Thermal Properties Metric English Comments
CTE, linear, Transverse to Flow 20.0 µm/m-°C
11.1 µin/in-°F
XY Direction
Premix Premi-Glas® 1281-47 VE SMC
Description: Premi-Glas® 1281-47 VE is a sheet molding compound.Market: StructuralInformation provided by Premix.
CTE, linear, Transverse to Flow 20.0 µm/m-°C
11.1 µin/in-°F
XY Direction
Premix Premi-Glas® 1286 Glass Reinforced SMC
Description: Premi-Glas® 1286 is a glass reinforced thermoset sheet molding compound designed for automotive under the hood applications. Key features and benefits: Designed for compression molding..
CTE, linear, Transverse to Flow 20.0 - 40.0 µm/m-°C
11.1 - 22.2 µin/in-°F
Average value: 33.3 µm/m-°C Grade Count:3
Overview of materials for Silicone, Molded, Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Silicone, Molded, Glass Fiber Filled". Each property range of values reported is minimum and maximum val..
CTE, linear, Transverse to Flow 20.0 - 139 µm/m-°C
11.1 - 77.2 µin/in-°F
Average value: 59.8 µm/m-°C Grade Count:4
Overview of materials for Silicone Rubber
This property data is a summary of similar materials in the MatWeb database for the category "Silicone Rubber". Each property range of values reported is minimum and maximum values of appropriate Ma..
CTE, linear, Transverse to Flow 20.0 - 45.0 µm/m-°C
11.1 - 25.0 µin/in-°F
Average value: 28.7 µm/m-°C Grade Count:10
Overview of materials for Phenolic, Novolac, Mineral/Glass Filled
This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Mineral/Glass Filled". Each property range of values reported is minimum and maximum ..
CTE, linear, Transverse to Flow 20.0 - 40.0 µm/m-°C
11.1 - 22.2 µin/in-°F
Average value: 26.5 µm/m-°C Grade Count:3
Overview of materials for Phenolic, Carbon Fiber Composite
This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Carbon Fiber Composite". Each property range of values reported is minimum and maximum values ..
CTE, linear, Transverse to Flow 20.0 - 70.0 µm/m-°C
11.1 - 38.9 µin/in-°F
Average value: 52.9 µm/m-°C Grade Count:11
Overview of materials for Nylon 6-3
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6-3". Each property range of values reported is minimum and maximum values of appropriate MatWeb e..
CTE, linear, Transverse to Flow 20.0 µm/m-°C

@Temperature 20.0 °C
11.1 µin/in-°F

@Temperature 68.0 °F
y-axis
Industrial Laminates/Norplex NP631 Paper Base Laminate
Description: Hot punching grade with excellent electrical properties and low moisture absorption.Thickness Tested: 0.062", 0.125" and 0.500"
CTE, linear, Transverse to Flow 20.0 µm/m-°C

@Thickness 1.57 mm,
Temperature 20.0 °C
11.1 µin/in-°F

@Thickness 0.0620 in,
Temperature 68.0 °F
x-axis; IPC-TM 650-2.4.24
Industrial Laminates/Norplex NP691 Paper Base Laminate
Description: Flame resistant, room temperature punching grade. NP691 is very similar to NP612 in electrical properties and mechanical strength, with improved moisture resistance.Thickness Tested: 0...
CTE, linear, Transverse to Flow 20.0 µm/m-°C

@Temperature -40.0 - 150 °C
11.1 µin/in-°F

@Temperature -40.0 - 302 °F
ASTM E 831
SABIC Innovative Plastics LNP THERMOCOMP LC00APXQ PEEK
LNP* THERMOCOMP* LC00APXQ is a compound based on Polyetheretherketone resin containing 50% Carbon Fiber. Added features of this material include: Exceptional Processing, Electrically Conductive.
CTE, linear, Transverse to Flow 20.0 µm/m-°C
11.1 µin/in-°F
ASTM E831
Sumitomo Bakelite North America CF 9040A Carbon Fiber Reinforced Phenolic
CF 9040A is a high strength carbon fiber phenolic molding compoundInformation provided by Sumitomo Bak North America, Inc.
CTE, linear, Transverse to Flow 20.0 - 30.0 µm/m-°C

@Temperature 20.0 °C
11.1 - 16.7 µin/in-°F

@Temperature 68.0 °F
TMA
Vyncolit 3640 CG Novolac Phenolic
Graphite filled phenolic molding compound with excellent dimensional stability. Self-lubricating and has a low coefficient of friction. Not suitable for electrical applications.USES: Gas meter par..
CTE, linear, Transverse to Flow 20.0 µm/m-°C

@Temperature 20.0 °C
11.1 µin/in-°F

@Temperature 68.0 °F
TMA
Vyncolit X655 Novolac Phenolic
Glass fiber and mineral filled phenolic molding compound with excellent dimensional stability and a very low coefficient of thermal expansion. UL listed.USES: Automotive disc brake pistons and gask..
CTE, linear, Transverse to Flow 20.0 - 30.0 µm/m-°C

@Temperature 20.0 °C
11.1 - 16.7 µin/in-°F

@Temperature 68.0 °F
TMA
Vyncolit X658 Novolac Phenolic
Glass fiber and mineral filled phenolic molding compound with excellent mechanical and thermal properties and a very good dimensional stability.USES: Complex precision parts.Information provided by ..
CTE, linear, Transverse to Flow 20.0 µm/m-°C

@Temperature 50.0 - 150 °C
11.1 µin/in-°F

@Temperature 122 - 302 °F
z direction; IPC TM-650 2.4.24
Arlon CLTE-AT Commercial Ceramic PTFE
Microwave material for improved thermal management, Excellent dimensional stability with high degree of phase stability vs. temperature.CLTE-AT is a micro-dispersed ceramic PTFE composite utilizing ..
CTE, linear, Transverse to Flow 20.0 µm/m-°C

@Temperature 50.0 - 150 °C
11.1 µin/in-°F

@Temperature 122 - 302 °F
z direction; IPC TM-650 2.4.24
Arlon CLTE-XT High Precision Ceramic PTFE
Microwave material for improved thermal management, Excellent dimensional stability with high degree of phase stability vs. temperature.CLTE-XT is a micro-dispersed ceramic PTFE composite utilizing ..
CTE, linear, Transverse to Flow 20.0 µm/m-°C
11.1 µin/in-°F
ASTM E 831
Arlon Thermabond® 48781A008 0.008" (0.203 mm) Uncured Silicone Rubber with Fiberglass Substrate
Description: Generation II Thermabond® NP electrically insulating electronic adhesive. Bonds without primer.Design/Construction: Liner 1: PolyethyleneSide 1: Uncured Silicone RubberSubstrate: Style..
CTE, linear, Transverse to Flow 20.0 µm/m-°C

@Temperature 50.0 - 150 °C
11.1 µin/in-°F

@Temperature 122 - 302 °F
z direction; IPC TM-650 2.4.24
Arlon AD1000 PTFE/Woven Fiberglass/Ceramic Filled Laminate for Microwave Printed Circuit Boards
Only Woven Glass Reinforced PTFE/Ceramic with Dk of 10.2 or greaterHigh Copper Peel Strength allows for thinner etched line widthsLowest insertion loss availableLarger Panel sizes availableLow moist..
CTE, linear, Transverse to Flow 20.0 µm/m-°C

@Temperature 23.0 °C
11.1 µin/in-°F

@Temperature 73.4 °F
Momentive Performance Materials HOPG Graphite Monochromator
Advanced Ceramics' graphite monochromators are highly oriented forms of high purity pyrolytic graphite which diffract x-rays and neutrons with greater efficiency than any other material. In x-r..
CTE, linear, Transverse to Flow 20.0 - 30.0 µm/m-°C

@Temperature 20.0 °C
11.1 - 16.7 µin/in-°F

@Temperature 68.0 °F
TMA
Vyncolit 3520 CG Novolac Phenolic
Graphite filled phenolic molding compound with excellent dimensional stability. Self-lubricating and has a low coefficient of friction. Not suitable for electrical applications.USES: Gas meter par..