Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

A. Schulman PP 1247-01 Polypropylene Homopolymer Polypropylene

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Molded
Manufacturer A. Schulman, Inc.
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF A. Schulman PP 1247-01 Polypropylene Homopolymer Polypropylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
DescriptionPolypropylene PP 1247-01 is a homopolymer polypropylene designed for general-purpose injection-molding applications where parts require excellent stiffness. ApplicationPolypropylene PP 1247-01 meets FDA Regulation 21 CFR 177.1250, for all food contact applications.Information provided by A. Schulman.
Physical Properties Metric English Comments
Specific Gravity 0.902 g/cc
0.902 g/cc
ASTM D792
Melt Index of Compound 4.0 g/10 min

@Load 2.16 kg,
Temperature 230 °C
4.0 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 95
95
ASTM D785
Tensile Strength, Yield 33.1 MPa
4800 psi
ASTM D638
Elongation at Break 12 %
12 %
ASTM D638
Flexural Modulus 1.41 GPa
205 ksi
ASTM D790
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 115.6 °C
240.1 °F
ASTM D648
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved