Category | Polymer , Thermoplastic , Nylon , Nylon 11 |
Manufacturer | SABIC Innovative Plastics (GE Plastics) |
Trade Name | LNP LUBRICOMP |
Port | Ningbo port,China |
Trade Terms | FOB, CFR, CIF |
Payment Terms | L/C, T/T, Western Union |
Download PDF | SABIC Innovative Plastics LNP LUBRICOMP HH0420A PA11.pdf ![]() |
Price | EMAIL US sales@lookpolymers.com |
Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 4.30 g/cc | 4.30 g/cc | ASTM D792 |
Density | 4.28 g/cc | 0.155 lb/in³ | ASTM D792 |
Moisture Absorption | 0.0200 % | 0.0200 % | 50% RH, 24 hrs; ASTM D570 |
0.0300 % | 0.0300 % | 23°C / 50% RH; ISO 62 | |
Linear Mold Shrinkage, Flow | 0.0070 - 0.0090 cm/cm @Time 86400 sec |
0.0070 - 0.0090 in/in @Time 24.0 hour |
ASTM D955 |
Linear Mold Shrinkage, Transverse | 0.0070 - 0.0090 cm/cm @Time 86400 sec |
0.0070 - 0.0090 in/in @Time 24.0 hour |
ASTM D955 |
Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 40.0 MPa | 5800 psi | Type I, 5 mm/min; ASTM D638 |
41.0 MPa | 5950 psi | 5 mm/min; ISO 527 | |
Tensile Strength, Yield | 40.0 MPa | 5800 psi | Type I, 5 mm/min; ASTM D638 |
41.0 MPa | 5950 psi | 5 mm/min; ISO 527 | |
Elongation at Break | 1.3 % | 1.3 % | Type I, 5 mm/min; ASTM D638 |
1.4 % | 1.4 % | 5 mm/min; ISO 527 | |
Elongation at Yield | 1.3 % | 1.3 % | Type I, 5 mm/min; ASTM D638 |
1.4 % | 1.4 % | 5 mm/min; ISO 527 | |
Tensile Modulus | 4.84 GPa | 702 ksi | 1 mm/min; ISO 527 |
5.77 GPa | 837 ksi | 50 mm/min; ASTM D638 | |
Flexural Strength | 61.0 MPa | 8850 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
62.0 MPa | 8990 psi | ISO 178 | |
Flexural Yield Strength | 61.0 MPa | 8850 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
Flexural Modulus | 4.77 GPa | 692 ksi | 2 mm/min; ISO 178 |
4.88 GPa | 708 ksi | 1.3 mm/min, 50 mm span; ASTM D790 | |
Izod Impact, Notched | 0.330 J/cm | 0.618 ft-lb/in | ASTM D256 |
Izod Impact, Unnotched | 2.02 J/cm | 3.78 ft-lb/in | ASTM D4812 |
Izod Impact, Notched (ISO) | 6.00 kJ/m² | 2.86 ft-lb/in² | 80*10*4; ISO 180/1A |
Izod Impact, Unnotched (ISO) | 13.0 kJ/m² | 6.19 ft-lb/in² | 80*10*4; ISO 180/1U |
Dart Drop, Total Energy | 9.00 J @Temperature 23.0 °C |
6.64 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
Impact Test | 1.00 J | 0.738 ft-lb | Multiaxial Impact; ISO 6603 |
Coefficient of Friction, Dynamic | 0.44 | 0.44 | ASTM D3702 Modified |
Coefficient of Friction, Static | 0.38 | 0.38 | ASTM D3702 Modified |
K (wear) Factor | 96.7 x 10-8 mm³/N-M | 48.0 x 10-10 in³-min/ft-lb-hr | Washer; ASTM D3702 Modified |
Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Parallel to Flow | 66.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
36.7 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
CTE, linear, Transverse to Flow | 65.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
36.1 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
Deflection Temperature at 0.46 MPa (66 psi) | 167 °C | 333 °F | Flatw 80*10*4 sp=64mm; ISO 75/Bf |
162 °C @Thickness 3.20 mm |
324 °F @Thickness 0.126 in |
unannealed; ASTM D648 | |
Deflection Temperature at 1.8 MPa (264 psi) | 95.0 °C | 203 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
84.0 °C @Thickness 3.20 mm |
183 °F @Thickness 0.126 in |
unannealed; ASTM D648 |