Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Impact Test | 1.00 J | 0.738 ft-lb | Multiaxial Impact; ISO 6603 |
SABIC Innovative Plastics LNP KONDUIT ITF2B PA 6/12 (Asia Pacific) LNP* Konduit* ITF2B is a compound based on Nylon 6/12 resin containing Glass Fiber, Proprietary Thermal Filler. Added features of this material include: Thermally Conductive. |
|||
Impact Test | 1.00 J | 0.738 ft-lb | Multiaxial Impact; ISO 6603 |
SABIC Innovative Plastics LNP LUBRICOMP HH0420A PA11 LNP* HH0420A is a compound based on Nylon 11 containing proprietary fillers. Added features of this material are High Specific Gravity. |
|||
Impact Test | 1.00 J | 0.738 ft-lb | Multiaxial Impact; ISO 6603 |
SABIC Innovative Plastics LNP LUBRICOMP KCL34A Acetal Homopolymer (Asia Pacific) LNP* Lubricomp* KCL34A is a compound based on Acetal Homopolymer resin containing PTFE, Carbon Fiber. Added features of this material include: Internally Lubricated, Electrically Conductive. |
|||
Impact Test | 1.00 J | 0.738 ft-lb | Multiaxial Impact; ISO 6603 |
SABIC Innovative Plastics LNP Lubricomp KP004AXZ Acetal Homopoly LNP* Lubricomp* KP004AXZ is a compound based on Acetal Homopolymer resin containing PTFE, Silicone. Added features of this material include: Internally Lubricated.This data was supplied by SABIC-IP.. |
|||
Impact Test | 1.00 J | 0.738 ft-lb | Multiaxial Impact; ISO 6603 |
SABIC Innovative Plastics LNP LUBRICOMP KP004AXZ ACETAL HOMOPOLYMER LNP* LUBRICOMP* KP004AXZ is a compound based on Acetal Homopolymer resin containing 20% PTFE/Silicone. Added feature of this material is: Wear Resistant. |
|||
Impact Test | 1.00 J | 0.738 ft-lb | Multiaxial Impact; ISO 6603 |
SABIC Innovative Plastics LNP Lubricomp KX99792 Acetal Copoly (Asia Pacific) LNP* Lubricomp* KX99792 is a compound based on Acetal Copolymer resin containing Silicone. Added features of this material include: Internally Lubricated.This data was supplied by SABIC-IP for the .. |
|||
Impact Test | 1.00 J | 0.738 ft-lb | Multiaxial Impact; ISO 6603 |
SABIC Innovative Plastics LNP LUBRICOMP LL004C PEEK (Asia Pacific) LNP* Lubricomp* LL004C is a compound based on Polyetheretherketone resin containing PTFE. Added features of this material include: Internally Lubricated, Clean Compounding System. |
|||
Impact Test | 1.00 J | 0.738 ft-lb | Multiaxial Impact; ISO 6603 |
SABIC Innovative Plastics LNP LUBRICOMP QAP22S PA6.10 LNP* LUBRICOMP* QAP22S is a compound based on Nylon 6/10 resin containing 10% PTFE/Silicone, 10% Aramid Fiber. Added features of this material include: Wear Resistant, Heat Stabilized. |
|||
Impact Test | 1.00 J | 0.738 ft-lb | Multiaxial Impact; ISO 6603 |
SABIC Innovative Plastics LNP LUBRICOMP RBL36L PA 66 LNP* LUBRICOMP* RBL36L is a compound based on Nylon 66 containing 30% Glass Bead, 15% PTFE. Added features s of this grade are: Low Extractable, Wear Resistant. |
|||
Impact Test | 1.00 J | 0.738 ft-lb | Multiaxial Impact; ISO 6603 |
SABIC Innovative Plastics LNP LUBRICOMP RFN14 PA 66 LNP* LUBRICOMP* RFN14 is a compound based on Nylon 66 containing 20% Glass Fiber, 5% MOS2. Added features of this grade include: Wear Resistant. |
|||
Impact Test | 1.00 J | 0.738 ft-lb | Multiaxial Impact; ISO 6603 |
SABIC Innovative Plastics LNP LUBRICOMP RL0019 PA 66 LNP LUBRICOMP* RL0019 is a compound based on Nylon 66 resin containing 5% PTFE. Added features of this material include: Flame Retardant, Wear Resistant. |
|||
Impact Test | 1.00 J | 0.738 ft-lb | Multiaxial Impact; ISO 6603 |
SABIC Innovative Plastics LNP LUBRICOMP RX85514 PA 66 LNP LUBRICOMP* RX85514 is a compound based on Nylon 66 resin containing Proprietary Filler(s). Added features of this material include: Internally Lubricated. |
|||
Impact Test | 1.00 J | 0.738 ft-lb | Multiaxial Impact; ISO 6603 |
SABIC Innovative Plastics LNP LUBRICOMP WFL33 PBT LNP* LUBRICOMP* WFL33 is a compound based on PBT containing 15% Glass Fiber, 15% PTFE. Added feature of this grade is: Wear Resistant. |
|||
Impact Test | 1.00 J | 0.738 ft-lb | Multiaxial Impact; ISO 6603 |
SABIC Innovative Plastics LNP STAT-KON KD000 Acetal Copolymer (Europe-Africa-Middle East) LNP STAT-KON KD000* is also know as: LNP STAT-KON K, LNP STAT-KON KXC. It is a compound based on Acetal resin containing Carbon Powder. Added features of this material include: Electrically Conduct.. |
|||
Impact Test | 1.00 J | 0.738 ft-lb | Multiaxial Impact; ISO 6603 |
SABIC Innovative Plastics LNP STAT-KON RFD03 PA 66 LNP* STAT-KON* RFD03 is a compound based on Nylon 66 containing 15% Glass Fiber. Added feature of this material is: Electrically Conductive. |
|||
Impact Test | 1.00 J | 0.738 ft-lb | Multiaxial Impact; ISO 6603 |
SABIC Innovative Plastics LNP STAT-KON WE002 PBT LNP STAT-KON* WE002 is a compound based on PBT resin containing 10% Carbon Fiber. Added features of this material include: Electrically Conductive. |
|||
Impact Test | 1.00 J | 0.738 ft-lb | Multiaxial Impact; ISO 6603 |
SABIC Innovative Plastics LNP Thermocomp 5X06476 FP-V (PVDF) LNP* FP-VM-3830 is a compound based on Polyvinylidine Fluoride (PVDF) containing Mineral.This data was supplied by SABIC-IP for the Americas region. |
|||
Impact Test | 1.00 J | 0.738 ft-lb | Multiaxial Impact; ISO 6603 |
SABIC Innovative Plastics LNP THERMOCOMP CF008 PS LNP* THERMOCOMP* CF008 is a compound based on Polystyrene resin containing 40% Glass Fiber. |
|||
Impact Test | 1.00 J | 0.738 ft-lb | Multiaxial Impact; ISO 6603 |
SABIC Innovative Plastics LNP THERMOCOMP KX97390 Acetal Copolymer LNP THERMOCOMP* KX97390 is a compound based on Acetal Copolymer resin containing Glass Fiber. Added features of this material include: Chemically Coupled. |
|||
Impact Test | 1.00 J | 0.738 ft-lb | Multiaxial Impact; ISO 6603 |
SABIC Innovative Plastics LNP THERMOCOMP KZ002 Acetal LNP* THERMOCOMP* KZ002 is a compound based on Acetal containing 10% Milled Glass. |
|||
Impact Test | 1.00 J | 0.738 ft-lb | Multiaxial Impact; ISO 6603 |
SABIC Innovative Plastics LNP THERMOCOMP MH0500C PP (Asia Pacific) LNP* Thermocomp* MH0500C is a compound based on Polypropylene resin containing High Specific Gravity Filler. Added features of this material include: High Specific Gravity. |
|||
Impact Test | 1.00 J | 0.738 ft-lb | Multiaxial Impact; ISO 6603 |
SABIC Innovative Plastics LNP Thermocomp OK006 PPS - Linear LNP* Thermocomp* OK006 is based on a Linear Polyphenylene Sulfide (PPS) containing Talc.This data was supplied by SABIC-IP for the Americas region. |
|||
Impact Test | 1.00 J | 0.738 ft-lb | Multiaxial Impact; ISO 6603 |
SABIC Innovative Plastics LNP THERMOCOMP RF002ES PA 66 LNP THERMOCOMP* RF002ES is a compound based on Nylon 66 resin containing 10% Glass Fiber. Added features of this material include: Easy Molding, Heat Stabilized. |
|||
Impact Test | 1.00 J | 0.738 ft-lb | Multiaxial Impact; ISO 6603 |
SABIC Innovative Plastics LNP THERMOCOMP WF006L PBT LNP* THERMOCOMP* WF006L is a compound based on PBT resin containing 30% Glass Fiber. Added feature of this material is: Low Extractible. |
|||
Impact Test | 1.00 J | 0.738 ft-lb | Multiaxial Impact; ISO 6603 |
SABIC Innovative Plastics LNP THERMOCOMP WH0270B PBT (Asia Pacific) LNP THERMOCOMP* WH0270B is a compound based on Polybutylene Terephalate resin containing High Specific Gravity Filler. Added features of this material include: High Specific Gravity. |
|||
Impact Test | 1.00 J | 0.738 ft-lb | Multiaxial Impact; ISO 6603 |
SABIC Innovative Plastics LNP THERMOCOMP WX05502 Polyester Elastomer LNP THERMOCOMP* WX05502 is a compound based on Polyester, TP resin containing Flame Retardant, Glass Fiber, Mineral. Added features of this material include: Flame Retardant. |
|||
Impact Test | 1.00 J | 0.738 ft-lb | Multiaxial Impact; ISO 6603 |
SABIC Innovative Plastics LNP LUBRICOMP WBL36L PBT (Asia Pacific) LNP* Lubricomp* WBL36L is a compound based on Polybutylene Terephalate resin containing Glass Bead, PTFE. Added features of this material include: Internally Lubricated, Low Extractible. |
|||
Impact Test | 1.00 J | 0.738 ft-lb | Multiaxial Impact; ISO 6603 |
SABIC Innovative Plastics LNP Stat-kon AD000Z ABS LNP* Stat-Kon AD000Z is a compound based on ABS resin with carbon powder. Grade characteristics: a statically conductive extrusion grade.This data was supplied by SABIC-IP for the Americas region... |
|||
Impact Test | 1.00 J | 0.738 ft-lb | Multiaxial Impact; ISO 6603 |
SABIC Innovative Plastics LNP THERMOCOMP BF004 SAN LNP* THERMOCOMP* BF004 is a compound based on SAN resin containing 20% Glass Fiber. |
|||
Impact Test | 1.00 J | 0.738 ft-lb | Multiaxial Impact; ISO 6603 |
SABIC Innovative Plastics LNP THERMOCOMP RF002 PA 66 LNP THERMOCOMP* RF002 is a compound based on Nylon 66 resin containing 10% Glass Fiber. |