Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.63 g/cc | 0.0589 lb/in³ | ASTM D792, ISO 1183 |
Nilit Nilitop BT G6 FR C3 is a 30% Glass Fiber Reinforced, Flame Retardant PBT Description: Nilitop BT G6 FR C3 is a 30% glass fiber reinforced, flame retardant PBT with halogens. The flame retardant does not contain PBB and PBDE, so it is compliant with the WEEE directive. It.. |
|||
Density | 1.63 g/cc | 0.0589 lb/in³ | ASTM D792 |
PolyOne Edgetek® ES-20GF-15GM/000 Polyethersulfone - 20% Glass Fiber - 15% Milled Glass
(discontinued **) Data provided by PolyOne. |
|||
Density | 1.63 g/cc | 0.0589 lb/in³ | DIN 53479; ASTM D792 |
Kolon SPESIN® KP212G30VO G/F Reinforced & Retardant PBT Resin SPESIN® is a thermoplastic PBT resin with excellent thermal, mechanical and electrical properties. SPESIN® is widely used in industrial parts and especially in electrical-electronic parts.High.. |
|||
Density | 1.63 g/cc | 0.0589 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP Lubricomp KFL34 Acetal Copolymer (Europe-Africa-Middle East) LNP* Lubricomp* KFL34 is a compound based on Acetal Copolymer resin containing Glass Fiber, PTFE.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Density | 1.63 g/cc | 0.0589 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP Lubricomp LFL36 PEEK LNP* Lubricomp* LFL36 is a compound based on PEEK containing Glass Fiber and PTFE.This data was supplied by SABIC-IP for the Americas region. |
|||
Density | 1.63 g/cc | 0.0589 lb/in³ | ISO 1183 |
Solvay Specialty Polymers Lavanta® 5115 WH 251 Polyester, High Performance (HPP), 15% Glass Fiber Lavanta® 5115 WH 251 is a high-performance polyester (HPP) is a 15% glass reinforced, injection molding grade developed specifically for HB LED packaging applications that utilize surface mount t.. |
|||
Density | 1.63 g/cc | 0.0589 lb/in³ | ASTM D792 |
Techmer ES HiFill FR® PA6 GF33 FR HS L GY300 33% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 33% Filler by WeightAdditive: Heat Stabilizer, UV Stabilizer and LubricantFeatures: Flame Retardant, Heat St.. |
|||
Density | 1.63 g/cc | 0.0589 lb/in³ | ASTM D792 |
Techmer ES Luriblend® POM CO GM30 TL5 30% Glass Milled Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Milled Glass Fiber, 30% Filler by WeightAdditive: PTFE Lubricant(5%)Features: Lubricated and CopolymerInformation provided by TP Compos.. |
|||
Density | 1.63 g/cc | 0.0589 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP Verton UV00A PPA LNP VERTON* UV00A is a compound based on Polyphthalamide resin containing Long Glass.This data was supplied by SABIC-IP for the Americas region. |
|||
Density | 1.63 g/cc | 0.0589 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP VERTON UX03320 PPA LNP* VERTON* UX03320 is a compound based on Polyphthalamide resin containing proprietary fillers. Added feature of this grade is: Structural. |
|||
Density | 1.63 g/cc | 0.0589 lb/in³ | D792 |
Zhejiang Juner 301-G25 25% Glass Fibre Reinforced and Flammable Resistant Applications: Electrons and Electricity: TV Components, Plugs of Computers, Exhaust Fans of Computers, Plugs, Sockets, Shells of Electronics, Framework of Level Output Transformers, Pipe Pedestals, .. |
|||
Density | 1.63 g/cc | 0.0589 lb/in³ | ASTM D792 |
Unitika UNILATE® 1 PC PET Standard gradeUNILATE® products are plate materials prepared by using a polyethylene terephthalate (PET resin) as the main component, blending it with glass staple fiber, inorganic filler, and othe.. |
|||
Density | 1.63 g/cc | 0.0589 lb/in³ | ISO 1183 |
Polyplastics Duranex® 7400W Polybutylene Terephthalate (PBT), Super low warpage, GF filled DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers .. |
|||
Density | 1.63 g/cc | 0.0589 lb/in³ | dry; ISO 1183 |
DSM Stanyl® TW271F8 (PA46+PTFE)-GF40 40% Glass Reinforced, Heat Stabilized, Wear and Friction Modified |
|||
Density | 1.63 g/cc | 0.0589 lb/in³ | ISO 1183 |
Eurotec® Tecomid® NT40 GR50 NL HS PPA, 50% glass fiber reinforced, heat stabilized, natural Information provided by Eurotec® |
|||
Density | 1.63 g/cc | 0.0589 lb/in³ | ISO 1183 |
DSM Arnite® AV2 370 XT PET-GF35 35% Glass Reinforced, Applications with extremely narrow tolerances |
|||
Density | 1.63 g/cc | 0.0589 lb/in³ | ISO 1183 |
DSM Arnite® AV2 372 PET-35% Glass Reinforced (European and Asian Grade) Arnite resins are engineered to provide specific performance in applications where DSM technology can offer value.Arnite Molding resins: Standard Unfilled and Reinforced materialsHigh modulus Flame .. |
|||
Density | 1.63 g/cc | 0.0589 lb/in³ | ISO 1183 |
Eurotec® Tecopet® PT74 GR20 BK002 XA20 PET, 20% glass fiber reinforced, flame retardant - halogen (RoHS compliant), heat stabilized, black Information provided by Eurotec® |
|||
Density | 1.63 g/cc | 0.0589 lb/in³ | ISO 1183 |
Azoty Tarnow™ TARNOFORM 500 GF6 POM 30% glass fiber reinforced, high flow injection molding grade, suitable for applications where high strength and stiffness is required, combined with higher flowability during molding.Information pr.. |
|||
Density | 1.63 - 1.75 g/cc | 0.0589 - 0.0632 lb/in³ | Molding; IS 867-1963 |
Amity Thermosets ATS 751 Phenolic Molding Inorganic and glass fiber Filler, Compression Molded Characteristics:High impact strength Dimensional stabilityHigh mechanical strengthHeat stability ( 200°C )Good media resistance ( eg. Oil, water ) Low shrinkageGood electrical resistanceColor-brown.. |
|||
Density | 1.63 g/cc | 0.0589 lb/in³ | |
A. Schulman ComAlloy Voloy® 461 Glass Reinforced, PBT Alloy, Flame Retardant, UL Data provided by the manufacturer, ComAlloy International Company.30% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Density | 1.63 g/cc | 0.0589 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP VERTON UX03320 PPA (Asia Pacific) VERTON* UX03320 is a compound based on Polyphthalamide resin containing Long Glass. |
|||
Density | 1.63 g/cc | 0.0589 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP VERTON UX06451 PPA (Europe-Africa-Middle East) LNP* Verton* UX06451 is a compound based on Polyphthalamide resin containing Long Glass Fiber. |
|||
Density | 1.63 g/cc | 0.0589 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP VERTON UX06451 PPA (Europe-Africa-Middle East) LNP* Verton* UX06451 is a compound based on Polyphthalamide resin containing Long Glass Fiber. |
|||
Density | 1.63 g/cc | 0.0589 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP VERTON UX06451 BK8-312 PPA (Asia Pacific) LNP* Verton* UX06451 BK8-312 is a compound based on Polyphthalamide resin containing Long Glass Fiber. |