| Category | Polymer , Thermoplastic , Polypropylene (PP) |
| Manufacturer | Techmer ES |
| Trade Name | HiFill® |
| Port | Ningbo port,China |
| Trade Terms | FOB, CFR, CIF |
| Payment Terms | L/C, T/T, Western Union |
| Download PDF | Techmer ES HiFill® PP 0159 B Polypropylene.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.59 g/cc | 0.0574 lb/in³ | ASTM D792 |
| Water Absorption | 0.050 % @Time 86400 sec |
0.050 % @Time 24.0 hour |
ASTM D570 |
| Linear Mold Shrinkage, Flow | 0.015 cm/cm @Thickness 3.17 mm |
0.015 in/in @Thickness 0.125 in |
ASTM D955 |
| Melt Flow | 10 g/10 min @Load 2.16 kg, Temperature 230 °C |
10 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Rockwell R | 95 | 95 | ASTM D785 |
| Tensile Strength, Yield | 18.6 MPa | 2700 psi | ASTM D638 |
| Elongation at Break | 20 % | 20 % | ASTM D638 |
| Flexural Strength | 34.5 MPa | 5000 psi | ASTM D790 |
| Flexural Modulus | 2.69 GPa | 390 ksi | ASTM D790 |
| Izod Impact, Notched | 0.267 J/cm @Thickness 3.17 mm |
0.500 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear, Parallel to Flow | 34.2 µm/m-°C | 19.0 µin/in-°F | ASTM D696 |
| Deflection Temperature at 0.46 MPa (66 psi) | 107 °C | 225 °F | Unannealed; ASTM D648 |