| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.38 g/cc | 1.38 g/cc | ASTM D792 |
| Maximum Moisture Content | 0.10 | 0.10 | Injection Molding |
| Linear Mold Shrinkage, Flow | 0.017 - 0.020 cm/cm @Thickness 3.20 mm |
0.017 - 0.020 in/in @Thickness 0.126 in |
ASTM D955 |
| Melt Flow | 7.0 g/10 min @Load 2.16 kg, Temperature 190 °C |
7.0 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Rockwell R | 60 | 60 | ASTM D785 |
| Tensile Strength, Yield | 41.2 MPa @Thickness 3.20 mm |
5970 psi @Thickness 0.126 in |
50mm/min; ASTM D638 |
| Elongation at Break | 150 % @Thickness 3.20 mm |
150 % @Thickness 0.126 in |
50mm/min; ASTM D638 |
| Flexural Yield Strength | 53.9 MPa @Thickness 3.20 mm |
7820 psi @Thickness 0.126 in |
1.3mm/min; ASTM D790 |
| Flexural Modulus | 1.47 GPa @Thickness 3.20 mm |
213 ksi @Thickness 0.126 in |
1.3mm/min; ASTM D790 |
| Izod Impact, Notched | 1.77 J/cm @Thickness 6.40 mm, Temperature 23.0 °C |
3.31 ft-lb/in @Thickness 0.252 in, Temperature 73.4 °F |
ASTM D256 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Deflection Temperature at 0.46 MPa (66 psi) | 135 °C @Thickness 6.40 mm |
275 °F @Thickness 0.252 in |
Unannealed; ASTM D648 |
| Deflection Temperature at 1.8 MPa (264 psi) | 85.0 °C @Thickness 6.40 mm |
185 °F @Thickness 0.252 in |
Unannealed; ASTM D648 |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Volume Resistivity | 1.00e+15 ohm-cm | 1.00e+15 ohm-cm | ASTM D257 |
| Surface Resistance | 1.00e+13 ohm | 1.00e+13 ohm | ASTM D257 |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Rear Barrel Temperature | 160 - 180 °C | 320 - 356 °F | Injection Molding |
| Middle Barrel Temperature | 170 - 190 °C | 338 - 374 °F | Injection Molding |
| Front Barrel Temperature | 180 - 200 °C | 356 - 392 °F | Injection Molding |
| Nozzle Temperature | 180 - 200 °C | 356 - 392 °F | Injection Molding |
| Melt Temperature | 200 - 220 °C | 392 - 428 °F | Injection Molding |
| Mold Temperature | 80.0 - 110 °C | 176 - 230 °F | Injection Molding |
| Drying Temperature | 90.0 - 110 °C | 194 - 230 °F | Injection Molding |
| Dry Time | 2.00 - 3.00 hour | 2.00 - 3.00 hour | Injection Molding |
| Back Pressure | 0.490 - 3.04 MPa | 71.1 - 441 psi | Injection Molding |
| Screw Speed | 50 - 100 rpm | 50 - 100 rpm | Injection Molding |