| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.45 g/cc | 0.0524 lb/in³ | ASTM D792 |
| 1.45 g/cc | 0.0524 lb/in³ | ISO 1183 | |
| Moisture Absorption | 0.280 % | 0.280 % | 50% RH, 24 hrs; ASTM D570 |
| 0.330 % | 0.330 % | 23°C / 50% RH; ISO 62 | |
| Linear Mold Shrinkage, Flow | 0.012 - 0.013 cm/cm | 0.012 - 0.013 in/in | mold temp=60°C; SABIC Method |
| 0.015 - 0.016 cm/cm | 0.015 - 0.016 in/in | mold temp=100°C; SABIC Method | |
| 0.015 - 0.035 cm/cm @Time 86400 sec |
0.015 - 0.035 in/in @Time 24.0 hour |
ASTM D955 | |
| 0.015 - 0.035 cm/cm @Time 86400 sec |
0.015 - 0.035 in/in @Time 24.0 hour |
ISO 294 | |
| Linear Mold Shrinkage, Transverse | 0.0090 - 0.010 cm/cm | 0.0090 - 0.010 in/in | mold temp=60°C; SABIC Method |
| 0.011 - 0.012 cm/cm | 0.011 - 0.012 in/in | mold temp=100°C; SABIC Method | |
| 0.015 - 0.035 cm/cm @Time 86400 sec |
0.015 - 0.035 in/in @Time 24.0 hour |
ASTM D955 | |
| 0.015 - 0.035 cm/cm @Time 86400 sec |
0.015 - 0.035 in/in @Time 24.0 hour |
ISO 294 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength at Break | 47.0 MPa | 6820 psi | ISO 527 |
| 54.0 MPa | 7830 psi | ASTM D638 | |
| Tensile Strength, Yield | 53.0 MPa | 7690 psi | ISO 527 |
| 58.0 MPa | 8410 psi | ASTM D638 | |
| Elongation at Break | 7.2 % | 7.2 % | ASTM D638 |
| 20 % | 20 % | ISO 527 | |
| Elongation at Yield | 3.6 % | 3.6 % | ASTM D638 |
| 5.0 % | 5.0 % | ISO 527 | |
| Tensile Modulus | 3.00 GPa | 435 ksi | 1 mm/min; ISO 527 |
| 3.50 GPa | 508 ksi | 50 mm/min; ASTM D638 | |
| Flexural Strength | 82.0 MPa | 11900 psi | ISO 178 |
| 95.0 MPa | 13800 psi | ASTM D790 | |
| Flexural Modulus | 3.20 GPa | 464 ksi | ISO 178 |
| 3.20 GPa | 464 ksi | 2 mm/min; ISO 178 | |
| 3.25 GPa | 471 ksi | ASTM D790 | |
| Izod Impact, Notched | 0.350 J/cm | 0.656 ft-lb/in | ASTM D256 |
| Izod Impact, Unnotched | 8.00 J/cm | 15.0 ft-lb/in | ASTM D4812 |
| Izod Impact, Notched (ISO) | 5.00 kJ/m² | 2.38 ft-lb/in² | 80*10*4; ISO 180/1A |
| Izod Impact, Unnotched (ISO) | 37.0 kJ/m² | 17.6 ft-lb/in² | 80*10*4; ISO 180/1U |
| Dart Drop, Total Energy | 5.00 J | 3.69 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
| Impact Test | 1.00 J | 0.738 ft-lb | Multiaxial Impact; ISO 6603 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear, Parallel to Flow | 101 µm/m-°C @Temperature -40.0 - 40.0 °C |
56.1 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
| 102 µm/m-°C @Temperature -40.0 - 40.0 °C |
56.7 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 | |
| CTE, linear, Transverse to Flow | 101 µm/m-°C @Temperature -40.0 - 40.0 °C |
56.1 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
| 101 µm/m-°C @Temperature -40.0 - 40.0 °C |
56.1 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 | |
| Deflection Temperature at 1.8 MPa (264 psi) | 105 °C | 221 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
| 108 °C @Thickness 3.20 mm |
226 °F @Thickness 0.126 in |
unannealed; ASTM D648 | |
| Flammability, UL94 | HB @Thickness 0.700 mm |
HB @Thickness 0.0276 in |
UL 94 |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Surface Resistance | 100 - 10000 ohm | 100 - 10000 ohm | ASTM D257 |