Manufacturer : Techmer ES Product List

Category
Nylon 6, 20% Glass Fiber Filled Nylon 6, Heat Stabilized Nylon 6, Impact Grade
Nylon 6, 30% Glass Fiber Filled Nylon 6, 40% Glass Fiber Filled Nylon 6, Nucleated
Nylon 66, 10% Glass Fiber Filled Nylon 66, Heat Stabilized Nylon 66, Impact Grade
Nylon 66, Glass Reinforced, Impact Grade Nylon 66, 20% Glass Fiber Filled Nylon 66, 30% Glass Fiber Filled
Nylon 66/6, 40% Glass Fiber Reinforced Nylon 66, 40% Glass Fiber Filled Nylon 66/6, Unreinforced
Polybutylene Terephthalate (PBT), Impact Grade Polybutylene Terephthalate (PBT), 30% Glass Fiber Filled Polycarbonate, Extruded
Polycarbonate, Impact Modified Polycarbonate, Molded Acetal Copolymer, Impact Modified
Nylon 66, 30% Mineral Filled Nylon 66, Mineral Filled, Impact Grade Acrylonitrile Butadiene Styrene (ABS), Stainless Steel Fiber Filled
Acrylonitrile Butadiene Styrene (ABS), 10% Carbon Fiber Filled Acrylonitrile Butadiene Styrene (ABS), 20% Carbon Fiber Filled Acrylonitrile Butadiene Styrene (ABS), 30% Carbon Fiber Filled
High Density Polyethylene (HDPE), Extruded Nylon 12, Carbon Fiber Filled Nylon 66, Conductive
Nylon 66, 10% Carbon Fiber Filled Nylon 66, 20% Carbon Fiber Filled Nylon 66, 30% Carbon Fiber Filled
Nylon 66, Stainless Steel Filled; EMI Grade Polycarbonate, Conductive Polycarbonate, Stainless Steel Fiber
Polycarbonate, Carbon Fiber Reinforced Polycarbonate/ABS Alloy, Antistat/Conductive Polycarbonate/PET Polyester Blend, Carbon Fiber Filled
PC/ABS + Stainless Steel Polyetherimide (PEI), Stainless Steel Filled Acetal Copolymer, Unreinforced
Acetal Copolymer, Carbon Fiber Filled Polyphenylene Sulfide (PPS) with 10% Carbon Fiber Filler Polyphenylene Sulfide (PPS), Conductive
Nylon 66, Carbon Fiber/PTFE Filled Nylon 66, 40% Carbon Fiber Filled Acrylonitrile Butadiene Styrene (ABS), 40% Carbon Fiber Filled
Polyphenylene Sulfide (PPS) with 20% Carbon Fiber Filler Polyphenylene Sulfide (PPS) with Carbon Fiber + PTFE Filler Nylon 6, Carbon Fiber Filled
Nylon 612, Carbon Fiber Filler Polycarbonate, Carbon + PTFE Filled Polystyrene, Carbon Black Filled
Acrylonitrile Butadiene Styrene (ABS), Unreinforced, Flame Retardant Acrylonitrile Butadiene Styrene (ABS), Glass Bead Filled Acrylonitrile Butadiene Styrene (ABS), 10% Glass Fiber Filled
Acrylonitrile Butadiene Styrene (ABS), 20% Glass Fiber Filled Acrylonitrile Butadiene Styrene (ABS), 30% Glass Fiber Filled Nylon 46, Flame Retarded + Glass Fiber Reinforced
Nylon 46, Lubricated + Glass Fiber Reinforced Nylon 6, Unreinforced, Flame Retardant Nylon 6, Unreinforced
Nylon 66, Unreinforced, Flame Retardant Nylon 66, Glass Bead Filled Polybutylene Terephthalate (PBT), Flame Retardant
Polybutylene Terephthalate (PBT), Carbon Fiber Filled ABS/Polyester Alloy Polycarbonate, Unreinforced, Flame Retardant
Polycarbonate, UV Stabilized Polycarbonate, 10% Glass Filled Polyethylene Terephthalate (PET), 20% Glass Reinforced
Polybutylene Terephthalate (PBT), Glass + Mineral Filled Acrylonitrile Butadiene Styrene (ABS), Molded Acrylonitrile Butadiene Styrene (ABS), Impact Grade, Molded
Acrylonitrile Butadiene Styrene (ABS), 40% Glass Fiber Filled Acrylonitrile/Styrene/Acrylate (ASA), Unreinforced, Molded Acrylonitrile/Styrene/Acrylate (ASA), 15% Glass Reinforced
ECTFE Fluoropolymer High Density Polyethylene (HDPE), Glass fiber Filled High Density Polyethylene (HDPE), Injection Molded
Polystyrene, Impact Grade, Glass Filled High Temperature Nylon Nylon 12, 30% Glass Fiber Filled
Nylon 46, Glass Fiber Reinforced Nylon 46, Unreinforced Nylon 6, 30% Mineral Filled
Nylon 6, 40% Mineral Filled Nylon 6, Extruded Nylon 6, Glass/Mineral Reinforced
Nylon 6, 50% Glass Fiber Filled Nylon 6, Glass Bead Filled Nylon 6, PTFE Filled
Nylon 6, 60% Glass Fiber Filled Nylon 610, Glass Reinforced Nylon 66, 20% Mineral Filled
Nylon 66, 40% Mineral Filled Nylon 66, Extruded Nylon 66, Glass/Carbon Fiber Filled
Nylon 66, Glass/Mineral Filled Nylon 66, PTFE Filled Nylon 66, 50% Glass Fiber Filled
Nylon 66, 60% Glass Fiber Filled Nylon 66, Nucleated Nylon 66, Unreinforced
Polybutylene Terephthalate (PBT), Extrusion Grade Polybutylene Terephthalate (PBT), Glass Bead Filled Polybutylene Terephthalate (PBT), 20% Glass Fiber Filled
Polybutylene Terephthalate (PBT), 40% Glass Fiber Filled Polybutylene Terephthalate (PBT), Heat Resistant Polybutylene Terephthalate (PBT), Mineral Filled
Polycarbonate, 20% Glass Filled Polycarbonate, 30% Glass Filled Polycarbonate, 40% Glass Filled
Polyetheretherketone, PEEK, Carbon Fiber Filled Polyetheretherketone, PEEK, Glass Fiber Filled Polyetherimide (PEI), 10% Glass Fiber
Polyetherimide (PEI), 20% Glass Fiber Polyetherimide (PEI), 30% Glass Fiber Polyethersulfone (PES), 10%Glass Fiber Filled
Polyethersulfone (PES), 20%Glass Fiber Filled Polyethersulfone (PES), PTFE Filled Polyethersulfone (PES), 30%Glass Fiber Filled
Polyethersulfone (PES), 40%Glass Fiber Filled Polyethylene Terephthalate (PET), Glass/Mineral Reinforced Polyethylene Terephthalate (PET), 50% Glass Reinforced
Polyethylene Terephthalate (PET), 60% Glass Reinforced Acetal Copolymer, Steel Filled Acetal Copolymer, Glass Bead Filled
Acetal Copolymer, 30% Glass Fiber Reinforced Acetal Copolymer, 10% Glass Fiber Reinforced Acetal Copolymer, 20% Glass Fiber Reinforced
Acetal Homopolymer, Unreinforced Polypropylene Copolymer Polypropylene, Molded
Polypropylene with 20% Glass Fiber Filler Polypropylene with 30% Glass Fiber Filler Polypropylene with 40% Glass Fiber Filler
Polypropylene, Carbon Black + Glass Fiber Filled Polypropylene with 10% Glass Fiber Filler Polypropylene Glass Bead Filled
Polypropylene with 60% Glass Fiber Filler Polypropylene, Glass/Mineral Reinforced Polypropylene with 50% Glass Fiber Filler
Polyphthalamide (PPA), 30% Glass Fiber Reinforced Polyphthalamide (PPA), 50% Glass Fiber Reinforced Polyphenylene Sulfide (PPS), Mineral/Glass-Fiber Filled
Polyphenylene Sulfide (PPS) with 40% Glass Fiber Filler Polysulfone, 10% Glass Fiber Reinforced Polyvinylidinefluoride (PVDF), with Carbon Fiber
Liquid Crystal Polymer (LCP), 30% Glass Fiber Filled Thermoplastic Polyurethane, Elastomer, Glass Filled Nylon 11 with 30% Glass Fiber Filler
Nylon 12, PTFE Filled Nylon 6, Carbon Fiber/PTFE Reinforced Nylon 612 with Molybdenum Sulfide Filler
Nylon 612, Unreinforced Nylon 66, Aramid Fiber Filled Polybutylene Terephthalate (PBT), PTFE Filled
Polycarbonate, PTFE Filled Polyetherimide (PEI), Carbon Fiber Filled Acetal Copolymer, PTFE Filled
Acetal Copolymer, Silicone Filled Acetal Homopolymer, PTFE-Filled Polyphthalamide (PPA), Carbon Fiber + PTFE Filled
Polyphenylene Sulfide (PPS), PTFE/Glass-Fiber Filled Polysulfone, 20% Glass Fiber Reinforced Nylon 66, 10% Mineral Filled
Polystyrene + Polyphenylene Ether + Nylon, Unreinforced Nylon 66, Glass Fiber/PTFE Filled Polybutylene Terephthalate (PBT), Glass Fiber + PTFE Filled
Nylon 6, Glass Fiber/Solid Lube Filled Nylon 612, Glass Fiber Filler Polycarbonate, Glass + PTFE Filled
Acrylonitrile Butadiene Styrene (ABS), Extruded Acrylonitrile Butadiene Styrene (ABS)/Nylon Blend Nylon 66/6, 60% Glass Fiber Reinforced
Acrylonitrile Butadiene Styrene (ABS)/Nylon Blend, Glass Reinforced ABS/Polyester Alloy + GF Polycarbonate/ABS Alloy, Unreinforced
Polycarbonate/ABS Alloy, Glass Fiber Filled Polycarbonate/ASA Alloy, Unreinforced Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Glass Filled
Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Unreinforced Polycarbonate/PET Polyester Blend Polysulfone, Modified
Polybutylene Terephthalate (PBT), 10% Glass Fiber Filled Polyphenylene Sulfide (PPS), Stainless Steel Fiber HDPE, Fiber Grade
Nylon 6, Stainless Steel Filled Polyethylene Terephthalate (PET), 30% Glass Reinforced Polypropylene, Extrusion Grade
Polypropylene, Flame Retardant Polypropylene, Impact Modified; Molded/Extruded Nylon 12, 50% Glass Fiber Filled
Polybutylene Terephthalate (PBT), Glass Filled, Impact Modified Polyphenylene Sulfide (PPS) with 10% Glass Fiber Filler Polyphenylsulfone (PPSU)
Acrylonitrile Butadiene Styrene (ABS), PTFE Filled Acetal Copolymer, Aramid Fiber Filled Polysulfone with PTFE/Silicone Filler
Thermoplastic Polyurethane, Elastomer, Polyester Grade Nylon 66, MoS2 Filled Polystyrene + Polyphenylene Ether, Glass + Mineral Filler
Polystyrene + Polyphenylene Ether, Glass Filler Syndiotactic Polystyrene (SPS) with Glass or Carbon Fiber
Trade Name
Elastoblend® Electrablend® Electrafil®
HiFill FR® HiFill® Luriblend®
Plaslube® Plastiblend® Statiblend®
Tips:Up to 100 items are displayed.
PRODUCT NO. Category Trade Name
Techmer ES Elastoblend® PA6 GF30 IM L 30% Glass Filled Nylon 6, 30% Glass Fiber Filled Elastoblend®
Techmer ES Electrablend® PA6/6 IM C BK Nylon 66, Conductive Electrablend®
Techmer ES Electrablend® PC 04006 FR BK Stainless Steel Filled Polycarbonate, Stainless Steel Fiber Electrablend®
Techmer ES Electrablend® PC/PET CF20 IM 20% Carbon Filled Polycarbonate/PET Polyester Blend, Carbon Fiber Filled Electrablend®
Techmer ES Electrablend® TPX-PC-02071 Stainless Steel Fiber Filled Polycarbonate, Stainless Steel Fiber Electrablend®
Techmer ES Electrafil® NY-7/EC NAT PA6 Nylon 6 Electrafil®
Techmer ES HiFill FR® TPX-HTN-01031 35% Glass Filled Nylon HiFill FR®
Techmer ES HiFill® HDPE TM30 30% Talc Filled HDPE HiFill®
Techmer ES HiFill® PA12 CM40 40% Mineral Filled Nylon 12 HiFill®
Techmer ES HiFill® PA6 0266 B Nylon 6 HiFill®
Techmer ES HiFill® PA6 AF Colors Nylon 6, Heat Stabilized HiFill®
Techmer ES HiFill® PA6 GF13 L BK 13% Glass Filled Nylon 6, 10% Glass Fiber Filled HiFill®
Techmer ES HiFill® PA6 GF20 L UV BK 20% Glass Filled Nylon 6, 20% Glass Fiber Filled HiFill®
Techmer ES HiFill® PA6 GF20 RM BK 20% Glass Filled Nylon 6, 20% Glass Fiber Filled HiFill®
Techmer ES HiFill® PA6 GF30 HS L BK 30% Glass Filled Nylon 6, 30% Glass Fiber Filled HiFill®
Techmer ES HiFill® PA6 GF33 IM L UV 33% Glass Filled Nylon 6, 30% Glass Fiber Filled HiFill®
Techmer ES HiFill® PA6 GF5 L 5% Glass Filled Nylon 6, 10% Glass Fiber Filled HiFill®
Techmer ES HiFill® PA6 GF50 RM LE 50% Glass Filled (Dry) Nylon 6, 50% Glass Fiber Filled HiFill®
Techmer ES HiFill® PA6/6 GF/M38 HS 38% Glass/Mineral Fiber Filled Nylon 66, Glass/Mineral Filled HiFill®
Techmer ES HiFill® PA6/6 GF33 HR HS BK 33% Glass Filled Nylon 66, Heat Stabilized HiFill®
Techmer ES HiFill® PA6/6 GF33 HS L BK 33% Glass Filled (Dry) Nylon 66, Heat Stabilized HiFill®
Techmer ES HiFill® PA6/6 LGF60 HS L BK 12 mm Nylon 66, 10% Glass Fiber Filled HiFill®
Techmer ES HiFill® PEEK CF30 HF 30% Carbon Filled Polyetheretherketone, PEEK, Carbon Fiber Filled HiFill®
Techmer ES HiFill® PP GF20 CC LE 20% Glass Filled Polypropylene with 20% Glass Fiber Filler HiFill®
Techmer ES Luriblend® PA6 ML3 BK Nylon 6 Nylon 6, Heat Stabilized Luriblend®
Techmer ES Luriblend® PA6/10 GF30 TS15 30% Glass Filled Nylon 610, Glass Reinforced Luriblend®
Techmer ES Luriblend® PA6/6 GF30 TL15 UV 30% Glass Filled Nylon 66, PTFE Filled Luriblend®
Techmer ES Luriblend® PA6/6 GF33 TL15 33% Glass Filled Nylon 66, PTFE Filled Luriblend®
Techmer ES Luriblend® PA6/6 GF33 TS15 33% Glass Filled Nylon 66, PTFE Filled Luriblend®
Techmer ES Luriblend® PA6/6 GF40 TL10 40% Glass Filled Nylon 66, PTFE Filled Luriblend®
Techmer ES Luriblend® PA6/6 X Nylon 66 Nylon 66, Unreinforced Luriblend®
Techmer ES Luriblend® PP GF20 GL2 BK 20% Glass Filled Polypropylene with 20% Glass Fiber Filler Luriblend®
Techmer ES Luriblend® TPX-PA6-95002 Nylon 6, Unreinforced Luriblend®
Techmer ES Plaslube® J-3/30/TF/13/SI/2 Nylon 6, 30% GFR, 13% PTFE, 2% Silicone Nylon 6, Glass Fiber/Solid Lube Filled Plaslube®
Techmer ES Plaslube® NY-1/TF/12 Nylon 66, 12% PTFE Nylon 66, PTFE Filled Plaslube®
Techmer ES Plastiblend® PC/ABS 720 BK Polycarbonate/ABS Alloy, Unreinforced Plastiblend®
Techmer ES Plastiblend® PC/PBT IM 5720 A BK Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Unreinforced Plastiblend®
Techmer ES Plastiblend® POM CO UV Acetal Copolymer, Unreinforced Plastiblend®
Techmer ES Plastiblend® PPS 05003 Polyphenylene Sulfide (PPS) Plastiblend®
Techmer ES Statiblend® PA6 GF30 AS BK 30% Glass Filled Nylon 6, 30% Glass Fiber Filled Statiblend®
Techmer ES Electrafil® J-50/CF/20 Polycarbonate, 20% Carbon Fiber Reinforced Polycarbonate, Carbon Fiber Reinforced Electrafil®
Techmer ES HiFill® PA6 0232 B Barium Sulfate Filler Nylon 6 HiFill®
Techmer ES HiFill® PA6 0390 S1 BK Nylon 6 HiFill®
Techmer ES HiFill® PBT GF15 15% Glass Filled Polybutylene Terephthalate (PBT), 20% Glass Fiber Filled HiFill®
Techmer ES Plaslube® J-1/30/TF/15 NAT PA66 Nylon 66, 30% Glass Fiber Filled Plaslube®
Techmer ES Plastiblend® PA6 GF20 RM L BK Nylon 6 Nylon 6, 20% Glass Fiber Filled Plastiblend®
Techmer ES Plaslube® J-50/30/TF/15 Polycarbonate, 30% Glass Reinforced, PTFE Lubricated Polycarbonate, Glass + PTFE Filled Plaslube®
Techmer ES HiFill® PA4/6 GF30 FR HS L 30% Glass Filled Nylon 46, Lubricated + Glass Fiber Reinforced HiFill®
Techmer ES HiFill® SPS GF40 BK 40% Glass Filled Syndiotactic Polystyrene (SPS) with Glass or Carbon Fiber HiFill®
Copyright © lookpolymers.com All Rights Reserved