Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched (ISO) | 28.0 kJ/m² | 13.3 ft-lb/in² | ISO 180 |
Solvay Specialty Polymers AvaSpire® AV-742 SL30 Polyaryletherketone (PAEK)
(Unverified Data**) AV-742 SL30 is a wear resistant grade of AvaSpire polyaryletherketone (PAEK) designed to provide low wear rates in both non-lubricated and lubricated environments. In addition to outstanding wear re.. |
|||
Izod Impact, Unnotched (ISO) | 28.0 kJ/m² | 13.3 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP LUBRICOMP DCP32 PC LNP* Lubricomp* DCP32 is a compound based on Polycarbonate resin containing 15% PTFE/Silicone, 10% Carbon Fiber. Added features of this material include: Electrically Conductive, Internally Lubrica.. |
|||
Izod Impact, Unnotched (ISO) | 28.0 - 90.0 kJ/m² @Temperature -30.0 - -30.0 °C |
13.3 - 42.8 ft-lb/in² @Temperature -22.0 - -22.0 °F |
Average value: 52.3 kJ/m² Grade Count:6 |
Overview of materials for Nylon 66, 10% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 10% Glass Fiber Filled". Specific grades with glass content between 5% and 14% are included. .. |
|||
Izod Impact, Unnotched (ISO) | 28.0 kJ/m² | 13.3 ft-lb/in² | |
Idemitsu Kosan Xarec® EA 537 SPS, 30% Glass Filled Crystalline Polymer, Glass Filled, Ignition Resistant, Impact Modified. Used in Electronic and Electrical applications |
|||
Izod Impact, Unnotched (ISO) | 28.0 kJ/m² | 13.3 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics NORYL SE1GFN2 PPE+PS (Asia Pacific) PPE+PS blend. 20% Glass reinforced. Non-brominated, non-chlorinated FR system. UL94 V1 listing. Dielectric strength. Dimensional stability. Suitable for E/E applications. |
|||
Izod Impact, Unnotched (ISO) | 28.0 kJ/m² | 13.3 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP LUBRICOMP OCP34E PPS - Linear LNP LUBRICOMP* OCP34E is a compound based on PPS - Linear resin containing 20% Carbon Fiber, 15% PTFE/Silicone. Added features of this material include: Easy Molding, Electrically Conductive, Wear .. |
|||
Izod Impact, Unnotched (ISO) | 28.0 kJ/m² | 13.3 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP LUBRICOMP OCP34E PPS - Linear (Asia Pacific) LNP LUBRICOMP* OCP34E is a compound based on PPS - Linear resin containing Silicone, Carbon Fiber, PTFE. Added features of this material include: Easy Molding. |
|||
Izod Impact, Unnotched (ISO) | 28.0 kJ/m² | 13.3 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP LUBRICOMP RX03643H PA 66 LNP* LUBRICOMP* RX03643H is a compound based on Nylon 66 resin containing Proprietary Filler(s). Added feature of this material is: Wear Resistant. |
|||
Izod Impact, Unnotched (ISO) | 28.0 kJ/m² | 13.3 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP LUBRICOMP RX03643H PA 66 (Asia Pacific) LNP* Lubricomp* RX03643H is a compound based on Nylon 66 resin containing Proprietary Filler(s). Added features of this material include: Internally Lubricated. |
|||
Izod Impact, Unnotched (ISO) | 28.0 kJ/m² | 13.3 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP LUBRICOMP ZFG26 PPE+PS LNP* LUBRICOMP* ZFG26 is a compound based on PPE+PS resin containing 30% Glass Fiber, 10% Graphite. Added features of this material include: Wear Resistant. |
|||
Izod Impact, Unnotched (ISO) | 28.0 kJ/m² | 13.3 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP LUBRICOMP ZFG26 PPE+PS (Asia Pacific) LNP* Lubricomp* ZFG26 is a compound based on PPE+PS Blend resin containing Glass Fiber, Graphite Powder. Added features of this material include: Internally Lubricated. |
|||
Izod Impact, Unnotched (ISO) | 28.0 kJ/m² | 13.3 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP LUBRICOMP ZFL24 PPE+PS LNP* LUBRICOMP* ZFL24 is a compound based on PPE+PS resin containing 20% Glass Fiber, 10% PTFE. Added feature of this grade is: Wear Resistant. |
|||
Izod Impact, Unnotched (ISO) | 28.0 kJ/m² @Temperature 23.0 °C |
13.3 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP Lubricomp ZFL24 PPO LNP* Lubricomp* ZFL24 is a compound based on Modified Polyphenylene Oxide (PPO) containing glass fiber and PTFE lubricant. Characteristics of this grade are: Internally Lubricated.This data was su.. |
|||
Izod Impact, Unnotched (ISO) | 28.0 kJ/m² | 13.3 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP STAT-KON DE0049P PC (Asia Pacific) LNP* Stat-kon* DE0049P is a compound based on Polycarbonate resin containing Flame Retardant, Carbon Fiber. Added features of this material include: Exceptional Processing, Flame Retardant. |
|||
Izod Impact, Unnotched (ISO) | 28.0 kJ/m² | 13.3 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics Valox® 4012 PBT (Europe-Africa-Middle East) VALOX 4012 is a 10% high strength glass fibre reinforced PBT injection moulding resin with improved mechanical properties. Applications: connectors. |
|||
Izod Impact, Unnotched (ISO) | 28.0 kJ/m² @Temperature 0.000 °C, Time 86400 sec |
13.3 ft-lb/in² @Temperature 32.0 °F, Time 24.0 hour |
|
Shandong Rike Chemical HELIâ„¢ HL-769 Weather-resistance Acrylic Impact Modifier (AIM) Outline of ACR Impact Modifiers:The PVC impact modifiers developed by our company are acrylic copolymers (ACR) with a core-shell structure, their cores are acrylic ester and shells are methacrylic c.. |
|||
Izod Impact, Unnotched (ISO) | 28.0 kJ/m² | 13.3 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP THERMOCOMP DE004ERP PC LNP* Thermocomp* DE004ERP is a compound based on Polycarbonate resin containing 20% Carbon Fiber. Added features include: Electrically Conductive, Easy Molding, Mold Release. |
|||
Izod Impact, Unnotched (ISO) | 28.0 kJ/m² | 13.3 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP THERMOCOMP DE004ERP PC (Asia Pacific) LNP* Thermocomp* DE004ERP is a compound based on Polycarbonate resin containing Carbon Fiber. Added features of this material include: Electrically Conductive, Easy Molding, Mold Release. |
|||
Izod Impact, Unnotched (ISO) | 28.0 kJ/m² | 13.3 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP THERMOCOMP SH0430AC_BK1D466 PA12 4.3 specific gravity nylon 12, clean compound system |
|||
Izod Impact, Unnotched (ISO) | 28.0 kJ/m² | 13.3 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP THERMOCOMP TH0750A PUR LNP THERMOCOMP* TH0750A is a compound based on Polyurethane resin. Added features of this material include: High Specific Gravity. |
|||
Izod Impact, Unnotched (ISO) | 28.0 kJ/m² @Temperature 23.0 °C |
13.3 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP Thermocomp WC006 Polyester, TP LNP* Thermocomp* WC006 is a compound based on Polyester, TP resin containing Carbon Fiber.This data was supplied by SABIC-IP for the Americas region. |
|||
Izod Impact, Unnotched (ISO) | 28.0 kJ/m² | 13.3 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP THERMOCOMP WC006 Polyester, TP (Asia Pacific) LNP* Thermocomp* WC006 is a compound based on Polyester, TP resin containing Carbon Fiber. |
|||
Izod Impact, Unnotched (ISO) | 28.0 kJ/m² | 13.3 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP STAT-KON DE0049P PC LNP* STAT-KON* DE0049P is a compound based on Polycarbonate resin containing 20% Carbon Fiber. Added features of this material include: Exceptional Processing, Flame Retardant. Electrically Conduct.. |
|||
Izod Impact, Unnotched (ISO) | 28.0 kJ/m² | 13.3 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP STAT-KON OE006A PPS - Branched LNP STAT-KON* OE006A is a compound based on PPS - Branched resin containing 30% Carbon Fiber. Added features of this material include: Electrically Conductive. |
|||
Izod Impact, Unnotched (ISO) | 28.0 kJ/m² | 13.3 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP THERMOCOMP MF003AS PP LNP* THERMOCOMP* MF003AS is a compound based on Polypropylene containing 15% Glass Fiber. Characteristics of this grade are: Heat Stabilized. |
|||
Izod Impact, Unnotched (ISO) | 28.0 kJ/m² | 13.3 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP THERMOTUF MF004AI PP LNP* Thermotuf* MF004AI is a compound based on Polypropylene resin containing Glass Fiber. Added features of this material include: High Impact. |
|||
Izod Impact, Unnotched (ISO) | 28.0 kJ/m² | 13.3 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP THERMOTUF MF004AI PP (Asia Pacific) LNP* Thermotuf* MF004AI is a compound based on Polypropylene resin containing Glass Fiber. Added features of this material include: High Impact. |
|||
Izod Impact, Unnotched (ISO) | 28.0 kJ/m² | 13.3 ft-lb/in² | 80x10x4; ISO 180/1U |
Eurostar Starpylen HZ 50E3 PP, Injection Molded PRELIMINARY-Starpylen HZ 50E3 is a High Specific Gravity Polypropylene (density 1.5), Injection Molding Resin (also known as HZ50E3)Information provided by Eurostar. |
|||
Izod Impact, Unnotched (ISO) | 28.0 kJ/m² @Temperature 23.0 °C |
13.3 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP Thermocomp MF0069S PP LNP* Thermocomp* MF0069S is a compound based on Polypropylene resin containing Glass Fiber, Flame Retardant. Added features of this material include: Chemically Coupled, Flame Retardant, Heat Stabi.. |