Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Izod Impact, Unnotched (ISO) = 90.0 kJ/m² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Unnotched (ISO) 11.0 - 90.0 kJ/m²
5.23 - 42.8 ft-lb/in²
Average value: 73.9 kJ/m² Grade Count:16
Overview of materials for Nylon 6, 40% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 40% Glass Fiber Filled". Specific grades with glass content between 35% and 44% are included. E..
Izod Impact, Unnotched (ISO) 10.0 - 90.0 kJ/m²

@Temperature -30.0 - -30.0 °C
4.76 - 42.8 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 63.5 kJ/m² Grade Count:6
Overview of materials for Nylon 6, 40% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 40% Glass Fiber Filled". Specific grades with glass content between 35% and 44% are included. E..
Izod Impact, Unnotched (ISO) 35.0 - 90.0 kJ/m²

@Temperature -30.0 - -30.0 °C
16.7 - 42.8 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 64.9 kJ/m² Grade Count:16
Overview of materials for Nylon 6, Glass Filled, Impact Grade
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Glass Filled, Impact Grade". Each property range of values reported is minimum and maximum valu..
Izod Impact, Unnotched (ISO) 25.0 - 90.0 kJ/m²

@Temperature -30.0 - -30.0 °C
11.9 - 42.8 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 62.5 kJ/m² Grade Count:12
Overview of materials for Nylon 66, Heat Stabilized
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Heat Stabilized". Each property range of values reported is minimum and maximum values of appr..
Izod Impact, Unnotched (ISO) 28.0 - 90.0 kJ/m²

@Temperature -30.0 - -30.0 °C
13.3 - 42.8 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 52.3 kJ/m² Grade Count:6
Overview of materials for Nylon 66, 10% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 10% Glass Fiber Filled". Specific grades with glass content between 5% and 14% are included. ..
Izod Impact, Unnotched (ISO) 30.0 - 90.0 kJ/m²
14.3 - 42.8 ft-lb/in²
Average value: 56.8 kJ/m² Grade Count:12
Overview of materials for Nylon 66, 20% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 20% Glass Fiber Filled". Specific grades with glass content between 15% and 24% are included. ..
Izod Impact, Unnotched (ISO) 7.00 - 90.0 kJ/m²
3.33 - 42.8 ft-lb/in²
Average value: 60.9 kJ/m² Grade Count:31
Overview of materials for Nylon 66, 30% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 30% Glass Fiber Filled". Specific grades with glass content between 25% and 34% are included. ..
Izod Impact, Unnotched (ISO) 50.0 - 90.0 kJ/m²
23.8 - 42.8 ft-lb/in²
Average value: 79.3 kJ/m² Grade Count:7
Overview of materials for Nylon 66, Glass Reinforced, Impact Grade
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass Reinforced, Impact Grade". Each property range of values reported is minimum and maximum..
Izod Impact, Unnotched (ISO) 10.0 - 90.0 kJ/m²
4.76 - 42.8 ft-lb/in²
Average value: 54.4 kJ/m² Grade Count:29
Overview of materials for Nylon 6, 20% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 20% Glass Fiber Filled".Specific grades with glass content between 15% and 24% are included. Ea..
Copyright © lookpolymers.com All Rights Reserved