Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.59 g/cc | 0.0574 lb/in³ | ASTM D792 |
PTS Lucet® GC-225 25% Glass Reinforced Acetal Copolymer Information provided by US distributor Polymer Technology and Services, LLC (PTS). |
|||
Density | 1.59 g/cc | 0.0574 lb/in³ | ISO 1183 |
LATI LATAN 13 G/303 30% Glass Fiber Reinforced Polyoxymethylene Copolymer (POM)
(discontinued **) Description: Latan series thermoplastics are polyoxymethylene copolymer (POM) products. The main applications for Latan feature good wear resistance, chemical inertness and low water absorption (gea.. |
|||
Density | 1.59 - 1.60 g/cc | 0.0574 - 0.0578 lb/in³ | Average value: 1.59 g/cc Grade Count:5 |
Overview of materials for Polyetherimide (PEI), 40% Glass Fiber This property data is a summary of similar materials in the MatWeb database for the category "Polyetherimide, 40% Glass Fiber". Specific grades with glass content between 35% and 44% are included. E.. |
|||
Density | 1.59 g/cc | 0.0574 lb/in³ | (DAM); ISO 1183 |
DSM Akulon® S224-KMV7 Nylon 66-35% Mineral Reinforced (European and Asian Grade) (Cond)
(discontinued **) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
Density | 1.59 - 1.86 g/cc | 0.0574 - 0.0672 lb/in³ | Average value: 1.75 g/cc Grade Count:15 |
Overview of materials for Modified ETFE, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Modified ETFE, Unreinforced". Each property range of values reported is minimum and maximum values of ap.. |
|||
Density | 1.59 g/cc | 0.0574 lb/in³ | |
LATI Latan 13 G/30 POM, 30% Glass Fiber Reinforced Polyoxymethylene (POM) based compound. Glass fibers. Medium viscosity. Good tribological properties.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation .. |
|||
Density | 1.59 g/cc | 0.0574 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP LUBRICOMP DX07035 PC (Europe-Africa-Middle East) LNP* LUBRICOMP* DX07035 is a compound based on Polycarbonate resin containing Glass Fiber, PTFE, Flame Retardant. Added features include: Flame retardant, Easy Molding, Internally Lubricated, Mold R.. |
|||
Density | 1.59 g/cc | 0.0574 lb/in³ | ASTM D 792 |
SABIC Innovative Plastics LNP Lubricomp EFP36G PEI LNP* EFP36G is a Polyetherimide base resin containing a Mixed Glass Fiber and PTFE/Silicone.This data was supplied by SABIC-IP for the Americas region. |
|||
Density | 1.59 g/cc | 0.0574 lb/in³ | ASTM D792 |
Techmer ES HiFill® PET GF/M35 35% Glass/Mineral Fiber Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass/Mineral, 35% Filler by WeightInformation provided by TP Composites, Inc. |
|||
Density | 1.59 g/cc | 0.0574 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP Thermocomp OK006 PPS - Linear LNP* Thermocomp* OK006 is based on a Linear Polyphenylene Sulfide (PPS) containing Talc.This data was supplied by SABIC-IP for the Americas region. |
|||
Density | 1.59 g/cc | 0.0574 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP THERMOCOMP RX05491 PA 66 LNP* Thermocomp* RX05491 is a compound based on Nylon 66 resin containing Glass Fiber. Added features of this material include: Heat Stabilized. |
|||
Density | 1.59 g/cc | 0.0574 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP VERTON RV00AE PA 66 LNP* VERTON* RV00AE is a compound based on Nylon 66 containing 50% Long Glass Fiber. Added features of this grade include: Easy Molding, Structural. |
|||
Density | 1.59 g/cc | 0.0574 lb/in³ | ASTM D792 |
Plenco 3509 Phenolic, Granular, Compression Molded PLENCO 03509 is a mineral and flock filled phenolic molding compound offering excellent electrical properties, dimensional stability, and improved heat resistance. UL recognized under component file.. |
|||
Density | 1.59 g/cc | 0.0574 lb/in³ | ASTM D792 |
Plenco 4527 Phenolic, Granular, Transfer Molded PLENCO 04527 is a heat resistant, mineral and flock filled phenolic molding compound, offering excellent mechanical strength, and resistance to cracking in a wet-dry environment. UL recognized under.. |
|||
Density | 1.59 g/cc | 0.0574 lb/in³ | |
Toyobo ECOVYLOPET® EMC2330 PET Bottle Recycling Grade, 30% Glass Reinforced Features: PET Bottle Recycling Grade, 30% Glass Fiber Reinforced, General PurposeApplications: Automobile engine head coversHot platesVending machine partsUmbrella ribsInformation provided by Toyobo.. |
|||
Density | 1.59 g/cc | 0.0574 lb/in³ | ASTM D792 |
Toyobo Vylopet® EMC310K Glass Reinforced Polyester, Easy Molding Grade Key Feature: HB UL-94 classApplications: General componentsGeneral features of Vylopet® include heat resistance, good mechanical properties, high dielectric strength and tracking resistance, chemic.. |
|||
Density | 1.59 g/cc | 0.0574 lb/in³ | ASTM D792 |
Toyobo Vylopet® EMC330K Glass Reinforced Polyester, Easy Molding Grade HB UL-94 classApplications: General and high rigidity componentsGeneral features of Vylopet® include heat resistance, good mechanical properties, high dielectric strength and tracking resistance, c.. |
|||
Density | 1.59 g/cc | 0.0574 lb/in³ | |
Trelleborg Emerson & Cuming Stycast® S5225 Two-Component Easy Mix Ratio Encapsulant Features and Typical ApplicationsPrimarily designed for ease of use in either meter mix or manual dispense operations. These products also offer a wide range of features including heat dissipation, .. |
|||
Density | 1.59 g/cc | 0.0574 lb/in³ | dry; ISO 1183 |
DSM Akulon® Ultraflow K-FKGS6 /B PA6-GF30 FR(17) 30% Glass Reinforced, Heat Stabilized, Flame Retardant, High Flow |
|||
Density | 1.59 g/cc | 0.0574 lb/in³ | ISO 1183 |
EMS-Grivory Grivory® G4V-5H black 9915 PA*-GF50 Product description: Grivory G4V-5H is a 50% glass fiber reinforced engineering thermoplastic material based on a semi-crystalline partially aromatic copolyamide. Grivory G4V-5H is used for injectio.. |
|||
Density | 1.59 g/cc | 0.0574 lb/in³ | ISO 1183 |
EMS-Grivory Grivory® XE 4116 nat PA1010-GF55 Product description: Grilamid XE 4116 natural is a 55% glass fiber reinforced Polyamide 1010 injection molding grade. This grade is especially suitable for the manufacturing of thin-walled, painted .. |
|||
Density | 1.59 g/cc | 0.0574 lb/in³ | DAM; ISO 1183 |
DuPont Performance Polymers Zytel® HTN 53G50HSLR NC010 Polyphthalamide (PPA)
(Unverified Data**) 50% Glass Reinforced High Performance Polyamide with Improved Impact and Stiffness Zytel HTN53G50HSLR NC010 is a 50% glass reinforced heat stabilized lubricated high performance polyamide resin deve.. |
|||
Density | 1.59 g/cc | 0.0574 lb/in³ | ISO 1183 |
DSM Arnite® B434 SE PBT-GF20 FR(17) 20% Glass Reinforced, Flame Retardant |
|||
Density | 1.59 g/cc | 0.0574 lb/in³ | cured 14 days @ 50% RH; AMS-S-8802 |
3M AC-251 Black Class B-1 Aerospace Sealant 3M Aerospace Sealant AC-251 Black Class B are two-part, quick curing, polysulfide based canopy and windshield sealants. These products are formulated for sealing acrylic, glass, and polycarbonate ai.. |
|||
Density | 1.59 g/cc | 0.0574 lb/in³ | cured 14 days @ 50% RH; AMS-S-8802 |
3M AC-251 Black Class B-1/2 Aerospace Sealant 3M Aerospace Sealant AC-251 Black Class B are two-part, quick curing, polysulfide based canopy and windshield sealants. These products are formulated for sealing acrylic, glass, and polycarbonate ai.. |
|||
Density | 1.59 g/cc | 0.0574 lb/in³ | cured 14 days @ 50% RH; AMS-S-8802 |
3M AC-251 Gray Class B-2 Aerospace Sealant 3M Aerospace Sealant AC-251 Gray Class B are two-part, quick curing, polysulfide based canopy and windshield sealants. These products are formulated for sealing acrylic, glass, and polycarbonate air.. |
|||
Density | 1.59 g/cc | 0.0574 lb/in³ | ISO 1183 |
Polyplastics Duracon® GB-25 Acetal Co-polymer (POM), Low warpage, GB 25% filling DURACON® is a crystalline thermoplastic acetal copolymer. The primary raw material trioxane, a trimer of formaldehyde.The thermoplastic adopts a copolymer structure in which polyoxymethylene (-C-O).. |