Polymer Property : Tensile Modulus = 15.0 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 13.0 - 15.0 GPa
1890 - 2180 ksi
ISO 527
Vyncolit 3520 CG Novolac Phenolic
Graphite filled phenolic molding compound with excellent dimensional stability. Self-lubricating and has a low coefficient of friction. Not suitable for electrical applications.USES: Gas meter par..