Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Flow | 0.015 - 0.019 cm/cm @Thickness 3.17 mm |
0.015 - 0.019 in/in @Thickness 0.125 in |
ASTM D955 |
Ravago Manufacturing Americas Enviramid™ N1300HL BK/UV2 Post Consumer Recycle Nylon 66 Heat Stabilized, Lubricated, UV Stabilized, Black and made from EnViramid Post Consumer Recycled NylonInformation provided by Ravago. |
|||
Linear Mold Shrinkage, Flow | 0.015 - 0.019 cm/cm @Thickness 3.17 mm |
0.015 - 0.019 in/in @Thickness 0.125 in |
ASTM D955 |
Ravago Manufacturing Americas Enviramid™ N1300STHL Post Consumer Recycle Nylon 66 Superior Toughness, Heat Stabilized, Lubricated, Black and made from EnViramid™ Post Consumer Recycled NylonInformation provided by Ravago. |
|||
Linear Mold Shrinkage, Flow | 0.015 - 0.019 cm/cm | 0.015 - 0.019 in/in | ASTM D955 |
PolyOne Geon™ Vinyl Flexible B70CA Polyvinyl Chloride, Flexible (PVC, Flexible) Improved adhesion.Information provided by PolyOne |
|||
Linear Mold Shrinkage, Flow | 0.015 - 0.018 cm/cm | 0.015 - 0.018 in/in | ASTM D955 |
LyondellBasell Moplen HP400H Polypropylene Homopolymer Description: Moplen HP400H is a homopolymer for extrusion applications. Moplen HP400H exhibits easy processability and a good stiffness/impact balance at ambient temperature. The main applications .. |
|||
Linear Mold Shrinkage, Flow | 0.015 cm/cm @Thickness 3.17 mm |
0.015 in/in @Thickness 0.125 in |
ASTM D955 |
Techmer ES Elastoblend® PA6 IM L N Availability: North AmericaForms: PelletsAdditive: Impact Modifier and LubricantFeatures: Impact Modified and LubricatedAppearance: Natural ColorInformation provided by TP Composites, Inc. |
|||
Linear Mold Shrinkage, Flow | 0.015 - 0.016 cm/cm | 0.015 - 0.016 in/in | mold temp=100°C; SABIC Method |
SABIC Innovative Plastics LNP STAT-KON KD000 Acetal Copolymer (Europe-Africa-Middle East) LNP STAT-KON KD000* is also know as: LNP STAT-KON K, LNP STAT-KON KXC. It is a compound based on Acetal resin containing Carbon Powder. Added features of this material include: Electrically Conduct.. |
|||
Linear Mold Shrinkage, Flow | 0.015 - 0.035 cm/cm @Time 86400 sec |
0.015 - 0.035 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP STAT-KON KD000 Acetal Copolymer (Europe-Africa-Middle East) LNP STAT-KON KD000* is also know as: LNP STAT-KON K, LNP STAT-KON KXC. It is a compound based on Acetal resin containing Carbon Powder. Added features of this material include: Electrically Conduct.. |
|||
Linear Mold Shrinkage, Flow | 0.015 cm/cm @Thickness 3.17 mm |
0.015 in/in @Thickness 0.125 in |
ASTM D955 |
Techmer ES HiFill® PA6/6 GB20 L BK 20% Glass Bead Filler Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Bead, 20% Filler by WeightAdditive: LubricantFeatures: LubricatedAppearance: BlackInformation provided by TP Composites, Inc. |
|||
Linear Mold Shrinkage, Flow | 0.015 cm/cm @Thickness 3.17 mm |
0.015 in/in @Thickness 0.125 in |
ASTM D955 |
Techmer ES HiFill® PA6/6 GB30 L 30% Glass Bead Filler Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Bead, 30% Filler by WeightAdditive: LubricantFeatures: LubricatedInformation provided by TP Composites, Inc. |
|||
Linear Mold Shrinkage, Flow | 0.015 cm/cm @Thickness 3.17 mm |
0.015 in/in @Thickness 0.125 in |
ASTM D955 |
Techmer ES HiFill® PP 0159 B Polypropylene Availability: North AmericaForms: PelletsFiller/Reinforcement: Unspecified Filler/ReinforInformation provided by TP Composites, Inc. |
|||
Linear Mold Shrinkage, Flow | 0.015 - 0.025 cm/cm | 0.015 - 0.025 in/in | ASTM D955 |
Shinkong Synthetic Fibers Shinite® T102 PET, Fire Retardant Information from Shinkong Synthetic Fibers Corp. |
|||
Linear Mold Shrinkage, Flow | 0.015 cm/cm @Thickness 3.17 mm |
0.015 in/in @Thickness 0.125 in |
ASTM D955 |
Techmer ES Luriblend® PA6/6 TL20 Nylon 66 Availability: North AmericaForms: PelletsAdditive: PTFE Lubricant(20%)Features: Lubricated, Low Friction and Good Wear ResistanceUL File Number: E157318TPCI# 9740101Information provided by TP Compos.. |
|||
Linear Mold Shrinkage, Flow | 0.015 - 0.035 cm/cm @Time 86400 sec |
0.015 - 0.035 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP STAT-KON KD000 Acetal Copolymer LNP* STAT-KON* KD000 is a compound based on Acetal resin containing Proprietary Filler(s). Added feature of this material is: Electrically Conductive. |
|||
Linear Mold Shrinkage, Flow | 0.015 cm/cm @Thickness 3.17 mm |
0.015 in/in @Thickness 0.125 in |
ASTM D955 |
Techmer ES Luriblend® HDPE TL10 Availability: North AmericaForms: PelletsAdditive: PTFE LubricantInformation provided by TP Composites, Inc. |
|||
Linear Mold Shrinkage, Flow | 0.015 - 0.019 cm/cm | 0.015 - 0.019 in/in | ISO DIS 294-4 |
Wellman Wellamid® 22LHI6 XE-NBK1 Impact Modified Nylon 66 Description: Impact Modified Nylon 66Information provided by Wellman. |
|||
Linear Mold Shrinkage, Flow | 0.015 - 0.025 cm/cm | 0.015 - 0.025 in/in | ASTM D955 |
Elastocon TPE Technologies Elastocon® 8028N Thermoplastic Elastomer Elastocon® 8028N is a colorable thermoplastic elastomer formulated for applications that require rubber-like properties and a good surface finish. Elastocon® 8028N is FDA compliant and well suited.. |
|||
Linear Mold Shrinkage, Flow | 0.015 - 0.025 cm/cm | 0.015 - 0.025 in/in | ASTM D955 |
Elastocon TPE Technologies Elastocon® STK60 Thermoplastic Elastomer Elastocon® STK60 thermoplastic elastomer has been developed for applications that require ultra soft rubber-like properties and a good surface finish. Elastocon® STK60 is FDA compliant and well s.. |
|||
Linear Mold Shrinkage, Flow | 0.015 - 0.025 cm/cm | 0.015 - 0.025 in/in | ASTM D955 |
Elastocon TPE Technologies Elastocon® STK70 Thermoplastic Elastomer Elastocon® STK70 thermoplastic elastomer has been developed for applications that require ultra soft rubber-like properties and a good surface finish. Elastocon® STK70 is well suited for consumer.. |
|||
Linear Mold Shrinkage, Flow | 0.015 cm/cm | 0.015 in/in | ISO 294-4 |
DSM Novamid® ST120 NAT PA6-I Impact Modified, Injection Molding |
|||
Linear Mold Shrinkage, Flow | 0.015 cm/cm | 0.015 in/in | DAM; ISO 294-4 2577 |
DuPont Performance Polymers Zytel® EFE1068 NC010T Nylon 66
(Unverified Data**) Unreinforced Polyamide 66Zytel EFE1068 NC010T is a lubricated polyamide 66 for injection molding. It has excellent flow characteristics and was developed for fast production cycles and high producti.. |
|||
Linear Mold Shrinkage, Flow | 0.015 cm/cm | 0.015 in/in | ASTM D955 |
Clariant Renol PA123 Nylon 66, Impact Modified, Heat Stabilized, Lubricated Data provided by Clariant Masterbatches |
|||
Linear Mold Shrinkage, Flow | 0.015 cm/cm | 0.015 in/in | ASTM D955 |
Clariant Renol 6642 2% Moly Nylon 66, Extrusion Grade, 2% Molybdenum Disulfide Lubricated Data provided by Clariant Masterbatches |
|||
Linear Mold Shrinkage, Flow | 0.015 cm/cm | 0.015 in/in | Eurotec |
Eurotec® Tecodur® PB70 NL XA20 PBT, flame retardant - halogen (RoHS compliant), heat stabilized, natural Information provided by Eurotec® |
|||
Linear Mold Shrinkage, Flow | 0.015 cm/cm | 0.015 in/in | Eurotec |
Eurotec® Tecomid® NA40 NL IX PA6.6, impact modified, natural Information provided by Eurotec® |
|||
Linear Mold Shrinkage, Flow | 0.015 cm/cm @Thickness 4.00 mm, Time 86400 sec |
0.015 in/in @Thickness 0.157 in, Time 24.0 hour |
|
Arkema Group Pebax® Rnew 72R53 SP 01 Polyether Block Amide (PEBA) Polyether block amide Pebax® 72R53 SP 01 is a thermoplastic elastomer made of flexible polyether and rigid polyamide based on renewable resources. This SP grade has been developed to be heat and UV.. |
|||
Linear Mold Shrinkage, Flow | 0.015 cm/cm | 0.015 in/in | |
BASF Procom® D 1189 Polypropylene Data was collected by ISO methods and provided by BASF. |
|||
Linear Mold Shrinkage, Flow | 0.015 cm/cm | 0.015 in/in | ISO 294-4 |
Azoty Tarnow™ Tarnamid® T-27 MTR Polyamide 6 - Transparent Medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.Transparent up to maximum 2.5 mm.Tarnamid® has the following main properties.. |
|||
Linear Mold Shrinkage, Flow | 0.015 cm/cm | 0.015 in/in | Sheet |
BASF Ultradur® B 4406 PBT Description: Is a PBT, flame-retardant injection-molding grades, unreinforced for parts requiring enhanced fire resistance, e.g. plug-and-socket connectors, housings, coil formers and lighting compo.. |
|||
Linear Mold Shrinkage, Flow | 0.015 cm/cm @Thickness 2.00 mm |
0.015 in/in @Thickness 0.0787 in |
DAM; ISO 294-4 |
DuPont Performance Polymers Zytel® FG408L NC010 Nylon 66
(Unverified Data**) Zytel® FG408L NC010 is a general purpose, lubricated, impact modified polyamide 66 resin with superior toughness for injection molding applications. It has been developed for consideration into app.. |
|||
Linear Mold Shrinkage, Flow | 0.015 cm/cm | 0.015 in/in | DAM; ISO 294-4 2577 |
DuPont Performance Polymers Zytel® RS 3261THSL BK041A Nylon 610
(Unverified Data**) Toughened Renewably Sourced Polyamide 610 Developed for Injection Molding Zytel RS 3261THSL BK041A is a renewably sourced polyamide 610 resin containing a minimum of 47% renewably sourced ingredient.. |