Vyncolit 3520 CG Novolac Phenolic

Category Polymer , Thermoset , Filled/Reinforced Thermoset , Phenolic , Phenolic, Novolac, Impact Grade, Filled
Manufacturer Vyncolit N.V., Sumitomo Bakelite
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Vyncolit 3520 CG Novolac Phenolic.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Graphite filled phenolic molding compound with excellent dimensional stability. Self-lubricating and has a low coefficient of friction. Not suitable for electrical applications.USES: Gas meter parts, water pump seals and self-lubricating bearings.Information provided by Vyncolit, a Sumitomo Bak Group
Physical Properties Metric English Comments
Bulk Density 0.750 - 0.900 g/cc
0.0271 - 0.0325 lb/in³
Powder Density; ISO 60
Density 1.63 g/cc
0.0589 lb/in³
Relative Density; ISO 1183
Linear Mold Shrinkage 0.0050 - 0.0060 cm/cm
0.0050 - 0.0060 in/in
Injection Molding; ISO 2577
Mechanical Properties Metric English Comments
Tensile Strength at Break 30.0 - 50.0 MPa
4350 - 7250 psi
ISO 527
Elongation at Break 0.20 - 0.30 %
0.20 - 0.30 %
Tensile; ISO 527
0.60 - 0.70 %
0.60 - 0.70 %
Flexure; ISO 178
Tensile Modulus 13.0 - 15.0 GPa
1890 - 2180 ksi
ISO 527
Flexural Strength 65.0 - 85.0 MPa
9430 - 12300 psi
At Rupture; ISO 178
Flexural Modulus 10.0 - 12.0 GPa
1450 - 1740 ksi
ISO 178
Compressive Strength 110 - 130 MPa
16000 - 18900 psi
ISO 604
Charpy Impact Unnotched 0.250 - 0.350 J/cm²
1.19 - 1.67 ft-lb/in²
ISO 179
Charpy Impact, Notched 0.150 - 0.250 J/cm²
0.714 - 1.19 ft-lb/in²
ISO 179
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 20.0 - 30.0 µm/m-°C

@Temperature 20.0 °C
11.1 - 16.7 µin/in-°F

@Temperature 68.0 °F
TMA
CTE, linear, Transverse to Flow 20.0 - 30.0 µm/m-°C

@Temperature 20.0 °C
11.1 - 16.7 µin/in-°F

@Temperature 68.0 °F
TMA
Deflection Temperature at 1.8 MPa (264 psi) 150 - 170 °C
302 - 338 °F
ISO 75 Af
Deflection Temperature at 8.0 MPa 130 - 150 °C
266 - 302 °F
ISO 75 C
Flammability, UL94 V-1

@Thickness 1.60 mm
V-1

@Thickness 0.0630 in
V-0

@Thickness 4.00 mm
V-0

@Thickness 0.157 in
Shrinkage 0.050 - 0.15 %
0.050 - 0.15 %
Post Shrinkage; ISO 2577
Descriptive Properties Value Comments
Color Black
ISO type PF 2 C4
Main Filler Graphite
Molding Method Compression, transfer, injection