Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 2.69 GPa | 390 ksi | ASTM D790 |
PolyOne Geon™ Vinyl Packaging JGR 136A Clear 01FG Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Flexural Modulus | 2.69 GPa | 390 ksi | ASTM D790 |
PolyOne Geon™ Vinyl Packaging VB7 White 215 Polyvinyl Chloride, Rigid (PVC, Rigid) A rigid PVC Compound designed for extrusion blow molding balusters for railings.Information provided by PolyOne |
|||
Flexural Modulus | 2.69 GPa | 390 ksi | ASTM D790 |
PolyOne Geon™ Vinyl Rigid Molding MR201 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Flexural Modulus | 2.69 GPa | 390 ksi | Tangent; ASTM D790 |
RheTech Products T28P100-01EG 28% Talc Reinforced Polypropylene, Black, Extrusion Grade Applications: Window trimConsumer goodsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Flexural Modulus | 2.69 GPa | 390 ksi | Test Method I, Procedure B (chs speed 0.05 in/min), Tangent; ASTM D790 |
Network Polymers NPP 30-0200 TF20 Description: 20% Talc Filled Homopolymer PolypropyleneInformation provided by Network Polymers Inc. |
|||
Flexural Modulus | 2.69 GPa @Thickness 3.17 mm |
390 ksi @Thickness 0.125 in |
ASTM D790 |
PTS PCA-2201NHV Non Bromine, Non Chlorine Flame Retardant Polycarbonate/ABS Alloy, UV Stabilized Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Flexural Modulus | 2.69 GPa | 390 ksi | 13 mm/min; ASTM D790 |
PolyOne Edgetek® X AS/018 White Acrylonitrile Butadiene Styrene (ABS) The Edgetek® Engineering Thermoplastic Compounds portfolio covers a broad range of standard and custom-formulated high performance materials. This portfolio includes high-temperature materials for .. |
|||
Flexural Modulus | 2.69 GPa | 390 ksi | ASTM D790 |
Polymer Resources PC/ABS-FR1-[color]-HH Flame Retardant PC/ABS Alloy, Low Flow PC/ABS Alloy, Flame Retardant, Low FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by P.. |
|||
Flexural Modulus | 2.69 GPa | 390 ksi | ASTM D790 |
PolyOne Lubri-Tech™ AS-10GB/02S Acrylonitrile Butadiene Styrene (ABS), Glass Bead Filled
(discontinued **)< Description/Features:Glass Bead FilledSilicone LubricatedPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Flexural Modulus | 2.69 GPa | 390 ksi | ASTM D790 |
Solvay Specialty Polymers Udel® P-1700 LCD Polysulfone (PSU)
(Unverified Data**) Udel P-1700 LCD polysulfone is especially well suited for the fabrication of porous membranes for filtration applications. The membranes are usually in the form of hollow fibers, but tube, plate or .. |
|||
Flexural Modulus | 2.69 GPa | 390 ksi | Tangent; ASTM D790 |
Fiberfil® J-60/10/E8 Polypropylene Homopolymer, 10% Glass Reinforced, Chemically coupled Information provided by FIBERFIL Engineered Plastics |
|||
Flexural Modulus | 2.69 GPa | 390 ksi | ASTM D 790 |
MRC Polymers NAXALOY™ 793MF6 PC + Polyester Blend, 6% Mineral Filled • Available in natural and custom colors• Can be UV Stabilized• Internal and external lubricants can be addedInformation provided by MRC Polymers Inc. |
|||
Flexural Modulus | 2.69 GPa | 390 ksi | ASTM D790 |
Solvay Specialty Polymers Udel® P-1700 LCD Polysulfone (PSU) Udel® P-1700 LCD polysulfone is especially well suited for the fabrication of porous membranes for filtration applications. The membranes are usually in the form of hollow fibers, but tube, plate.. |
|||
Flexural Modulus | 2.69 GPa | 390 ksi | ASTM D790 |
Solvay Specialty Polymers Udel® P-3500 LCD Polysulfone (PSU) Udel® P-3500 LCD is a very high molecular weight grade of polysulfone, and therefore offers the greatest toughness and chemical resistance of the available grades. It is well-suited for extrusion.. |
|||
Flexural Modulus | 2.69 GPa | 390 ksi | ASTM D790 |
Solvay Specialty Polymers Udel® P-3703 Polysulfone (PSU) Udel® P-3703 is a high-flow grade of polysulfone intended for injection molding applications with thin walls or long flow lengths. This grade has higher flow than Udel® P-1700 and a slightly g.. |
|||
Flexural Modulus | 2.69 GPa | 390 ksi | ASTM D790 |
Techmer ES Luriblend® PA6 TL10 Nylon 6 Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer and PTFE Lubricant (10%)Features: Heat Stabilized and LubricatedAppearance: BlackInformation provided by TP Composites, Inc. |
|||
Flexural Modulus | 2.69 GPa | 390 ksi | ASTM D790 |
Techmer ES Plastiblend® PC/ABS FR 1950 BK Availability: North AmericaForms: PelletsFeatures: Flame RetardantAppearance: BlackInformation provided by TP Composites, Inc. |
|||
Flexural Modulus | 2.69 GPa | 390 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP RI001 PA 66 LNP* LUBRICOMP* RI001 is a compound based on Nylon 66 resin containing 2% Silicone. Added feature of this grade is: Wear Resistant. |
|||
Flexural Modulus | 2.69 GPa @Thickness 3.20 mm |
390 ksi @Thickness 0.126 in |
Injection Molded; ASTM D790 |
Styron EMERGEâ„¢ 7700 Polycarbonate (PC) / Acrylonitrile Butadiene Styrene (ABS) Overview: EMERGEâ„¢ PC/ABS 7700 Advanced Resin is an ignition-resistant PC/ABS blend that contains no chlorine for bromine additives. It has superior processability for injection molding applicat.. |
|||
Flexural Modulus | 2.69 GPa | 390 ksi | ASTM D790 |
Techmer ES Plastiblend® ABS LE WT Availability: North AmericaForms: PelletsFeatures: Low Extractables and Medium Impact ResistanceAppearance: WhiteInformation provided by TP Composites, Inc. |
|||
Flexural Modulus | 2.69 GPa | 390 ksi | ASTM D790 |
Clariant Renol PCSP0005 Polycarbonate/ASA Alloy, Flame Retardant Data provided by Clariant Masterbatches |
|||
Flexural Modulus | 2.69 GPa @Temperature 22.8 °C |
390 ksi @Temperature 73.0 °F |
ASTM D790 |
Ensinger TECASON™ S Polysulfone (PSU) TECASON™ S is a transparent engineering plastic known for its chemical resistance, rigidity, high-temperature performance, and its ability to operate in an autoclave environment. TECASON™ S is FD.. |
|||
Flexural Modulus | 2.69 GPa | 390 ksi | ASTM D790 |
Clariant Renol 6601L Nylon 66, Lubricated Data provided by Clariant Masterbatches |
|||
Flexural Modulus | 2.69 GPa | 390 ksi | ASTM D790 |
Aaron Industries AVPS H 100-3 Virgin Polystyrene Melt flow index may be specified. |