Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 0.46 MPa (66 psi) | 107 °C | 225 °F | ASTM D648-95 |
Multibase Multi-Pro® 2005 T BLK Polypropylene PP compound suitable for automotive applications, meets elevated temperature resistance. Meets ESH-M4D-293-B specifications.Data provided by Multibase. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 107 °C | 225 °F | ASTM D648 |
RheTech Products FT4802-01UV Thermoplastic Polyolefin, UV Stabilized, Black Applications: Bodyside moldings and claddingsFacia and bumper coversInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 107 °C | 225 °F | ASTM D648 |
RheTech Products FT4802-691UV Thermoplastic Polyolefin, UV Stabilized, RJ3 Dark Grey Green Applications: Bodyside moldings and claddingsFacia and bumper coversExterior componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 107 °C | 225 °F | ASTM D648 |
RheTech Products FT4802-692UV Thermoplastic Polyolefin, UV Stabilized, RS8 Grey Applications: Bodyside moldings and claddingsFacia and bumper coversExterior componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 107 °C | 225 °F | ASTM D648 |
RheTech Products FT4802-693UV Thermoplastic Polyolefin, UV Stabilized, SPN Dark Teal Applications: Bodyside moldings and claddingsFacia and bumper coversExterior componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 107 °C | 225 °F | ISO 75 |
Polyplastic Armlen® PP MF 15-3 FR Polypropylene Homopolymer, Mineral Filled Flame retardant, RoHS compliantInformation provided by PolyPlastic Group. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 107 °C | 225 °F | ASTM D648 |
Polymer Resources PPX-FR5 Modified-PPO, V-0 Flame Retardant Modified-Polyphenylene Oxide, V-0 Flame Retardant, 225F HDTFeatures: • Bromine Free • Chlorine FreeProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 107 °C | 225 °F | ASTM D648 |
PolyMirae Moplen HP601N Injection Molding Grade Polypropylene Moplen HP601N is the polypropylene homopolymer manufactured by PMC under the license of BASELL using the Spheripol process. Moplen HP601N is a homopolymer typically used by customers in Glass Mat Sh.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 107 °C | 225 °F | Unannealed; ASTM D648 |
Multibase Multi-Pro® 2003 TI Polypropylene Talc Filler, 20% by weight.Forms:PelletsProcessing Methods:Injection MoldingInformation provided by Multibase |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 107 °C | 225 °F | |
Polimeri Europa SINKRAL B260 ABS, Heat Stabilized
(discontinued **) Symbol according to ISO 1043-1: ABS Grade designation according to ISO 2580-ABS 1,MG,115-04-09-25 Very high heat injection moulding grade with good impact resistance for this category of ABS. Main.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 107 °C | 224 °F | ASTM D648 |
Ravago Manufacturing Americas Hybrid S555 ABS + Polycarbonate Alloy Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 107 °C | 225 °F | ASTM D648 |
Spartech PP5230 Calcium Carbonate Filled Homopolymer Offers improved stiffness versus unfilled materials. They offer substantial improvements in drop weight (Gardner) impact over both unfilled polypropylene and other types of filled polypropylene. Cal.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 107 °C | 225 °F | ASTM D648 |
Spartech PP7130 Talc Filled High Impact Copolymer Good material choice for applications where low to medium levels of impact are required and where stiffness and heat deflection properties remain criticalInformation provided by Spartech |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 107 °C | 225 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® PP 0121 B Polypropylene Availability: North AmericaForms: PelletsFiller/Reinforcement: Unspecified Filler/ReinforInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 107 °C | 225 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® PP 0159 B Polypropylene Availability: North AmericaForms: PelletsFiller/Reinforcement: Unspecified Filler/ReinforInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 107 °C | 225 °F | ISO 75 |
Styrolution Novodur® H802 ABS Novodur H802 is a high heat injection molding grade with high stiffness, especially suitable for being painted.Information provided by Styrolution |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 107 °C | 225 °F | ASTM D648 |
Plastics Group Polifil® GFABS-30 30% Glass-Reinforced Acrylonitrile-Butadiene Styrene (ABS) Polifil® GFABS series compounds combine the most desirable properties of both components - allowing for enhanced processability and toughness together with the stiffness of glass.Applications: Fire.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 107 °C | 225 °F | ASTM D648 |
Washington Penn Homopolymer Polypropylene 10% Talc Filled Talc-filled polypropylene compounds have been tailored specifically to meet the requirements of each of the major automobile producers. Grades are available to meet FDA food and drug packaging requi.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 107 °C | 225 °F | ASTM D648 |
A. Schulman PP 3449-01 Polypropylene Copolymer Polypropylene DescriptionPolypropylene PP 3449-01 is a new generation copolymer polypropylene utilizing unique catalyst technology. Combining an excellent balance of high stiffness and impact. This product inc.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 107 °C | 225 °F | ASTM D648 |
ExxonMobil PP7033N Impact Copolymer Product Description: A high crystallinity, high stiffness, high impact copolymer resin designed for injection molding applications requiring medium melt flow rate, good processing characteristics a.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 107 °C | 225 °F | Flatw 80x10x4, sp=64 mm; ISO 75/Bf |
Eurostar Starpylen MB006SU PP, Glass Bead Filled, Injection Molding Resin Starpylen MB006SU is a Glass Bead Reinforced Polypropylene Injection Molding ResinInformation provided by Eurostar. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 107 °C | 225 °F | ASTM D648 |
Braskem H 201 Injection Molding Polypropylene Description: H 201 is a high melt flow rate additivated homopolymer suitable for injection molding and fiber extrusion applications. This product exhibits excellent processability with good melt sta.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 107 °C | 225 °F | ASTM D648 |
Aclo Accutech Polypropylene Homopolymer HP0334W10L1 Wollastonite Reinforced |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 107 °C | 225 °F | ASTM D648 |
Cheng Yu Plastic A702G15 ABS 15% Glass Fiber Reinforced |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 107 - 157 °C | 225 - 315 °F | Average value: 126 °C Grade Count:9 |
Overview of materials for Polyphenylene Ether + Styrene-Butadiene Blend This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether + Styrene-Butadiene Blend". Each property range of values reported is minimum and ma.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 107 °C | 225 °F | |
Polimeri Europa SINKRAL D160 ABS, Heat Stabilized
(discontinued **) Symbol according to ISO 1043-1: ABS Grade designation according to ISO 2580-ABS 1,MG,115-08-09-25 Very high heat injection moulding grade with good flow. Permits production of complex, thin walled.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 107 °C | 225 °F | ASTM D648 |
SK Chemicals SKYPEL P155D Productivity Grade SKYPEL is a thermoplastic polyester elastomer (TPEE). It is a polymer resin having the property somewhere between plastics and rubber, which have various properties ranging from high hardness plasti.. |