Thermal Properties Metric English Comments
CTE, linear, Transverse to Flow 20.0 - 30.0 µm/m-°C

@Temperature 20.0 °C
11.1 - 16.7 µin/in-°F

@Temperature 68.0 °F
TMA
Vyncolit 3640 CG Novolac Phenolic
Graphite filled phenolic molding compound with excellent dimensional stability. Self-lubricating and has a low coefficient of friction. Not suitable for electrical applications.USES: Gas meter par..
CTE, linear, Transverse to Flow 20.0 - 30.0 µm/m-°C

@Temperature 20.0 °C
11.1 - 16.7 µin/in-°F

@Temperature 68.0 °F
TMA
Vyncolit X658 Novolac Phenolic
Glass fiber and mineral filled phenolic molding compound with excellent mechanical and thermal properties and a very good dimensional stability.USES: Complex precision parts.Information provided by ..
CTE, linear, Transverse to Flow 20.0 - 30.0 µm/m-°C

@Temperature 20.0 °C
11.1 - 16.7 µin/in-°F

@Temperature 68.0 °F
TMA
Vyncolit 3520 CG Novolac Phenolic
Graphite filled phenolic molding compound with excellent dimensional stability. Self-lubricating and has a low coefficient of friction. Not suitable for electrical applications.USES: Gas meter par..