| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Middle Barrel Temperature | 230 °C | 446 °F | |
|
NYCOA 1637 PA 6
plasticized and heat stabilized extrusion grade for the wire jacketing industry to 7,000+ fpm. UL Flammability Component listing for use as cable jacketing.Information provided by NYCOA, Inc.
|
|||
| Middle Barrel Temperature | 230 °C | 446 °F | |
|
NYCOA 2001 PA 6
high melt strength general extrusion and molding grade of nylon 6Information provided by NYCOA, Inc.
|
|||
| Middle Barrel Temperature | 230 °C | 446 °F | |
|
NYCOA 2012 Copolymer Nylon
easy flowing, exceptional toughness and flexibility with lower water absorptionInformation provided by NYCOA, Inc.
|
|||
| Middle Barrel Temperature | 230 °C | 446 °F | |
|
NYCOA 2061 Copolymer Nylon 6/69
monofilament weed eater, fishing lineInformation provided by NYCOA, Inc.
|
|||
| Middle Barrel Temperature | 230 °C | 446 °F | |
|
NYCOA 2062 Copolymer Nylon 6/66
FDA approved extrusion grade for film.Information provided by NYCOA, Inc.
|
|||
| Middle Barrel Temperature | 230 °C | 446 °F | |
|
NYCOA 27/300I Glass Filled Nylon 6
30% glass filled, flame retardant to UL 94 V-0 nylon 6Information provided by NYCOA, Inc.
|
|||
| Middle Barrel Temperature | 230 °C | 446 °F | |
|
NYCOA 534H PA 6
high viscosity, heat stabilized, nucleated nylon for tubing, sheet, film and moldingInformation provided by NYCOA, Inc.
|
|||
| Middle Barrel Temperature | 230 °C | 446 °F | |
|
NYCOA 578 PA 6
very high viscosity molding & extrusion grade for tubing, pipes, film and tapesInformation provided by NYCOA, Inc.
|
|||
| Middle Barrel Temperature | 230 °C | 446 °F | Zone 6; Cylinder |
|
Premix Thermoplastics PRE-ELEC® PE 1291
PRE-ELEC PE 1291 is a conductive thermoplastic compound based on PE-HD. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-ELEC PE 129..
|
|||
| Middle Barrel Temperature | 230 °C | 446 °F | Zone 6; Cylinder |
|
Premix Thermoplastics PRE-ELEC® PE 1294
PRE-ELEC PE 1294 is a conductive thermoplastic compound based on PE-HD. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-ELEC PE 129..
|
|||
| Middle Barrel Temperature | 230 °C | 446 °F | Zone 6; Cylinder |
|
Premix Thermoplastics PRE-ELEC® PP 1386
PRE-ELEC PP 1386 is a conductive thermoplastic compound based on polypropylene. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-ELE..
|
|||
| Middle Barrel Temperature | 230 °C | 446 °F | Zone 4; Cylinder |
|
Premix Thermoplastics PRE-ELEC® PS 1326
PRE-ELEC PS 1326 is a conductive thermoplastic compound based on polystyrene. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-ELEC ..
|
|||
| Middle Barrel Temperature | 230 - 240 °C | 446 - 464 °F | |
|
NHEP Spectron™ E6046 Nylon 6, 15% Glass Fiber
Natural color. E6046 exhibits high rigidity and mechanical strength. It is suitable for wide range of applications. Property data measured at room temperature, 50% RH.Information provided by Bieglo..
|
|||
| Middle Barrel Temperature | 230 °C | 446 °F | Zone 5; Cylinder |
|
Premix Thermoplastics PRE-ELEC® CP 1318
(discontinued **)
PRE-ELEC CP 1318 is a conductive thermoplastic compound based on a polyolefin copolymer. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivit..
|
|||
| Middle Barrel Temperature | 230 - 250 °C | 446 - 482 °F | |
|
Gichem GIBLEND F70X3/VO ABS - Polycarbonate - PC/ABS Flame Retardant
(discontinued **)
Blend PC-ABS self-extinguishing class V0 high fluidity. Medium injection speed.Information provided by GICHEM Gruppo Industriale Chimico
|
|||
| Middle Barrel Temperature | 230 - 260 °C | 446 - 500 °F | Cast Film |
|
Honeywell Aegisâ„¢ H135MP Nylon 6 Extrusion Grade Homopolymer Film
Description: Aegis H135MP is a lubricated and nucleated high viscosity, nylon 6 extrusion grade homopolymer for cast or blown film. It conforms to Food and Drug Administration requirements of 21 CFR..
|
|||
| Middle Barrel Temperature | 230 - 260 °C | 446 - 500 °F | Cast Film |
|
Honeywell Aegisâ„¢ H73QP Nylon 6 Extrusion Grade Homopolymer Film
Description: Aegis H73QP is a lubricated low viscosity, nylon 6 extrusion grade homopolymer for cast coextrusion. If conforms to Food and Drugs Administration requirements of 21 CFR 177.1500 as well..
|
|||
| Middle Barrel Temperature | 230 - 260 °C | 446 - 500 °F | Cast Film |
|
Honeywell Aegisâ„¢ H73ZP Nylon 6 Extrusion Grade Homopolymer Film
Description: Aegis H73ZP is a low viscosity, nylon 6 film extrusion grade homopolymer for cast or blown film. It conforms to Food and Drug Administration requirements of 21 CFR 177.1500 as well as E..
|
|||
| Middle Barrel Temperature | 230 - 250 °C | 446 - 482 °F | Start Point: 240°C |
|
Kingfa PBT-T15 15% Mineral Filled PBT
Features:Excellent size stabilityLow tendency to wrapLow abrasionGood surfaceApplications:Injection moldingApplication partsE & E partsInformation Provided by Kingfa Sci. & Tech. Co., Ltd.
|
|||
| Middle Barrel Temperature | 230 - 250 °C | 446 - 482 °F | Injection Molding |
|
LG Chemical KEYFLEX BT 1072D Ester Type TPE
Description: Injection Molding, TPC-ET, General Purpose, High ModulusApplication: Injection Parts for Automotives, Leisure & SportsCAS: 37282-12-5Information provided by LG Chemical
|
|||
| Middle Barrel Temperature | 230 - 245 °C | 446 - 473 °F | Injection Molding |
|
LG Chemical LUMAX HR5157 PBT+ABS+GF15%, Heat Resistance
Description: Injection Molding Grade, PBT+ABS+GF15%, Heat ResistanceApplication: E&E (CD ROM Tray)CAS: 9003-56-9, 65997-17-3, 24968-12-5 and 25038-59-9Information provided by LG Chemical
|
|||
| Middle Barrel Temperature | 230 - 240 °C | 446 - 464 °F | |
|
LG Chemical Lupox® GP-2000 General Purpose PBT, Unreinforced, Medium Viscosity
LUPOX semi-crystalline thermoplastic PBT resins exhibit properties including high strength, rigidity and good resistance to fatigue and creep at elevated temperatures. Furthermore, LUPOX resins sho..
|
|||
| Middle Barrel Temperature | 230 - 270 °C | 446 - 518 °F | |
|
LG Chemical LUPOY HF-5000 High Flow PC/ABS Alloy, Unreinforced
Among the characteristics of LUPOY polycarbonate resins are excellent mechanical properties, high heat resistance, high impact strength, and dimensional stability.Applications:Automotive: Automotive..
|
|||
| Middle Barrel Temperature | 230 - 260 °C | 446 - 500 °F | |
|
Gromax 1172LL TPE
1172LL is high modulus grade with nominal Durometer hardness of 72D. It contains color stable antioxidants. It can be processed by thermoplastic processing techniques like blow molding grade. Charac..
|
|||
| Middle Barrel Temperature | 230 - 250 °C | 446 - 482 °F | Start Point: 235°C |
|
Kingfa MAC-701 PC/ABS Alloy
Features:Excellent balance propertiesHigh impact strengthGood electro-plating propertiesGood processing propertiesApplications:Injection moldingAutomobile instrument panelElectrical and electronic p..
|
|||
| Middle Barrel Temperature | 230 - 250 °C | 446 - 482 °F | Start Point: 240°C |
|
Kingfa PBT-G15 15% Glass Fiber Reinforced PBT
Features:Good size stabilityHigh mechanical propertiesHigh heat resistanceExcellent balance propertiesApplications:Injection moldingApplication partsAuto handleDoor latchE & E partsInformation Provi..
|
|||
| Middle Barrel Temperature | 230 - 250 °C | 446 - 482 °F | Start Point: 240°C |
|
Kingfa PBT-R0N Flame Retardant PBT
Features:Flame retardantGood chemical resistanceOutstanding surfaceEasy processingHigh impactApplications:Injection moldingConnectors, terminal blocksRelay, switchBobbinsPlugsE & E partsInformation ..
|
|||
| Middle Barrel Temperature | 230 - 240 °C | 446 - 464 °F | |
|
Solvay Technyl® C 216 Nylon 6, 30% Glass Fiber, EH0
Polyamide PA6, reinforced with 30% of glass fiber, for injection molding.It has good mechanical properties. It is used in all sectors of industry, offering an excellent combination between thermal ..
|
|||
| Middle Barrel Temperature | 230 °C | 446 °F | Extrusion Coating |
|
DuPont Appeel® LSR20D752 Lidding Sealant Resin
Appeel® LSR20D752 is a modified ethylene acrylate copolymer designed to function as a sealing layer for lidding applications. It is most often suggested to provide peelable seals over a broad tempe..
|
|||
| Middle Barrel Temperature | 230 - 240 °C | 446 - 464 °F | Zone 2 |
|
Eurostar Staramide BST01 PA6, Impact Modified, Injection Molded
BST01 is an Impact Modified Polyamide 6 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier.
|
|||