Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched (ISO) | 11.0 - 90.0 kJ/m² | 5.23 - 42.8 ft-lb/in² | Average value: 73.9 kJ/m² Grade Count:16 |
Overview of materials for Nylon 6, 40% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 40% Glass Fiber Filled". Specific grades with glass content between 35% and 44% are included. E.. |
|||
Izod Impact, Unnotched (ISO) | 10.0 - 90.0 kJ/m² @Temperature -30.0 - -30.0 °C |
4.76 - 42.8 ft-lb/in² @Temperature -22.0 - -22.0 °F |
Average value: 63.5 kJ/m² Grade Count:6 |
Overview of materials for Nylon 6, 40% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 40% Glass Fiber Filled". Specific grades with glass content between 35% and 44% are included. E.. |
|||
Izod Impact, Unnotched (ISO) | 35.0 - 90.0 kJ/m² @Temperature -30.0 - -30.0 °C |
16.7 - 42.8 ft-lb/in² @Temperature -22.0 - -22.0 °F |
Average value: 64.9 kJ/m² Grade Count:16 |
Overview of materials for Nylon 6, Glass Filled, Impact Grade This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Glass Filled, Impact Grade". Each property range of values reported is minimum and maximum valu.. |
|||
Izod Impact, Unnotched (ISO) | 25.0 - 90.0 kJ/m² @Temperature -30.0 - -30.0 °C |
11.9 - 42.8 ft-lb/in² @Temperature -22.0 - -22.0 °F |
Average value: 62.5 kJ/m² Grade Count:12 |
Overview of materials for Nylon 66, Heat Stabilized This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Heat Stabilized". Each property range of values reported is minimum and maximum values of appr.. |
|||
Izod Impact, Unnotched (ISO) | 28.0 - 90.0 kJ/m² @Temperature -30.0 - -30.0 °C |
13.3 - 42.8 ft-lb/in² @Temperature -22.0 - -22.0 °F |
Average value: 52.3 kJ/m² Grade Count:6 |
Overview of materials for Nylon 66, 10% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 10% Glass Fiber Filled". Specific grades with glass content between 5% and 14% are included. .. |
|||
Izod Impact, Unnotched (ISO) | 30.0 - 90.0 kJ/m² | 14.3 - 42.8 ft-lb/in² | Average value: 56.8 kJ/m² Grade Count:12 |
Overview of materials for Nylon 66, 20% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 20% Glass Fiber Filled". Specific grades with glass content between 15% and 24% are included. .. |
|||
Izod Impact, Unnotched (ISO) | 7.00 - 90.0 kJ/m² | 3.33 - 42.8 ft-lb/in² | Average value: 60.9 kJ/m² Grade Count:31 |
Overview of materials for Nylon 66, 30% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 30% Glass Fiber Filled". Specific grades with glass content between 25% and 34% are included. .. |
|||
Izod Impact, Unnotched (ISO) | 50.0 - 90.0 kJ/m² | 23.8 - 42.8 ft-lb/in² | Average value: 79.3 kJ/m² Grade Count:7 |
Overview of materials for Nylon 66, Glass Reinforced, Impact Grade This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass Reinforced, Impact Grade". Each property range of values reported is minimum and maximum.. |
|||
Izod Impact, Unnotched (ISO) | 10.0 - 90.0 kJ/m² | 4.76 - 42.8 ft-lb/in² | Average value: 54.4 kJ/m² Grade Count:29 |
Overview of materials for Nylon 6, 20% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 20% Glass Fiber Filled".Specific grades with glass content between 15% and 24% are included. Ea.. |