Processing Properties | Metric | English | Comments |
---|---|---|---|
Middle Barrel Temperature | 165 - 190 °C | 329 - 374 °F | Extrusion |
Huntsman IROGRAN® A 78 E 4506 TPU-Polyester Introduction: IROGRAN A 78 E 4506 is a thermoplastic polyester- polyurethane for injection molding and extrusion applications. Additional characteristics of the product are excellent mechanical prop.. |
|||
Middle Barrel Temperature | 165 - 190 °C | 329 - 374 °F | Extrusion |
Huntsman IROGRAN® A 85 E 4607 E TPU-Polyester Introduction: IROGRAN A 85 E 4607 is a thermoplastic polyether- polyurethane intended for extrusion and injection molding applications. Additional characteristics of the product are excellent mechan.. |
|||
Middle Barrel Temperature | 165 - 190 °C | 329 - 374 °F | Extrusion |
Huntsman IROGRAN® A 85 P 4722 TPU-Polyester Introduction: IROGRAN A 85 P 4722 is a halogen-free thermoplastic- polyurethane for injection molding and extrusion applications. Additional characteristics of the product are good microbial resista.. |
|||
Middle Barrel Temperature | 170 - 190 °C | 338 - 374 °F | Start Point: 180°C |
Kingfa HF-606 Flame Retardant ABS Features:UL 94 V-0 @ 1.6-3.0mm, 5VB @ 2.0mmHigh flowModerate UV stabilityHigh stiffnessApplications:Injection moldingMonitor cabinetCD-ROMPower switchInformation Provided by Kingfa Sci. & Tech. Co.,.. |
|||
Middle Barrel Temperature | 170 - 190 °C | 338 - 374 °F | Start Point: 180°C |
Kingfa HF-618 Flame Retardant ABS Features:UL 94 V-0 @ 1.6-3.0mmHigh toughnessEasy flowApplications:Injection moldingShell of applianceCD-ROMPower switchInformation Provided by Kingfa Sci. & Tech. Co., Ltd. |
|||
Middle Barrel Temperature | 170 - 190 °C | 338 - 374 °F | Injection Molding |
LG Chemical KEYFLEX BT 3140D Ester Type TPE Description: Injection Molding, TPC-ET, Specialty, Low Melting Temperature, Low ModulusApplication: Masterbatch Carrier, Cable Compound BaseCAS: 37282-12-5Information provided by LG Chemical |
|||
Middle Barrel Temperature | 170 - 190 °C | 338 - 374 °F | Injection Molding |
LG Chemical LUCEL FW700N Modified POM, Friction Resistance, Abrasion Resistance Feature: Injection Molding, Modified POM, Friction Resistance, Abrasion ResistanceApplication: Gears, Printer Roller Pumps, Gear Worm WheelsCAS No. 66455-31-0Information provided by LG Chemical |
|||
Middle Barrel Temperature | 170 - 190 °C | 338 - 374 °F | Injection Molding |
LG Chemical LUCEL FW700S Modified POM, Friction Resistance, Abrasion Resistance Feature: Injection Molding, Modified POM, Friction Resistance, Abrasion ResistanceApplication: Gears, Printer Roller Pumps, Gear Worm WheelsCAS No. 66455-31-0Information provided by LG Chemical |
|||
Middle Barrel Temperature | 170 - 190 °C | 338 - 374 °F | Injection Molding |
LG Chemical LUCEL FW715CS Modified POM, Friction Resistance, Abrasion Resistance Feature: Injection Molding, Modified POM, Friction Resistance, Abrasion ResistanceApplication: Gears, Printer Roller Pumps, Gear Worm WheelsCAS No. 66455-31-0 and 471-34-1Information provided by LG .. |
|||
Middle Barrel Temperature | 170 - 190 °C | 338 - 374 °F | Injection Molding |
LG Chemical LUCEL FW720F Modified POM, Friction Resistance, Abrasion Resistance Feature: Injection Molding, Modified POM, Friction Resistance, Abrasion ResistanceApplication: Gears, Printer Roller Pumps, Gear Worm WheelsCAS No. 66455-31-0 and 9002-84-2Information provided by LG.. |
|||
Middle Barrel Temperature | 170 - 190 °C | 338 - 374 °F | Injection Molding |
LG Chemical LUCEL HI515W POM+Rubber, High Impact Feature: Injection Molding, POM+Rubber, High ImpactApplication: Gears, Automobile ClipCAS No. 66455-31-0 and 155123-66-3Information provided by LG Chemical |
|||
Middle Barrel Temperature | 170 - 190 °C | 338 - 374 °F | Injection Molding |
LG Chemical LUCEL HI520 POM+Rubber, High Impact Feature: Injection Molding, POM+Rubber, High ImpactApplication: GearsCAS No. 66455-31-0 and 155123-66-3Information provided by LG Chemical |
|||
Middle Barrel Temperature | 170 - 190 °C | 338 - 374 °F | Injection Molding |
LG Chemical LUCEL HI525L POM+Rubber, High Impact Feature: Injection Molding, POM+Rubber, High ImpactApplication: GearsCAS No. 66455-31-0 and 155123-66-3Information provided by LG Chemical |
|||
Middle Barrel Temperature | 165 - 190 °C | 329 - 374 °F | |
Huntsman AVALON® 65 AC Thermoplastic Polyurethane Introduction: AVALON 65 AC is a polyester based thermoplastic polyurethane for injection molding. AVALON 65 AC is part of the AVALON Crystal Range and offers a specially designed transparent materia.. |
|||
Middle Barrel Temperature | 180 - 190 °C | 356 - 374 °F | |
Huntsman AVALON® 65 AE Thermoplastic Polyurethane Introduction: AVALON 65 AE is a polyester based thermoplastic polyurethane for injection molding. AVALON 65 AE is part of the AVALON Soft Range and offers a premium soling material for casual, sport.. |
|||
Middle Barrel Temperature | 175 - 190 °C | 347 - 374 °F | |
Huntsman AVALON® 70 AE Thermoplastic Polyurethane Introduction: AVALON 70 AE is a general purpose polyester based thermoplastic polyurethane for injection molding. AVALON 70 AE is part of the AVALON Soft Range and offers a premium soiling material .. |
|||
Middle Barrel Temperature | 180 - 190 °C | 356 - 374 °F | |
Huntsman AVALON® 75 AE Thermoplastic Polyurethane Introduction: AVALON 75 AE is a general purpose polyester based thermoplastic polyurethane for injection molding. AVALON 75 AE is part of the AVALON Soft Range and offers a premium soiling material .. |
|||
Middle Barrel Temperature | 165 - 190 °C | 329 - 374 °F | Extrusion |
Huntsman IROGRAN® A 88 H 4622 TPU-Polyester Introduction: IROGRAN A 88 H 4622 is a black colored thermoplastic polyether/polyester-polyurethane for injection molding and extrusion applications. Additional characteristics of the product are hi.. |
|||
Middle Barrel Temperature | 170 - 190 °C | 338 - 374 °F | Start Point: 180°C |
Kingfa FRABS-518 Flame Retardant ABS Features:UL 94 V-0 @ 1.6-3.0mm, 5VB @ 2.0mmLow temperature impact resistanceApplications:Injection moldingPower tools accessoriesInformation Provided by Kingfa Sci. & Tech. Co., Ltd. |
|||
Middle Barrel Temperature | 170 - 190 °C | 338 - 374 °F | Injection Molding |
Stellarchem DIOSHY® MP-960NC TPE Compound This grade of Stellarchem MP series is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, styrene block copolymers based, .. |
|||
Middle Barrel Temperature | 170 - 190 °C | 338 - 374 °F | Injection Molding |
Stellarchem LP-830 TPE Compound This grade of Stellarchem LP series is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, styrene block copolymers based, .. |
|||
Middle Barrel Temperature | 170 - 190 °C | 338 - 374 °F | Injection Molding |
Stellarchem SV-B40D TPV Compound This grade of Stellarchem SV series is a dynamic crosslinked, EPDM/PP compound. It's design to replace thermoset elastomers, such as EPDM, and traditional Thermoplastic TPVs. It can be process on .. |
|||
Middle Barrel Temperature | 170 - 190 °C | 338 - 374 °F | Injection Molding |
Stellarchem SV-B65E TPV Compound This grade of Stellarchem SV series is a dynamic crosslinked, EPDM/PP compound. It's design to replace thermoset elastomers, such as EPDM, and traditional Thermoplastic TPVs. It can be process on .. |
|||
Middle Barrel Temperature | 170 - 190 °C | 338 - 374 °F | Injection Molding |
Stellarchem SV-B70E TPV Compound This grade of Stellarchem SV series is a dynamic crosslinked, EPDM/PP compound. It's design to replace thermoset elastomers, such as EPDM, and traditional Thermoplastic TPVs. It can be process on .. |
|||
Middle Barrel Temperature | 170 - 190 °C | 338 - 374 °F | Injection Molding |
Stellarchem SV-B75E TPV Compound This grade of Stellarchem SV series is a dynamic crosslinked, EPDM/PP compound. It's design to replace thermoset elastomers, such as EPDM, and traditional Thermoplastic TPVs. It can be process on .. |
|||
Middle Barrel Temperature | 170 - 190 °C | 338 - 374 °F | Injection Molding |
Stellarchem SV-B87E TPV Compound This grade of Stellarchem SV series is a dynamic crosslinked, EPDM/PP compound. It's design to replace thermoset elastomers, such as EPDM, and traditional Thermoplastic TPVs. It can be process on .. |
|||
Middle Barrel Temperature | 170 - 190 °C | 338 - 374 °F | |
Borealis BS2581 High Density Polyethylene for Blow Molding BS2581 is a high density polyethylene intended for blow molding products with high stiffness and very good environmental stress crack resistance (ESCR). Applications: industrial chemicals, househol.. |
|||
Middle Barrel Temperature | 170 - 190 °C | 338 - 374 °F | Mid-2. Region Temperature |
Tisan TISETILEN® Flame Retardant (V0) Polyethylene TISETILEN has a wide area of application in construction, building auxiliary materials, lighting equipment, household appliance, toy industries, etc. General specifications include Low densityFlexib.. |
|||
Middle Barrel Temperature | 170 - 190 °C | 338 - 374 °F | Mid-2. Region Temperature |
Tisan TISETILEN® UNR Polyethylene TISETILEN has a wide area of application in construction, building auxiliary materials, lighting equipment, household appliance, toy industries, etc. General specifications include Low densityFlexib.. |
|||
Middle Barrel Temperature | 170 - 190 °C | 338 - 374 °F | |
Borealis BS2541 High Density Polyethylene BS2541 is a high density polyethylene with very high ESCR This product is intended for blow molding. Applications: household and chemical containers such as detergents, cleaners, and motor oils, an.. |