Polymer Property : Izod Impact, Unnotched (ISO) = 13.3 ft-lb/in² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Unnotched (ISO) 28.0 kJ/m²
13.3 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP KONDUIT ITF2B PA 6/12 (Asia Pacific)
LNP* Konduit* ITF2B is a compound based on Nylon 6/12 resin containing Glass Fiber, Proprietary Thermal Filler. Added features of this material include: Thermally Conductive.
Izod Impact, Unnotched (ISO) 28.0 kJ/m²
13.3 ft-lb/in²
ISO 180
Solvay Specialty Polymers AvaSpire® AV-742 SL30 Polyaryletherketone (PAEK)  (Unverified Data**)
AV-742 SL30 is a wear resistant grade of AvaSpire polyaryletherketone (PAEK) designed to provide low wear rates in both non-lubricated and lubricated environments. In addition to outstanding wear re..
Izod Impact, Unnotched (ISO) 28.0 kJ/m²
13.3 ft-lb/in²
Idemitsu Kosan Xarec® EA 537 SPS, 30% Glass Filled
Crystalline Polymer, Glass Filled, Ignition Resistant, Impact Modified. Used in Electronic and Electrical applications
Izod Impact, Unnotched (ISO) 28.0 kJ/m²

@Temperature 23.0 °C
13.3 ft-lb/in²

@Temperature 73.4 °F
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP Lubricomp IP003 PA6.12
LNP* Lubricomp* IP003 is a Nylon 6/12 base resin containing PTFE and Silicone.This data was supplied by SABIC-IP for the Americas region.
Izod Impact, Unnotched (ISO) 28.0 kJ/m²
13.3 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP LUBRICOMP OCP34E PPS - Linear
LNP LUBRICOMP* OCP34E is a compound based on PPS - Linear resin containing 20% Carbon Fiber, 15% PTFE/Silicone. Added features of this material include: Easy Molding, Electrically Conductive, Wear ..
Izod Impact, Unnotched (ISO) 28.0 kJ/m²
13.3 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP LUBRICOMP OCP34E PPS - Linear (Asia Pacific)
LNP LUBRICOMP* OCP34E is a compound based on PPS - Linear resin containing Silicone, Carbon Fiber, PTFE. Added features of this material include: Easy Molding.
Izod Impact, Unnotched (ISO) 28.0 kJ/m²
13.3 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP LUBRICOMP RX03643H PA 66
LNP* LUBRICOMP* RX03643H is a compound based on Nylon 66 resin containing Proprietary Filler(s). Added feature of this material is: Wear Resistant.
Izod Impact, Unnotched (ISO) 28.0 kJ/m²
13.3 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP LUBRICOMP RX03643H PA 66 (Asia Pacific)
LNP* Lubricomp* RX03643H is a compound based on Nylon 66 resin containing Proprietary Filler(s). Added features of this material include: Internally Lubricated.
Izod Impact, Unnotched (ISO) 28.0 kJ/m²

@Temperature 23.0 °C
13.3 ft-lb/in²

@Temperature 73.4 °F
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP Lubricomp ZFL24 PPO
LNP* Lubricomp* ZFL24 is a compound based on Modified Polyphenylene Oxide (PPO) containing glass fiber and PTFE lubricant. Characteristics of this grade are: Internally Lubricated.This data was su..
Izod Impact, Unnotched (ISO) 28.0 kJ/m²
13.3 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics Valox® 4012 PBT (Europe-Africa-Middle East)
VALOX 4012 is a 10% high strength glass fibre reinforced PBT injection moulding resin with improved mechanical properties. Applications: connectors.
Izod Impact, Unnotched (ISO) 28.0 kJ/m²
13.3 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP STAT-KON DX05474 PC
LNP* STAT-KON* DX05474 is a compound based on Polycarbonate resin containing 10% Carbon Fiber. Added features of this material include: Electrically Conductive, Easy Molding, Flame Retardant, Mold ..
Izod Impact, Unnotched (ISO) 28.0 kJ/m²
13.3 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP STAT-KON DX05474 PC (Asia Pacific)
LNP* Stat-kon* DX05474 is a compound based on Polycarbonate resin containing Flame Retardant, Carbon Fiber. Added features of this material include: Electrically Conductive, Easy Molding, Flame Ret..
Izod Impact, Unnotched (ISO) 27.9 kJ/m²

@Temperature 0.000 °C,
Time 86400 sec
13.3 ft-lb/in²

@Temperature 32.0 °F,
Time 24.0 hour
Shandong Rike Chemical HELIâ„¢ HL-740 Weather-resistance Acrylic Impact Modifier (AIM)
Outline of ACR Impact Modifiers:The PVC impact modifiers developed by our company are acrylic copolymers (ACR) with a core-shell structure, their cores are acrylic ester and shells are methacrylic c..
Izod Impact, Unnotched (ISO) 28.0 kJ/m²
13.3 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP STAT-KON EEF42 PEI
LNP STAT-KON* EEF42 is a compound based on Polyetherimide resin containing 10% Carbon Fiber, 20% Glass Fiber. Added features of this material include: Electrically Conductive.
Izod Impact, Unnotched (ISO) 28.0 kJ/m²

@Temperature 23.0 °C
13.3 ft-lb/in²

@Temperature 73.4 °F
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP Thermocomp EC002E PEI
LNP THERMOCOMP* EC002E is a compound based on Polyetherimide resin containing Carbon Fiber. Added features of this material include: Easy Molding.This data was supplied by SABIC-IP for the Americas..
Izod Impact, Unnotched (ISO) 28.0 kJ/m²
13.3 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP THERMOCOMP SH0430AC_BK1D466 PA12
4.3 specific gravity nylon 12, clean compound system
Izod Impact, Unnotched (ISO) 28.0 kJ/m²
13.3 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP THERMOCOMP TH0750A PUR (Asia Pacific)
LNP THERMOCOMP* TH0750A is a compound based on Polyurethane resin. Added features of this material include: High Specific Gravity.
Izod Impact, Unnotched (ISO) 28.0 kJ/m²

@Temperature 23.0 °C
13.3 ft-lb/in²

@Temperature 73.4 °F
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP Thermocomp WC006 Polyester, TP
LNP* Thermocomp* WC006 is a compound based on Polyester, TP resin containing Carbon Fiber.This data was supplied by SABIC-IP for the Americas region.
Izod Impact, Unnotched (ISO) 28.0 kJ/m²

@Temperature 23.0 °C
13.3 ft-lb/in²

@Temperature 73.4 °F
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP Lubricomp KFI12A Acetal Homopolymer
LNP LUBRICOMP* KFI12A is a compound based on Acetal Homopolymer resin containing Glass Fiber, Silicone. Added features of this material include: Internally Lubricated.This data was supplied by SABI..
Izod Impact, Unnotched (ISO) 28.0 kJ/m²
13.3 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP STAT-KON DE0049P PC
LNP* STAT-KON* DE0049P is a compound based on Polycarbonate resin containing 20% Carbon Fiber. Added features of this material include: Exceptional Processing, Flame Retardant. Electrically Conduct..
Izod Impact, Unnotched (ISO) 28.0 kJ/m²
13.3 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP STAT-KON OE006A PPS - Branched
LNP STAT-KON* OE006A is a compound based on PPS - Branched resin containing 30% Carbon Fiber. Added features of this material include: Electrically Conductive.
Izod Impact, Unnotched (ISO) 28.0 kJ/m²
13.3 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP THERMOCOMP MF003AS PP
LNP* THERMOCOMP* MF003AS is a compound based on Polypropylene containing 15% Glass Fiber. Characteristics of this grade are: Heat Stabilized.
Izod Impact, Unnotched (ISO) 28.0 kJ/m²
13.3 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP THERMOCOMP WC006 PBT
LNP* THERMOCOMP* WC006 is a compound based on PBT resin containing 30% Carbon Fiber. Added feature of this grade is: Electrically Conductive.
Izod Impact, Unnotched (ISO) 28.0 kJ/m²
13.3 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP THERMOTUF MF004AI PP
LNP* Thermotuf* MF004AI is a compound based on Polypropylene resin containing Glass Fiber. Added features of this material include: High Impact.
Izod Impact, Unnotched (ISO) 28.0 kJ/m²
13.3 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP THERMOTUF MF004AI PP (Asia Pacific)
LNP* Thermotuf* MF004AI is a compound based on Polypropylene resin containing Glass Fiber. Added features of this material include: High Impact.
Izod Impact, Unnotched (ISO) 28.0 kJ/m²
13.3 ft-lb/in²
ISO 180/1eU
Solvay TECHNYL® 52G1MX 25 Grey 7035 PA6, DRY
Description: Flame retardant polyamide PA6 reinforced with mineral filler for injection molding, also suitable for thin wall parts.Available in: Asia Pacific, Europe, Latin America and North America..
Izod Impact, Unnotched (ISO) 28.0 kJ/m²

@Temperature -30.0 °C
13.3 ft-lb/in²

@Temperature -22.0 °F
50%RH; ISO 180/1U
DuPont Performance Polymers Zytel® 70G13HS1L NC010 Nylon 66  (Unverified Data**)
13% Glass Reinforced Heat Stabilized Polyamide 66 Zytel 70G13HS1L NC010 is a 13% glass fiber reinforced heat stabilized polyamide 66 resin for injection molding.Information provided by DuPont Perfor..
Izod Impact, Unnotched (ISO) 28.0 kJ/m²
13.3 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP LUBRICOMP DCP32 PC (Asia Pacific)
LNP* Lubricomp* DCP32 is a compound based on Polycarbonate resin containing PTFE, Carbon Fiber, Silicone. Added features of this material include: Electrically Conductive, Internally Lubricated.
Izod Impact, Unnotched (ISO) 28.0 - 55.0 kJ/m²
13.3 - 26.2 ft-lb/in²
Average value: 42.2 kJ/m² Grade Count:9
Overview of materials for Polypropylene with 30% Glass Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 30% Glass Fiber Filler". Specific grades with glass content between 25% and 34% are i..