580 °F | |
Polymer Resources PPX-FR3 Modified PPO, UL 94 V-1 with HDT of 265 F
(Unverified Data**) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |