Mechanical Properties Metric English Comments
Flexural Strength 34.5 MPa
5000 psi
ASTM D790
Network Polymers Softflex® 1104
Description: Softflex® Thermoplastic Elastomer AlloyInformation provided by Network Polymers Inc.
Flexural Strength 34.5 MPa
5000 psi
ASTM D790
Ravago Manufacturing Americas Hylon® N1000THL Nylon 6/6 (DAM)
Information provided by Ravago.
Flexural Strength 34.5 MPa
5000 psi
ASTM D790-95
Multibase Multi-Pro® 2510 XGW High Gloss Polypropylene
PP High Gloss compound formulated for small appliances such as food-processors and coffee machines. This product is high heat stabilized for use in irons and other appliances with elevated temperat..
Flexural Strength 34.5 MPa
5000 psi
ASTM D790
PolyOne Lubri-Tech™ ATH-000/5M Acetal-Homopolymer  (discontinued **)
Description/Features:Molybdenum Disulfide LubricatedInformation provided by PolyOne Corporation.
Flexural Strength 34.5 MPa
5000 psi
ASTM D790
PolyOne Edgetek® PE-40MC/000 High Density Polyethylene (HDPE)  (discontinued **)
Description/Features:Mica FilledInformation provided by PolyOne Corporation.
Flexural Strength 34.5 MPa
5000 psi
Conditioned; ASTM D790
Ravago Manufacturing Americas Hylon® N1000THLUV2 Polyamide 66  (discontinued **)
Available in North America Additive: Heat Stabilizer, Lubricant and UV StabilizerFeatures: Lubricated, Heat Stabilized and Good ToughnessRoHS CompliantAuto Specifications: GM GMP.PA66.079 Color: Bla..
Flexural Strength 34.5 MPa
5000 psi
ASTM D790
Ravago Manufacturing Americas Hylon® N1000TL Nylon 6/6 (Cond)  (discontinued **)
Information provided by Ravago
Flexural Strength 34.5 MPa
5000 psi
SGL Carbon Group EK 40 Graphite
Good mechanical strength, good sliding properties, high temperature resistance, high thermal shock resistance, low wettability, high corrosion resistance, high thermal conductivity, high purity, and..
Flexural Strength 34.5 MPa
5000 psi
ASTM D790
Techmer ES HiFill® PP 0159 B Polypropylene
Availability: North AmericaForms: PelletsFiller/Reinforcement: Unspecified Filler/ReinforInformation provided by TP Composites, Inc.
Flexural Strength 34.5 MPa
5000 psi
ASTM D790
Techmer ES Luriblend® HIPS E SL5
Availability: North AmericaForms: PelletsAdditive: Silicone Lubricant (5%)Appearance: Natural ColorProcessing Method: ExtrusionInformation provided by TP Composites, Inc.
Flexural Strength 34.5 MPa
5000 psi
ASTM D790
Total PSI 960E Polystyrene
Polystyrene 960E is a high impact polystyrene designed for extrusion/thermoforming applications that require exceptional resistance to attack from fats and oils. This ESCR material is used for lids ..
Flexural Strength 34.5 MPa
5000 psi
ASTM D790
Ecomass® 1002TU96 Tungsten Powder Filled PEBA, Injection Molding Grade
High Specific Gravity, Tungsten Powder Filled Polyether Block Amide (PEBA), Product Form - PelletsProcessing Method: Injection MoldingNontoxic alternative to Lead, weighting, balancing and radiatio..
Flexural Strength 34.5 - 172 MPa
5000 - 25000 psi
Du-Co Ceramics S-699 Alumina
Du-Co Ceramics Company manufactures a variety of crushable ceramic materials for use worldwide in cartridge heaters, thermocouples, and mineral insulated cable. The crushable ceramic products are cu..
Flexural Strength 34.5 MPa
5000 psi
ASTM D790
Aclo Accucomp Polypropylene CPO425BAV Automotive Approved Copolymer Expandable Grade
Flexural Strength 34.5 MPa
5000 psi
ASTM D790
Adell EZ-14 Homopolymer Polypropylene, 20% Calcium Carbonate Filled
Data provided by Adell Plastics, Inc.
Flexural Strength 34.5 MPa
5000 psi
ASTM D790
Americas Styrenics STYRON A-TECH® 1290 High Impact Polystyrene
Product CharacteristicsEasy processingGood impact resistanceESCRFood Contact CompliantUL Classification 94HBTypical ApplicationsCreamer and yot containersExtrusion/ thermoformingInformation provided..
Flexural Strength 34.5 - 89.6 MPa
5000 - 13000 psi
Compared to 500 for concrete
Abatron AboJet Structural Crack-Injection Resin
Structural crack injection resin for foundations, dikes, columns, load-bearing walls and structures. Offers strength, performance, durability, cost effectiveness and restoration instead of demoliti..
Flexural Strength 34.5 MPa
5000 psi
ASTM D790
Asahi Kasei Thermofil P-9900-1760 Unreinforced, Heat Stabilized, Impact Modified
Information provided by Asahi Thermofil
Flexural Strength 34.5 MPa
5000 psi
ASTM D790
Americas Styrenics STYRON® 487 High Impact Polystyrene
Product CharacteristicsGood TrimmabilityToughnessHeat resistanceFood Contact CompliantUL Classification 94HBTypical ApplicationsLidsAppliancesPackaging/disposablesHousewaresInformation provided by A..
Flexural Strength 34.5 MPa
5000 psi
ASTM D790
Techmer ES Statiblend® PP TM10 BK
Availability: North AmericaForms: PelletsFiller/Reinforcement: Talc Filler, 10% Filler by WeightFeatures: ConductiveUL File Number: E157318Appearance: BlackInformation provided by TP Composites, Inc..
Flexural Strength 34.5 MPa
5000 psi
ASTM D790
Chase Plastics CP Pryme® PPC100-35M Polypropylene Copolymer
Information provided by Chase Plastics.