Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Transverse to Flow | 20.0 µm/m-°C | 11.1 µin/in-°F | XY Direction |
Premix Premi-Glas® 1281-47 VE SMC Description: Premi-Glas® 1281-47 VE is a sheet molding compound.Market: StructuralInformation provided by Premix. |
|||
CTE, linear, Transverse to Flow | 20.0 µm/m-°C | 11.1 µin/in-°F | XY Direction |
Premix Premi-Glas® 1286 Glass Reinforced SMC Description: Premi-Glas® 1286 is a glass reinforced thermoset sheet molding compound designed for automotive under the hood applications. Key features and benefits: Designed for compression molding.. |
|||
CTE, linear, Transverse to Flow | 20.0 - 40.0 µm/m-°C | 11.1 - 22.2 µin/in-°F | Average value: 33.3 µm/m-°C Grade Count:3 |
Overview of materials for Silicone, Molded, Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Silicone, Molded, Glass Fiber Filled". Each property range of values reported is minimum and maximum val.. |
|||
CTE, linear, Transverse to Flow | 20.0 - 139 µm/m-°C | 11.1 - 77.2 µin/in-°F | Average value: 59.8 µm/m-°C Grade Count:4 |
Overview of materials for Silicone Rubber This property data is a summary of similar materials in the MatWeb database for the category "Silicone Rubber". Each property range of values reported is minimum and maximum values of appropriate Ma.. |
|||
CTE, linear, Transverse to Flow | 20.0 - 45.0 µm/m-°C | 11.1 - 25.0 µin/in-°F | Average value: 28.7 µm/m-°C Grade Count:10 |
Overview of materials for Phenolic, Novolac, Mineral/Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Mineral/Glass Filled". Each property range of values reported is minimum and maximum .. |
|||
CTE, linear, Transverse to Flow | 20.0 - 40.0 µm/m-°C | 11.1 - 22.2 µin/in-°F | Average value: 26.5 µm/m-°C Grade Count:3 |
Overview of materials for Phenolic, Carbon Fiber Composite This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Carbon Fiber Composite". Each property range of values reported is minimum and maximum values .. |
|||
CTE, linear, Transverse to Flow | 20.0 - 70.0 µm/m-°C | 11.1 - 38.9 µin/in-°F | Average value: 52.9 µm/m-°C Grade Count:11 |
Overview of materials for Nylon 6-3 This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6-3". Each property range of values reported is minimum and maximum values of appropriate MatWeb e.. |
|||
CTE, linear, Transverse to Flow | 20.0 µm/m-°C @Temperature 20.0 °C |
11.1 µin/in-°F @Temperature 68.0 °F |
y-axis |
Industrial Laminates/Norplex NP631 Paper Base Laminate Description: Hot punching grade with excellent electrical properties and low moisture absorption.Thickness Tested: 0.062", 0.125" and 0.500" |
|||
CTE, linear, Transverse to Flow | 20.0 µm/m-°C @Thickness 1.57 mm, Temperature 20.0 °C |
11.1 µin/in-°F @Thickness 0.0620 in, Temperature 68.0 °F |
x-axis; IPC-TM 650-2.4.24 |
Industrial Laminates/Norplex NP691 Paper Base Laminate Description: Flame resistant, room temperature punching grade. NP691 is very similar to NP612 in electrical properties and mechanical strength, with improved moisture resistance.Thickness Tested: 0... |
|||
CTE, linear, Transverse to Flow | 20.0 µm/m-°C @Temperature -40.0 - 150 °C |
11.1 µin/in-°F @Temperature -40.0 - 302 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP THERMOCOMP LC00APXQ PEEK LNP* THERMOCOMP* LC00APXQ is a compound based on Polyetheretherketone resin containing 50% Carbon Fiber. Added features of this material include: Exceptional Processing, Electrically Conductive. |
|||
CTE, linear, Transverse to Flow | 20.0 µm/m-°C | 11.1 µin/in-°F | ASTM E831 |
Sumitomo Bakelite North America CF 9040A Carbon Fiber Reinforced Phenolic CF 9040A is a high strength carbon fiber phenolic molding compoundInformation provided by Sumitomo Bak North America, Inc. |
|||
CTE, linear, Transverse to Flow | 20.0 - 30.0 µm/m-°C @Temperature 20.0 °C |
11.1 - 16.7 µin/in-°F @Temperature 68.0 °F |
TMA |
Vyncolit 3640 CG Novolac Phenolic Graphite filled phenolic molding compound with excellent dimensional stability. Self-lubricating and has a low coefficient of friction. Not suitable for electrical applications.USES: Gas meter par.. |
|||
CTE, linear, Transverse to Flow | 20.0 µm/m-°C @Temperature 20.0 °C |
11.1 µin/in-°F @Temperature 68.0 °F |
TMA |
Vyncolit X655 Novolac Phenolic Glass fiber and mineral filled phenolic molding compound with excellent dimensional stability and a very low coefficient of thermal expansion. UL listed.USES: Automotive disc brake pistons and gask.. |
|||
CTE, linear, Transverse to Flow | 20.0 - 30.0 µm/m-°C @Temperature 20.0 °C |
11.1 - 16.7 µin/in-°F @Temperature 68.0 °F |
TMA |
Vyncolit X658 Novolac Phenolic Glass fiber and mineral filled phenolic molding compound with excellent mechanical and thermal properties and a very good dimensional stability.USES: Complex precision parts.Information provided by .. |
|||
CTE, linear, Transverse to Flow | 20.0 µm/m-°C @Temperature 50.0 - 150 °C |
11.1 µin/in-°F @Temperature 122 - 302 °F |
z direction; IPC TM-650 2.4.24 |
Arlon CLTE-AT Commercial Ceramic PTFE Microwave material for improved thermal management, Excellent dimensional stability with high degree of phase stability vs. temperature.CLTE-AT is a micro-dispersed ceramic PTFE composite utilizing .. |
|||
CTE, linear, Transverse to Flow | 20.0 µm/m-°C @Temperature 50.0 - 150 °C |
11.1 µin/in-°F @Temperature 122 - 302 °F |
z direction; IPC TM-650 2.4.24 |
Arlon CLTE-XT High Precision Ceramic PTFE Microwave material for improved thermal management, Excellent dimensional stability with high degree of phase stability vs. temperature.CLTE-XT is a micro-dispersed ceramic PTFE composite utilizing .. |
|||
CTE, linear, Transverse to Flow | 20.0 µm/m-°C | 11.1 µin/in-°F | ASTM E 831 |
Arlon Thermabond® 48781A008 0.008" (0.203 mm) Uncured Silicone Rubber with Fiberglass Substrate Description: Generation II Thermabond® NP electrically insulating electronic adhesive. Bonds without primer.Design/Construction: Liner 1: PolyethyleneSide 1: Uncured Silicone RubberSubstrate: Style.. |
|||
CTE, linear, Transverse to Flow | 20.0 µm/m-°C @Temperature 50.0 - 150 °C |
11.1 µin/in-°F @Temperature 122 - 302 °F |
z direction; IPC TM-650 2.4.24 |
Arlon AD1000 PTFE/Woven Fiberglass/Ceramic Filled Laminate for Microwave Printed Circuit Boards Only Woven Glass Reinforced PTFE/Ceramic with Dk of 10.2 or greaterHigh Copper Peel Strength allows for thinner etched line widthsLowest insertion loss availableLarger Panel sizes availableLow moist.. |
|||
CTE, linear, Transverse to Flow | 20.0 µm/m-°C @Temperature 23.0 °C |
11.1 µin/in-°F @Temperature 73.4 °F |
|
Momentive Performance Materials HOPG Graphite Monochromator Advanced Ceramics' graphite monochromators are highly oriented forms of high purity pyrolytic graphite which diffract x-rays and neutrons with greater efficiency than any other material. In x-r.. |
|||
CTE, linear, Transverse to Flow | 20.0 - 30.0 µm/m-°C @Temperature 20.0 °C |
11.1 - 16.7 µin/in-°F @Temperature 68.0 °F |
TMA |
Vyncolit 3520 CG Novolac Phenolic Graphite filled phenolic molding compound with excellent dimensional stability. Self-lubricating and has a low coefficient of friction. Not suitable for electrical applications.USES: Gas meter par.. |