Material Notes:
Description: Aegis H100QP is a lubricated medium viscosity, Nylon 6 film extrusion grade homopolymer for cast or blown film. It conforms to FDA requirements of 21 CFR 177.1500 as well as EU Directive 2002/72/EC. It possesses the combination of strength, toughness and thermo-forming properties associated with Nylon 6 as well as excellent heat, chemical, and abrasion resistance.Applications:Processed MeatFresh Red MeatPoultryFishCheeseDried FoodChilled Fruit JuicesInformation provided by Honeywell.
Physical Properties Metric English Comments
Specific Gravity 1.13 g/cc
1.13 g/cc
ASTM D1505
Water Absorption 0.70 %
0.70 %
Extractable Content
1.6 %
1.6 %
in 24 hours
Moisture Absorption at Equilibrium 2.7 %
2.7 %
at 50% RH
Water Absorption at Saturation 9.5 %
9.5 %
Oxygen Transmission Rate 40.3 cc/m²/day
2.60 cc/100 in²/day
Nitrogen Transmission 14.0 cc-mm/m²-24hr-atm
35.6 cc-mil/100 in²-24hr-atm
cc/m²/day, No thickness given
Carbon Dioxide Transmission 72.8 cc-mm/m²-24hr-atm
185 cc-mil/100 in²-24hr-atm
cc/m²/day, No thickness given
Viscosity Measurement 3.35
3.35
96% SAV
100
100
FAV; ASTM D789
Maximum Moisture Content 0.080
0.080
Melt Flow 2.6 g/10 min

@Load 1.00 kg,
Temperature 235 °C
2.6 g/10 min

@Load 2.20 lb,
Temperature 455 °F
ASTM D1238
Thermal Properties Metric English Comments
Melting Point 220 °C
428 °F
ASTM D3418
Processing Properties Metric English Comments
Middle Barrel Temperature 230 - 260 °C
446 - 500 °F
Cast Film
246 - 254 °C
475 - 489 °F
Tubular (Blown) Film
Adapter Temperature 260 °C
500 °F
Tubular (Blown) Film
260 - 266 °C
500 - 511 °F
Cast Film
Die Temperature 254 °C
490 °F
Tubular (Blown) Film
260 °C
500 °F
Cast Film
Melt Temperature 254 - 260 °C
489 - 500 °F
Tubular (Blown) Film
260 - 270 °C
500 - 518 °F
Cast Film
Moisture Content 0.040 %
0.040 %
Users viewing this material also viewed the following: