Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 0.46 MPa (66 psi) | 107 °C | 225 °F | Unannealed; ASTM D648 |
Multibase Multi-Pro® 2006 T Polypropylene Talc Filler, 20% by weight.Forms:PelletsProcessing Methods:Injection MoldingInformation provided by Multibase |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 107 °C | 225 °F | ASTM D648 |
RheTech Products FT4802-01 Thermoplastic Polyolefin, Non-UV Stabilized, Black Applications: Bodyside moldings and claddingsFacia and bumper coversExterior componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 107 °C | 225 °F | ASTM D648 |
RheTech Products FT4802-690UV Thermoplastic Polyolefin, UV Stabilized, HS5 Medium Dark Neutral Applications: Bodyside moldings and claddingsFacia and bumper coversExterior componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 107 °C | 225 °F | ASTM D648 |
RheTech Products FT4802-691UV Thermoplastic Polyolefin, UV Stabilized, RJ3 Dark Grey Green Applications: Bodyside moldings and claddingsFacia and bumper coversExterior componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 107 °C | 225 °F | ASTM D648 |
RheTech Products FT4802-693UV Thermoplastic Polyolefin, UV Stabilized, SPN Dark Teal Applications: Bodyside moldings and claddingsFacia and bumper coversExterior componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 107 °C | 225 °F | ISO 75 |
Polyplastic Armlen® PP MF 15-3 FR Polypropylene Homopolymer, Mineral Filled Flame retardant, RoHS compliantInformation provided by PolyPlastic Group. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 107 °C | 225 °F | ASTM D648 |
PolyMirae Moplen HP600N Injection Molding Grade Polypropylene Moplen HP600N is the polypropylene homopolymer manufactured by PMC under the license of BASELL using the Spheripol process. Moplen HP600N is a homopolymer particularly suitable for injection molding.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 107 °C | 225 °F | ASTM D648 |
PolyMirae Moplen HP601N Injection Molding Grade Polypropylene Moplen HP601N is the polypropylene homopolymer manufactured by PMC under the license of BASELL using the Spheripol process. Moplen HP601N is a homopolymer typically used by customers in Glass Mat Sh.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 107 °C | 225 °F | ASTM D648 |
PolyMirae Moplen HP602N Injection Molding Grade Polypropylene Moplen HP602N is the polypropylene homopolymer manufactured by PMC under the license of BASELL using the Spheripol process. Moplen HP602N is a homopolymer particularly suitable for injection molding.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 107 °C | 225 °F | ASTM D648 |
Polymer Resources ABS-G20 ABS, 20% Glass Reinforced Acrylonitrile Butadiene Styrene, 20% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 107 °C | 225 °F | Unannealed; ASTM D648 |
PolyOne Stat-Tech™ AS-10NCF/000 ABS - 10% Nickel Coated Carbon Fiber
(discontinued **) Data provided by PolyOne. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 107 °C | 225 °F | Annealed, 80°C, 4 hours; ISO 75 |
LG Chemical XR-472 ABS, High Heat Resistance, High Gloss Information Provided by LG Chem |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 107 °C | 225 °F | ISO 75 |
LyondellBasell Hifaxâ„¢ BB222GC Thermoplastic Olefin Resin Key Features: medium melt flow, very high modulus, UV-stabilized thermoplastic elastomeric olefin resin, excellent impact and stiffness balance, excellent weatherability, high stiffness, good dimens.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 107 °C @Thickness 6.40 mm |
225 °F @Thickness 0.252 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics Xenoy® 5220U PBT+PC (Asia Pacific) Unreinforced PBT+PC Alloy. Impact Modified. Improved retention of mechanical properties under UV exposure. Excellent low temperature impact and chemical resistance. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 107 °C | 225 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® PP 0159 B Polypropylene Availability: North AmericaForms: PelletsFiller/Reinforcement: Unspecified Filler/ReinforInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 107 °C | 225 °F | Unannealed; ASTM D648 |
Techmer ES Plastiblend® ABS 8009 FR Availability: North AmericaForms: PelletsFeatures: Flame Retardant and High Heat ResistanceInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 107 °C | 225 °F | ISO 75 |
Styrolution Novodur® E211 ABS Novodur E211 is a high heat extrusion grade and suitable for blow moldingInformation provided by Styrolution |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 107 °C | 225 °F | ISO 75 |
Styrolution Novodur® H802 ABS Novodur H802 is a high heat injection molding grade with high stiffness, especially suitable for being painted.Information provided by Styrolution |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 107 °C | 225 °F | Flatw 80*10*4 sp=64mm; ISO 75/Bf |
SABIC Innovative Plastics LNP STAT-KON AE002 ABS (Europe-Africa-Middle East) LNP* STAT-KON* AE002 is a compound based on Acrylonitrile Butadiene Styrene resin containg Carbon Fiber. Added features include: Electrically Conductive |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 107 °C | 225 °F | ASTM D648 |
Plastics Group Polifil® GFABS-30 30% Glass-Reinforced Acrylonitrile-Butadiene Styrene (ABS) Polifil® GFABS series compounds combine the most desirable properties of both components - allowing for enhanced processability and toughness together with the stiffness of glass.Applications: Fire.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 107 °C | 225 °F | Unannealed; ASTM D648 |
Chase Plastics CP Pryme® A120 ABS, 20% Glass Fiber Reinforced Features: Glass fiber reinforcementInjection moldingForm: PelletsInformation provided by Chase Plastics. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 107 °C | 225 °F | ASTM D648 |
A. Schulman PP 3449-01 Polypropylene Copolymer Polypropylene DescriptionPolypropylene PP 3449-01 is a new generation copolymer polypropylene utilizing unique catalyst technology. Combining an excellent balance of high stiffness and impact. This product inc.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 107 °C | 225 °F | ASTM D648 |
A. Schulman PP 3449-01 Polypropylene Copolymer Polypropylene DescriptionPolypropylene PP 3449-01 is a new generation copolymer polypropylene utilizing unique catalyst technology. Combining an excellent balance of high stiffness and impact. This product inc.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 107 °C | 225 °F | ASTM D648 |
A. Schulman ComAlloy Hiloy® 272 Polystyrene Alloy, Glass Reinforced, Flow Enhanced Data provided by the manufacturer, ComAlloy International Company.20% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 107 °C | 225 °F | ASTM D648 |
Aaron Industries AAROLENE® ARPS HI-100-4 Polystyrene Compounded Resin AAROLENE® ARPS 100 Series Polystyrene Compounded ResinColor may be specified. Melt Flow Index may be specified. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 107 °C | 225 °F | ASTM D648 |
RheTech Products CC20P100-01 20% Calcium Carbonate Reinforced Polypropylene, Black Applications: ElectronicsConsumer GoodsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 107 °C | 225 °F | Unannealed; ISO 75-2/Bf |
Styron INSPIRE™ TF7000 ES Natural Performance Polymer INSPIRE* TF7000 ES Natural Performance Polymer DA™ is a very high stiffness (2400 MPa) TPO designed for instrument panel upper and lower components, as well as other interior trim applications wher.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 107 °C | 225 °F | Unannealed; ASTM D648 |
Teknor Apex Sinpolene CPP2030 Polypropylene Availability: Africa & Middle East; Latin America; Asia Pacific; South America Calcium Carbonate Filler, 30% Filler by Weight Features: Copolymer Uses: Automotive Applications; Industrial Applicati.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 107 °C | 225 °F | ASTM D648 |
Ineos H28U-00 Polypropylene Homopolymer
(discontinued **) Suggested fabrication methods: Injection moldingFeatures: Radiation stableTypical applications: MedicalComplies with FDA specification, Title 21, CFR 177.1520.Typical property data below from inject.. |