Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 0.150 - 0.250 J/cm² @Temperature 23.0 °C |
0.714 - 1.19 ft-lb/in² @Temperature 73.4 °F |
Compression; ISO 179/ 1eA |
Raschig Group AMPLA® 7250 melamine-modified polyester Cellulose reinforced melamine-modified Polyester molding compound. Very good electrical values, excellent heat resistance, excellent surface quality, low post shrinkage. This product meets the allow.. |
|||
Charpy Impact, Notched | 0.150 - 0.250 J/cm² | 0.714 - 1.19 ft-lb/in² | ISO 179/1eA |
Raschig Group EN 5004 Epoxy Molding Compound Mica reinforced molding compound. Low mold shrinkage and post-shrinkage, very good electrical values, outstanding heat resistance, very goo pourablity. This product meets the allowed upper limits fo.. |
|||
Charpy Impact, Notched | 0.150 - 0.450 J/cm² | 0.714 - 2.14 ft-lb/in² | Average value: 0.211 J/cm² Grade Count:32 |
Overview of materials for Phenolic, Novolac, Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Mineral Filled". Each property range of values reported is minimum and maximum values.. |
|||
Charpy Impact, Notched | 0.150 J/cm² @Temperature 23.0 °C |
0.714 ft-lb/in² @Temperature 73.4 °F |
ISO 179-1/2 eA |
Hexion Bakelite™ PF 31 Phenolic Formaldehyde Resin, UL Listed
(discontinued **) Phenolic molding compound, mainly organically filled, standard molding compound for normal stress, UL listed molding compound 1.5 mm/V-1 (All), 3 mm/V-0 (All), standardized molding compound.Applicat.. |
|||
Charpy Impact, Notched | 0.150 J/cm² @Temperature 23.0 °C |
0.714 ft-lb/in² @Temperature 73.4 °F |
ISO 179-1/2 eA |
Hexion Bakelite™ PF 85 Phenolic Formaldehyde Resin, UL Listed
(discontinued **) Phenolic molding compound, organically filled, reinforced with cotton fibers, average notched impact strength, UL listed molding compound 1.5 mm/HB (BK, BN).Application areas: Switch covers, rolls, .. |
|||
Charpy Impact, Notched | 0.150 J/cm² @Temperature 23.0 °C |
0.714 ft-lb/in² @Temperature 73.4 °F |
ISO 179-1/2 eA |
Hexion Bakelite™ PF 2137 Phenolic Formaldehyde Resin, High Surface Quality, Dishwasher Proof
(discontinued ** Phenolic molding compound, inorganically/organically filled, glass fiber reinforced, increased heat resistance, minimal distortion, dish washer proof.Application areas: Iron heat shields, fittings f.. |
|||
Charpy Impact, Notched | 0.150 J/cm² @Temperature 23.0 °C |
0.714 ft-lb/in² @Temperature 73.4 °F |
ISO 179-1/2 eA |
Hexion Bakelite™ 460124 Phenolic Formaldehyde Resin
(discontinued **) Phenolic molding compound, mainly organically filled, standard molding compound for normal stress.Application areas: Cookware fittings, electric devices.Information provided by Bak AGBak AG became a.. |
|||
Charpy Impact, Notched | 0.150 J/cm² @Temperature 23.0 °C |
0.714 ft-lb/in² @Temperature 73.4 °F |
ISO 179-1/2 eA |
Hexion Bakelite™ X22 Phenolic Formaldehyde Resin, UL Listed
(discontinued **) Phenolic molding compound, mainly organically filled, UL listed molding compound 3.0 mm/V-0 (BN, BK).Application areas: Pot handles, operating controls, electrical isolators, housing parts.Informati.. |
|||
Charpy Impact, Notched | 0.150 J/cm² - NB @Temperature -40.0 - -20.0 °C |
0.714 ft-lb/in² - NB @Temperature -40.0 - -4.00 °F |
Average value: 0.311 J/cm² Grade Count:15 |
Overview of materials for Nylon 66, Unreinforced, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Unreinforced, Flame Retardant". Each property range of values reported is minimum and maximum .. |
|||
Charpy Impact, Notched | 0.150 - 0.800 J/cm² @Temperature -40.0 - 30.0 °C |
0.714 - 3.81 ft-lb/in² @Temperature -40.0 - 86.0 °F |
Average value: 0.357 J/cm² Grade Count:32 |
Overview of materials for Nylon 66, 40% Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 40% Mineral Filled". Specific grades with primary filler content between 35% and 44% are inclu.. |
|||
Charpy Impact, Notched | 0.150 J/cm² @Temperature 23.0 °C |
0.714 ft-lb/in² @Temperature 73.4 °F |
ISO 179-1/1eA |
FKuR Kunststoff Bio-Flex® S 9533 Compostable PLA Blend The BIO-FLEX® trade name indicates blends of co-polyester and PLA* with, depending on the particular grade, a very high content of natural resource material. BIO-FLEX® does not contain any sta.. |
|||
Charpy Impact, Notched | 0.150 J/cm² @Temperature -23.0 °C |
0.714 ft-lb/in² @Temperature -9.40 °F |
DIN 53453 |
Global PP-1140-T Polypropylene Homopolymer Description-transparency, high stiffness, high heat resistantApplications-disposable drinkware, thin-walled partsInformation provided by Global Polymers Corporation. |
|||
Charpy Impact, Notched | 0.150 J/cm² @Temperature 23.0 °C |
0.714 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
Grupo Repol Dinalon® A1X25 V0 PA66, V0 red phosphorus and halogen free Mechanical properties for Dry As Molded samplesInformation provided by Grupo Repol |
|||
Charpy Impact, Notched | 0.150 J/cm² | 0.714 ft-lb/in² | |
LATI Latigray 62-01 CX/75 PA 6 Radiopaque compound based on Polyamide 6 (PA6). Special mineral filler. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria T.. |
|||
Charpy Impact, Notched | 0.150 J/cm² | 0.714 ft-lb/in² | |
LATI Latilub 80-10T Y/15 PPS, 15% Aramid Fiber Reinforced, PTFE Filled Self-lubricating product based on Polyphenylene Sulfide (PPS). PTFE. Aramid fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati.. |
|||
Charpy Impact, Notched | 0.150 J/cm² | 0.714 ft-lb/in² | ASTM D256 |
Plenco 4002 Phenolic, Granular, Injection Molded PLENCO 04002 is a heat resistant, mineral filled phenolic molding compound offering excellent mechanical strength and dimensional stability at elevated temperatures. UL recognized under component fi.. |
|||
Charpy Impact, Notched | 0.150 J/cm² @Temperature -30.0 °C |
0.714 ft-lb/in² @Temperature -22.0 °F |
|
BASF Novolen® 1100 RC Polypropylene, Injection Molding Grade Injection molded partsData was collected by ISO methods and provided by BASF. |
|||
Charpy Impact, Notched | 0.150 J/cm² @Temperature -30.0 °C |
0.714 ft-lb/in² @Temperature -22.0 °F |
|
BASF Novolen® 1101 R Polypropylene Data was collected by ISO methods and provided by BASF. |
|||
Charpy Impact, Notched | 0.150 J/cm² @Temperature -30.0 °C |
0.714 ft-lb/in² @Temperature -22.0 °F |
|
BASF Novolen® 3240 NC Polypropylene Grade containing nucleating agent for transparent injection molded parts.Data was collected by ISO methods and provided by BASF. |
|||
Charpy Impact, Notched | 0.150 - 13.0 J/cm² | 0.714 - 61.9 ft-lb/in² | Average value: 1.44 J/cm² Grade Count:56 |
Overview of materials for Nylon 6, Heat Stabilized This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Heat Stabilized". Each property range of values reported is minimum and maximum values of appro.. |
|||
Charpy Impact, Notched | 0.150 - 2.00 J/cm² @Temperature -30.0 - -20.0 °C |
0.714 - 9.52 ft-lb/in² @Temperature -22.0 - -4.00 °F |
Average value: 0.863 J/cm² Grade Count:43 |
Overview of materials for Nylon 6, Heat Stabilized This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Heat Stabilized". Each property range of values reported is minimum and maximum values of appro.. |
|||
Charpy Impact, Notched | 0.150 - 0.500 J/cm² | 0.714 - 2.38 ft-lb/in² | Average value: 0.278 J/cm² Grade Count:9 |
Overview of materials for Acetal Copolymer, Glass Bead Filled This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Glass Bead Filled". Each property range of values reported is minimum and maximum valu.. |
|||
Charpy Impact, Notched | 0.150 J/cm² @Temperature -30.0 °C |
0.714 ft-lb/in² @Temperature -22.0 °F |
|
BASF Novolen® 1101 N Polypropylene Data was collected by ISO methods and provided by BASF. |
|||
Charpy Impact, Notched | 0.150 J/cm² @Temperature -30.0 °C |
0.714 ft-lb/in² @Temperature -22.0 °F |
|
BASF Novolen® 1148 UC Polypropylene Nucleated grade with antistatic agent for injection molded parts.Data was collected by ISO methods and provided by BASF. |
|||
Charpy Impact, Notched | 0.150 - 9.00 J/cm² | 0.714 - 42.8 ft-lb/in² | Average value: 0.657 J/cm² Grade Count:53 |
Overview of materials for Polypropylene, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Flame Retardant". Each property range of values reported is minimum and maximum values of.. |
|||
Charpy Impact, Notched | 0.150 - 5.40 J/cm² | 0.714 - 25.7 ft-lb/in² | Average value: 2.85 J/cm² Grade Count:12 |
Overview of materials for Epoxy Molding Compound This property data is a summary of similar materials in the MatWeb database for the category "Epoxy Molding Compound". Each property range of values reported is minimum and maximum values of appropr.. |
|||
Charpy Impact, Notched | 0.150 - 0.500 J/cm² | 0.714 - 2.38 ft-lb/in² | Average value: 0.317 J/cm² Grade Count:3 |
Overview of materials for Polybutylene Terephthalate (PBT), PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), PTFE Filled". Each property range of values reported is minimum and ma.. |
|||
Charpy Impact, Notched | 0.150 J/cm² @Temperature 23.0 °C |
0.714 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
Styrolution Luran® 348 Q Transparent SAN Description: Highly transparent grade with light natural color.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS |
|||
Charpy Impact, Notched | 0.150 J/cm² | 0.714 ft-lb/in² | ISO 179-1/1eA |
Quadrant EPP Duratron® PI D7015G PI, bearing grade (ISO Data) This grade contains 15 % graphite, added to provide long wear and low friction Good performance at elevated temperature (>425 °C) Good chemical resistance Easily machined from a broad range of shap.. |