Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 18.6 MPa | 2700 psi | Type IV, 510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Wire & Cable 2510-xx05D Polyvinyl Chloride Alloy (PVC Alloy) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne |
|||
Tensile Strength, Yield | 18.6 MPa | 2700 psi | 2 in/min; ASTM D638 |
Polimeros Mexicanos Rotolene® Industrial Black Linear Medium Density Polyethylene Hexene Copolymer Linear Medium Density Polyethylene grade which is fully UV8 stabilized. High quality Polyethylene compounded in black, formulated for rotational molding applications requiring excel.. |
|||
Tensile Strength, Yield | 18.6 MPa | 2700 psi | 2 in per min; ASTM D638 |
Network Polymers NPP 25-2001 Description: Copolymer PolypropyleneInformation provided by Network Polymers Inc. |
|||
Tensile Strength, Yield | 18.6 MPa | 2700 psi | |
Resinlab® CYNERGY CA6012 Adhesive Description: The CYNERGY 6000 SERIES are for use in demanding applications where very fast cure speeds are required. These are single component solvent free materials manufactured in a wide variety.. |
|||
Tensile Strength, Yield | 18.6 MPa | 2700 psi | |
Resinlab® CYNERGY CA6301 Adhesive Description: The CYNERGY 6300 SERIES products are for use in applications where a faster set time is desired or low moisture conditions exist. Provides good bonds to a wide variety of materials.Appl.. |
|||
Tensile Strength, Yield | 18.6 MPa | 2700 psi | |
Resinlab® CYNERGY CA6309 Adhesive Description: The CYNERGY 6300 SERIES products are for use in applications where a faster set time is desired or low moisture conditions exist. Provides good bonds to a wide variety of materials.Appl.. |
|||
Tensile Strength, Yield | 18.6 MPa | 2700 psi | |
Resinlab® CYNERGY CA6310 Adhesive Description: The CYNERGY 6300 SERIES products are for use in applications where a faster set time is desired or low moisture conditions exist. Provides good bonds to a wide variety of materials.Appl.. |
|||
Tensile Strength, Yield | 18.6 MPa | 2700 psi | |
Resinlab® CYNERGY CA6902 Adhesive Description: The CYNERGY 6900 SERIES are for use in demanding applications where very fast cure speeds and high temperature resistance are required. These are single component solvent free materials.. |
|||
Tensile Strength, Yield | 18.6 MPa | 2700 psi | Type IV, 510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Flexible R7661A Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne |
|||
Tensile Strength, Yield | 18.6 MPa | 2700 psi | ASTM D638 |
Rochling Engineered Plastics Polystone® MPG Glass filled (UHMW-PE) Polystone® M is a highly versatile polymer that features: Low coefficient of friction Excellent abrasion resistance High-impact strength Chemical resistance Complies with FDA regulations under the .. |
|||
Tensile Strength, Yield | 18.6 MPa | 2700 psi | 2" (50mm) per min.; ASTM D638 |
Formosa Plastics Formolene® L63565 Rotational Molding LLDPE
(discontinued **) Hexene CopolymerApplications: Toys, medium tanks, material handling equipment and flat surface rotational molding applications.Meets all requirements of the U.S. Food and Drug Administration as spec.. |
|||
Tensile Strength, Yield | 18.6 MPa | 2700 psi | 2" (50mm) per min; ASTM D638 |
Formosa Plastics Formolene® L63568 Rotational Molding LLDPE
(discontinued **) Linear Low Density Polyethylene Hexene Copolymer for Rotational Molding Formolene® L63568 is a general-purpose rotational molding linear low density resin made using the BP Gas Phase Process™. The.. |
|||
Tensile Strength, Yield | 18.6 MPa | 2700 psi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 30 PHR Iceberg Clay Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
Tensile Strength, Yield | 18.6 MPa | 2700 psi | ASTM D638 |
Ineos B35-150-134 MDPE
(discontinued **) Fortiflex® B35-150-134 is an intermediate density polyethylene copolymer developed for injection blow molding. It exhibits excellent gloss and environmental stress crack resistance (ESCR) in molde.. |
|||
Tensile Strength, Yield | 18.6 MPa | 2700 psi | |
Resinlab® CYNERGY CA6304 Adhesive Description: The CYNERGY 6300 SERIES products are for use in applications where a faster set time is desired or low moisture conditions exist. Provides good bonds to a wide variety of materials.Appl.. |
|||
Tensile Strength, Yield | 18.6 MPa | 2700 psi | |
Resinlab® CYNERGY CA6307 Adhesive Description: The CYNERGY 6300 SERIES products are for use in applications where a faster set time is desired or low moisture conditions exist. Provides good bonds to a wide variety of materials.Appl.. |
|||
Tensile Strength, Yield | 18.6 MPa | 2700 psi | |
Resinlab® CYNERGY CA6808 Adhesive Description: The CYNERGY 6800 SERIES are clear, high strength products ideal for bonding dissimilar materials with excellent performance on a wide range of surfaces. This series of products has USP .. |
|||
Tensile Strength, Yield | 18.6 MPa | 2700 psi | |
Resinlab® CYNERGY CA6810 Adhesive Description: The CYNERGY 6800 SERIES are clear, high strength products ideal for bonding dissimilar materials with excellent performance on a wide range of surfaces. This series of products has USP .. |
|||
Tensile Strength, Yield | 18.6 MPa | 2700 psi | |
Green Dot Terratek® BD 4015 Biodegradable Polymer Terratek BD biodegradable composites are created from a proprietary blend of starch-based ingredients and other materials, the natural components derived from renewable grain sources account for the.. |
|||
Tensile Strength, Yield | 18.6 MPa | 2700 psi | 9.8 in/min; ASTM D638 |
Teknor Apex Sinvicomp SGH 3500 Polyvinyl Chloride, Flexible Availability: Asia Pacific Uses: Garden Hose Forms: Pellets Processing Method: ExtrusionInformation Provided by Teknor Apex |
|||
Tensile Strength, Yield | >= 18.6 MPa | >= 2700 psi | Heat Aging (7 Days at 121°C); ASTM D412 |
Borealis Visico™/Ambicat™ ME4425/LE4472 Ambient Curing, Moisture-Crosslinking Polyethylene Compound for Low Voltage Insulation Visico LE4423 is a natural, ethylene vinyl silane copolymer that, when combined with the catalyst masterbatch Ambicat LE4472, will undergo an accelerated, moisture-induced crosslinking reaction. Th.. |
|||
Tensile Strength, Yield | 18.6 MPa | 2700 psi | |
Zylog Hipolyene® 5198 FLM Thermoplastic Polyolefin & PP Compound Information provided by Zylog Plastalloys Pvt. Ltd. |
|||
Tensile Strength, Yield | 18.6 MPa | 2700 psi | ASTM D638 |
Borealis Supersmooth™ LE0500 Crosslinkable Semiconductive Shielding Compound Supersmooth LE0500 is a crosslinkable compound recommended as conductor and bonded insulation shielding for crosslinked polyethylene insulation. Supersmooth LE0500 is based on an ethylene butyl acry.. |
|||
Tensile Strength, Yield | 18.6 MPa | 2700 psi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 60 PHR Atomite Whiting Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
Tensile Strength, Yield | 18.6 MPa | 2700 psi | 50 mm/min cross speed; ASTM D638 |
DuPont™ Surlyn® 8150 Ionomer Resin, Sodium Surlyn® 8150 thermoplastic resin is an advanced ethylene/methacrylic acid (E/MAA) copolymer, in which the MAA acid groups have been partially neutralized with sodium ions. The high MAA content and .. |
|||
Tensile Strength, Yield | >= 18.6 MPa | >= 2700 psi | ASTM D638 |
Buckeye Polymers BP PPC 0212 BLK Polypropylene Copolymer Product Information: Black Polypropylene Copolymer good for general purpose programs requiring moderate impact resistance.Product Features:Good impact resistanceGood UV resistanceGood chemical resis.. |
|||
Tensile Strength, Yield | 18.6 MPa | 2700 psi | ASTM D-638 |
Axiall 22950 Coax & Telecom Flexible PVC Riser jacket, 25 mil over HDPE primaries.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Tensile Strength, Yield | 18.6 MPa | 2700 psi | ASTM D-638 |
Axiall EX1063 Coax & Telecom Flexible PVC Non-lead stabilized, fiber optic compound.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Tensile Strength, Yield | 18.6 MPa | 2700 psi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 30 PHR Iceberg Clay Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |