Polymer Property : Charpy Impact, Notched = 0.250 J/cm² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Charpy Impact, Notched 0.150 - 0.250 J/cm²

@Temperature 23.0 °C
0.714 - 1.19 ft-lb/in²

@Temperature 73.4 °F
Injection and Compression; ISO 179/ 1eA
Raschig Group 3536 Epoxy
Glass-fiber reinforced epoxy molding compound. Good mechanical strength, very good electrical isolation properties and dimensional stability even at high temperatures. This product meets the allowed..
Charpy Impact, Notched 0.150 - 0.250 J/cm²

@Temperature 23.0 °C
0.714 - 1.19 ft-lb/in²

@Temperature 73.4 °F
Compression; ISO 179/ 1eA
Raschig Group AMPLA® 7250 melamine-modified polyester
Cellulose reinforced melamine-modified Polyester molding compound. Very good electrical values, excellent heat resistance, excellent surface quality, low post shrinkage. This product meets the allow..
Charpy Impact, Notched 0.150 - 0.250 J/cm²
0.714 - 1.19 ft-lb/in²
ISO 179/1eA
Raschig Group EN 5004 Epoxy Molding Compound
Mica reinforced molding compound. Low mold shrinkage and post-shrinkage, very good electrical values, outstanding heat resistance, very goo pourablity. This product meets the allowed upper limits fo..
Charpy Impact, Notched 0.150 - 0.250 J/cm²
0.714 - 1.19 ft-lb/in²
ISO 179/1eA
Raschig Group EN 5007 Epoxy Molding Compound
Mica reinforced molding compound. Low mold shrinkage and post-shrinkage, very good electrical values, outstanding heat resistance, very goo pourablity. This product meets the allowed upper limits fo..
Charpy Impact, Notched 0.150 - 0.250 J/cm²
0.714 - 1.19 ft-lb/in²
Injection; ISO 179/1eA
Raschig Group RALUPOL® 2100 UP Polyester
Organically and inorganically filled polyester molding compound. Low post-shrinkage, very good electrical values, good mechanical strength. This product meets the allowed upper limits for heavy meta..
Charpy Impact, Notched 0.200 - 0.250 J/cm²
0.952 - 1.19 ft-lb/in²
Compression; ISO 179/1eA
Raschig Group RALUPOL® 4566 UP Polyester
Glass-fiber reinforced polyester molding compound. Low mold shrinkage and post-shrinkage, good electrical values, excellent heat resistance, outstanding pourability. This product meets the allowed u..
Charpy Impact, Notched 0.150 - 0.250 J/cm²
0.714 - 1.19 ft-lb/in²
ISO 179
Vyncolit 3520 CG Novolac Phenolic
Graphite filled phenolic molding compound with excellent dimensional stability. Self-lubricating and has a low coefficient of friction. Not suitable for electrical applications.USES: Gas meter par..