Polymer Property : Middle Barrel Temperature = 255 °C Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Middle Barrel Temperature 240 - 255 °C
464 - 491 °F
Honeywell Aegis™ PL56HS High Viscosity, Heat Stabilized, Flexible Nylon 6/66 Copolymer  (discontinued **)
Description: Aegis PL56HS is a high viscosity, heat stabilized, flexible nylon 6/66 copolymer. It possesses a balance of flexibility, toughness and abrasion resistance. Combined with its high melt v..
Middle Barrel Temperature 240 - 255 °C
464 - 491 °F
Honeywell Aegis™ PL75HS Medium Viscosity, Heat Stabilized, Flexible Nylon 6  (discontinued **)
Description: Aegis PL75HS is a medium viscosity, heat stabilized, flexible nylon 6 especially suited to the production of extrusion profiles offering a combination of good flexibility, toughness and..
Middle Barrel Temperature 230 - 255 °C
446 - 491 °F
Start Point: 225°C
Kingfa JH960 6300 Non-halogenated Flame Retardant PC/ABS Alloy
Features:Halogen free flame retardant, V-0/1.5mm5VB/1.6mm, 5VA/3.2mmExcellent balance propertiesHigh heat resistanceGood chemical resistanceGood hydrolysis resistanceSuit for paint and electo-platin..
Middle Barrel Temperature 235 - 255 °C
455 - 491 °F
Start Point: 245°C
Kingfa PBT-G30 30% Glass Fiber Reinforced PBT
Features:Good size stabilityHigh mechanical propertiesHigh heat resistanceExcellent balance propertiesApplications:Injection moldingApplication partsAuto handleDoor latchE & E partsInformation Provi..
Middle Barrel Temperature 235 - 255 °C
455 - 491 °F
Start Point: 245°C
Kingfa PBT-RG20 Flame Retardant, 20% Glass Fiber Reinforced PBT
Features:Flame retardantHigh strengthHigh temperature propertiesOutstanding electrical propertiesGood heat resistanceApplications:Injection moldingConnectorsRelayBobbins, plugsE & E partsInformation..
Middle Barrel Temperature 235 - 255 °C
455 - 491 °F
Start Point: 245°C
Kingfa PBT-RG30 Flame Retardant, 30% Glass Fiber Reinforced PBT
Features:Flame retardantHigh strengthHigh temperature propertiesOutstanding electrical propertiesGood heat resistanceApplications:Injection moldingConnectorsRelayBobbins, plugsE & E partsInformation..
Middle Barrel Temperature 240 - 255 °C
464 - 491 °F
Injection Molding
Ineos ABS Lustran® 288 ABS, Injection Molding Grade
Lustran® ABS 288 is a very high-flow injection molding grade of ABS (acrylonitrile butadiene styrene) with good impact strength and high gloss. It is intended for use in a wide range of applicati..
Middle Barrel Temperature 240 - 255 °C
464 - 491 °F
Injection Molding
Ineos ABS Lustran® 308 ABS, Medical Grade
Lustran® ABS 308 resin is a low gloss, easy-flowing grade of ABS (acrylonitrile butadiene styrene). This injection molding grade offers a good balance of rigidity, impact strength, and abuse resi..
Middle Barrel Temperature 240 - 255 °C
464 - 491 °F
Injection Molding
Ineos ABS Lustran® ABS 248FC Medical & Food Contact Grade
Lustran® ABS 248FC resin is a high-gloss, medium-impact grade of ABS (acrylonitrile butadiene styrene). This injection molding grade offers a good balance of physical properties and has been desi..
Middle Barrel Temperature 235 - 255 °C
455 - 491 °F
Injection Molding
LG Chemical LUPOY GN5001RFT PC/ABS, Halogen Free Flame Retardant
Description: Injection Molding, PC/ABS, Halogen Free Flame Retardant, Good FlowApplication: E&E (TV, Navigation Housing)CAS: 103598-77-2, 9003-56-9 and 181028-79-5Information provided by LG Chemical..
Middle Barrel Temperature 235 - 255 °C
455 - 491 °F
Injection Molding
LG Chemical LUPOY GN5008HF PC/ABS, Halogen Free Flame Retardant, High Impact
Description: Injection Molding, PC/ABS, Halogen Free Flame Retardant, Heat Resistance, High FlowApplication: E&E (OA, Navigation Housing)CAS: 103598-77-2, 9003-56-9 and 181028-79-5Information provid..
Middle Barrel Temperature 235 - 255 °C
455 - 491 °F
Injection Molding
LG Chemical LUPOY GP5008A PC/ABS
Description: Injection Molding, PC/ABS, General Purpose, High FlowApplication: Miscellaneous GoodsCAS: 103598-77-2, 9003-56-9 and 181028-79-5Information provided by LG Chemical
Middle Barrel Temperature 235 - 255 °C
455 - 491 °F
Injection Molding
LG Chemical LUPOY GP5100 PC/ABS+GF10%
Description: Injection Molding, PC/ABS+GF10%, General Purpose, GF ReinforcedApplication: Electrical Appliance Housing, Automotive I/PCAS: 103598-77-2, 9003-56-9 and 65997-17-3Information provided by..
Middle Barrel Temperature 235 - 255 °C
455 - 491 °F
Injection Molding
LG Chemical LUPOY GP5106F PC/ABS+GF10%, Flame Retardance
Description: Injection Molding, PC/ABS+GF10%, Flame RetardanceApplication: IT/OA (Housing)CAS: 103598-77-2, 9003-56-9, 68928-70-1, 1309-64-4 and 65997-17-3Information provided by LG Chemical
Middle Barrel Temperature 235 - 255 °C
455 - 491 °F
Injection Molding
LG Chemical LUPOY GP5206F PC/ABS+GF20%, Flame Retardance
Description: Injection Molding, PC/ABS+GF20%, Flame Retardance, General PurposeApplication: IT/OA (Housing)CAS: 103598-77-2, 9003-56-9, 68928-70-1, 1309-64-4 and 65997-17-3Information provided by LG..
Middle Barrel Temperature 235 - 255 °C
455 - 491 °F
Start Point: 245°C
Kingfa PBT-RG151 Flame Retardant, 15% Glass Fiber Reinforced PBT
Features:Flame retardantHigh strengthHigh temperature propertiesGood electric propertiesExcellent size stabilityNo bloomingApplications:Injection moldingConnectorsRelayBobbinsPlugsE & E partsInforma..
Middle Barrel Temperature 235 - 255 °C
455 - 491 °F
Injection Molding
LG Chemical LUPOY GN5001RF PC/ABS, Halogen Free Flame Retardant
Description: Injection Molding, PC/ABS, Halogen Free Flame Retardant, Good FlowApplication: E&E (TV, Navigation Housing)CAS: 103598-77-2, 9003-56-9 and 181028-79-5Information provided by LG Chemical..
Middle Barrel Temperature 235 - 255 °C
455 - 491 °F
Injection Molding
LG Chemical LUPOY GN5001RFJ PC/ABS, Halogen Free Flame Retardant
Description: Injection Molding, PC/ABS, Halogen Free Flame Retardant, High FlowApplication: IT/OA (OA Housing)CAS: 103598-77-2, 9003-56-9 and 181028-79-5Information provided by LG Chemical
Middle Barrel Temperature 235 - 255 °C
455 - 491 °F
Injection Molding
LG Chemical LUPOY GN5101RF PC/ABS Mineral Filler
Description: Injection Molding, PC/ABS Mineral Filler, General Purpose, High Stiffness, Halogen Free Flame RetardantApplication: E&E (Housing), IT/OA (Notebook PC Housing)CAS: 103598-77-2, 9003-56-9..
Middle Barrel Temperature 245 - 255 °C
473 - 491 °F
Solvay Technyl® B 50H1 Nylon 66/6, Flame Retardant, EH0
Flame retardant copolyamide 66/6, unreinforced, heat stabilized, for injection molding.This phosphorus and halogen free flame retardant grade, UL 94 VO (0.4 mm), offers excellent filling qualities a..
Middle Barrel Temperature 250 - 255 °C
482 - 491 °F
Compression Zone
Solvay Technyl® C 218 MT25 V15 25% Mineral, 15% Glass Filled, Heat Stabilized Nylon 6
Information provided by Rhodia; Rhodia has been acquired by Solvay.
Middle Barrel Temperature 225 - 255 °C
437 - 491 °F
Beijing Chemical Industry KAIFA® 201-G20R PBT Resin
15% glass fiber reinforced, good flow and toughnessInformation provided by Beijing Chemical Industry Research Institute (Group)
Middle Barrel Temperature 225 - 255 °C
437 - 491 °F
Beijing Chemical Industry KAIFA® 201-G30R PBT Resin
30% glass fiber reinforced, good flow and toughnessInformation provided by Beijing Chemical Industry Research Institute (Group)
Middle Barrel Temperature 225 - 255 °C
437 - 491 °F
Beijing Chemical Industry KAIFA® 201-G30 PBT Resin
30% glass fiber reinforcedInformation provided by Beijing Chemical Industry Research Institute (Group)
Middle Barrel Temperature 225 - 255 °C
437 - 491 °F
Beijing Chemical Industry KAIFA® 301-G15RF PBT Resin
15% glass fiber reinforced, flame retardant, good toughness, low bleedingInformation provided by Beijing Chemical Industry Research Institute (Group)