Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Huntsman AVALON® 70 AE Thermoplastic Polyurethane

Category Polymer , Thermoplastic , Polyurethane, TP , Thermoplastic Polyurethane (TPUR), Polyester Grade
Manufacturer Huntsman Corporation
Trade Name Avalon®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Huntsman AVALON® 70 AE Thermoplastic Polyurethane.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Introduction: AVALON 70 AE is a general purpose polyester based thermoplastic polyurethane for injection molding. AVALON 70 AE is part of the AVALON Soft Range and offers a premium soiling material for casual, sport and protect foot wear. The features offered include:Cut & scratch resistanceRapid processingAbrasion resistanceCold flex resistancePhthalate free TPU Information provided by Alliance Polymers
Physical Properties Metric English Comments
Density 1.21 g/cc
0.0437 lb/in³
ISO 2781
Mechanical Properties Metric English Comments
Hardness, Shore A 70
70
ISO 868
Tensile Strength at Break 22.0 MPa
3190 psi
ISO 37
Elongation at Break 700 %
700 %
ISO 37
100% Modulus 0.00300 GPa
0.435 ksi
ISO 37
300% Modulus 0.00500 GPa
0.725 ksi
ISO 37
Tear Strength 65.0 kN/m
371 pli
ISO 34B
Abrasion 35
35
mm<sup>3</sup>; ISO 4649
Compression Set 20 %
20 %
ISO 815
Processing Properties Metric English Comments
Feed Temperature 25.0 - 35.0 °C
77.0 - 95.0 °F
Rear Barrel Temperature 170 - 185 °C
338 - 365 °F
Middle Barrel Temperature 175 - 190 °C
347 - 374 °F
Front Barrel Temperature 180 - 195 °C
356 - 383 °F
Nozzle Temperature 175 - 190 °C
347 - 374 °F
Mold Temperature 25.0 - 50.0 °C
77.0 - 122 °F
Injection Pressure 2.00 - 10.0 MPa
290 - 1450 psi
Hold Pressure 1.00 - 5.00 MPa
145 - 725 psi
Back Pressure 0.0300 - 0.300 MPa
4.35 - 43.5 psi
Screw Speed 20 - 80 rpm
20 - 80 rpm
Descriptive Properties Value Comments
Compression Ratio 2-3:1
L/D Ratio 20-25:1
Ross Flex -10°C, BS 5131
Typical Screw Diameter 40-120 nm